journal article·2013-03

Wetting and interfacial phenomena in relation to joining of alumina via Co/Nb/Co interlayers

Fabrizio Valenza, Maria L. Muolo, Alberto Passerone, Andreas M. Glaeser

Publisher page

Abstract

When designing multilayer metallic interlayers for transient-liquid-phase (TLP) bonding of ceramics, the phenomena that occur at the interface between the liquid metal alloy formed at the joining temperature and the solid ceramic to be joined have a major effect on the success or failure of the joining process. To assess the behavior of liquids that could develop when using Co/Nb/Co trilayers to bond Al2O3 ceramics, the wettability and interfacial behavior of pure Co and Co-Nb alloys on sapphire and polycrystalline Al2O3 were studied. Contact angles were measured at 1500°C using the sessile-drop technique, and the microstructures of the resulting metal/ceramic interfaces were characterized by scanning electron microscopy and energy-dispersive spectroscopy. Observations were assessed and evaluated in the context of predictions of thermodynamic properties. Additions of Nb to Co reduced the contact angle and thus improved the adhesion between the ceramic and metal. Nb additions also enhanced dissolution of Al2O3.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Advanced ceramic materials synthesis · Materials Engineering and Processing · Intermetallics and Advanced Alloy Properties

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (47)

Show source-provided references
1. Paulonis, D.F., Duvall, D.S., Owczarski, W.A., Diffusion bonding utilizing transient liquid phase, 1972; US Patent 3678570.
2. Transient liquid phase bonding10.1146/annurev.ms.22.080192.000323 ↗
3. Ceramic Joining – Part I – partial transient liquid-phase bonding of alumina via Cu/Pt interlayers10.1007/BF00363367 ↗
4. Ultrarapid transient-liquid-phase bonding of Al2O3 ceramics10.1002/adma.200801550 ↗
5. Overview of transient liquid phase and partial transient liquid phase bonding10.1007/s10853-011-5561-1 ↗
6. Nicholas · 1998
7. Joining of ceramics and metals10.1146/annurev.ms.18.080188.000403 ↗
8. Ceramic/metal joining for structures and materials
9. Interaction between two Ni-base alloys and oxide ceramics: SiO2, ZrO2, HfO2, Al2O310.4028/www.scientific.net/MSF.251-254.925 ↗
10. Wetting and interactions of Ni- and Co-based superalloys with different ceramic materials10.1007/s10853-009-3801-4 ↗
11. The wetting characteristics and surface tension of some Ni-based alloys on yttria, hafnia alumina and zirconia substrates10.1007/BF02645152 ↗
12. On measuring wettability in infiltration processing10.1016/j.scriptamat.2007.02.002 ↗
13. Wetting in infiltration of alumina particle preforms with molten copper10.1007/s10853-005-1980-1 ↗
14. The wetting of solids by molten metals and its relation to the preparation of metal-matrix composites composites10.1007/BF01160545 ↗
15. Interfacial and capillary phenomena in solidification processing of metalmatrix composites10.1016/0956-7143(93)90012-W ↗
16. Interfaces in oxide–fibre-based composites10.1016/j.cossms.2006.05.004 ↗
17. Wettability and interface considerations in advanced heat-resistant Ni-base composites
18. Influence of gas impurities on the solid-state bonding of Nb/Al2O3 composites above 1200°C
19. Bonding mechanism between alumina and niobium10.1007/BF00542374 ↗
20. Investigations of the chemistry and bonding at niobium sapphire interfaces10.1557/JMR.1994.2574 ↗
21. Extraordinary adhesion of niobium on sapphire substrates10.1103/PhysRevLett.79.5062 ↗
22. Ceramic joining IV effects of processing conditions on the properties of alumina joined via Cu/Nb/Cu interlayers10.1023/A:1012565600601 ↗
23. Joining of alumina via Cu/Nb/Cu interlayers
24. Rapid transient-liquid-phase bonding of Al2O3 with microdesigned Ni/Nb/Ni interlayers10.3139/146.110249 ↗
25. Surface grain boundary and interfacial energies in Al2O3 and Al2O3-Sn Al2O3-Co systems10.1007/BF00552390 ↗
26. The strength of metal/alumina interfaces10.1007/BF00757901 ↗
27. Effect of oxygen on the surface tension of liquid Co and Co-Fe alloys and the wettability of Al2O310.2320/jinstmet1952.46.10_957 ↗
28. Adhesion therrnodynamique dans les systems non-reactifs metal liquide-alumine10.1051/jcp/1986830561 ↗
29. Effect of Ti admixtures on the surface tension of Ni and Co and on their interfacial tension with aluminum oxide
30. New strategies for joining ceramics for high-temperature applications10.4028/www.scientific.net/KEM.111-112.157 ↗
31. Effect of Nb on the interfacial wettability in Al2O3/medium Mn steel
32. Co-Nb (Cobalt-Niobium)10.1007/s11669-009-9632-9 ↗
33. Diffusion of Nb, Fe, Co Ni and Cu in Nb10.1080/14786437708232950 ↗
34. Eustathopoulos · 1999
35. An automatic technique for measuring the surface tension of liquid metals
36. Wettability of by molten Ni(B) alloys interpreted by CALPHAD methods Part 2: wetting and interfacial reactivity10.1016/j.calphad.2009.10.006 ↗
37. Wettability and work of adhesion of nonreactive liquid metals on silica10.1111/j.1151-2916.1988.tb06407.x ↗
38. Measurement of contact angle and work of adhesion at high temperature10.1007/s10853-005-1945-4 ↗
39. Thermodynamics of cobalt precipitation in cobalt-doped Al2O310.1111/j.1151-2916.1975.tb19030.x ↗
40. The thermodynamics of spinel interphase formation at diffusion bonded NiAl/Al2O3 interfaces10.1016/0956-7151(91)90160-3 ↗
41. Phase diagrams of Ti-Al-C, Ti-Y-O, Nb-Y-O, Nb-Al-O at 1100°C10.1007/BF02649396 ↗
42. Massalski · 1990
43. The wettability of solids by liquid metals
44. Ridging effects on wetting and spreading liquids on solids10.1016/S1359-6454(97)00391-1 ↗
45. Segregation of aluminium at nickel–sapphire interfaces10.1023/A:1015198409536 ↗
46. Effect of Cr on interfacial interaction and wetting mechanisms in Ni Alloy/Alumina systems10.1016/0956-7151(92)90415-B ↗
47. Barin · 1973