Thermal degradation of an oxide fibre (Nextel 720)/aluminosilicate composite
Source abstract
Abstract
Abstract The effect of thermal exposure on the microstructure and tensile stress–strain behaviour has been investigated for composites of woven continuous oxide fibres (Nextel 720) in a porous aluminosilicate matrix. The tensile tests were carried out on straight-sided, centre hole notched plates with 0/90° and ±45° orientations. The as-received material was slightly notch sensitive in that the net section fracture stress decreased somewhat with increasing hole diameter but much less than predicted for an ideally elastic, fully notch-sensitive material. After exposure at 1100 °C and for long time at 1000 °C in air the composite was embrittled. In the 0/90 composite this resulted in a reduced fracture strength, a reduced strain to failure as well as a reduced fracture toughness and damage zone size. After exposure for 100 h at 1100 °C (the most extreme exposure applied) the material also became significantly more notch sensitive and had failure characteristics similar to those of a monolithic ceramic. The ±45 composite was also embrittled which resulted in a reduced strain to failure but an increase in fracture strength. Density measurements and observations on the microstructure and fracture surfaces indicated that the embrittlement was due mainly to localised densification of the matrix and an increase in fibre/matrix bonding.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Advanced ceramic materials synthesis · Mechanical Behavior of Composites · Composite Material Mechanics
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (29)
Show source-provided references
1. Concept for a damage-tolerant ceramic composite with “strong” interfaces10.1111/j.1151-2916.1996.tb08138.x ↗
2. Processing and performance of an all-oxide ceramic composite10.1111/j.1151-2916.1998.tb02590.x ↗
3. 2000
4. Antti, M.-L. and Lara-Curzio, E., Effect of notches, specimen size, and fiber orientation on the monotonic tensile behavior of composites at ambient and elevated temperatures. Ceram. Eng. Sci. Proc., 2001, 22, 643–650.10.1002/9780470294680.ch74 ↗
5. Mechanisms of deformation and failure in carbon-matrix composites subject to tensile and shear loading10.1111/j.1151-2916.1995.tb08897.x ↗
6. Notch effects in carbon matrix composites10.1111/j.1151-2916.1994.tb04510.x ↗
7. Mechanical properties of continuous-fiber-reinforced carbon matrix composites and relationships to constituent properties10.1111/j.1151-2916.1992.tb04381.x ↗
8. Notch sensitivity of fiber-reinforced ceramic-matrix composites10.1111/j.1151-2916.1999.tb01899.x ↗
9. Notched fracture behavior of oxide/oxide Nextel™720/AS composite10.1002/9780470294628.ch68 ↗
10. In-plane mechanical properties of an all-oxide ceramic composite10.1111/j.1151-2916.1999.tb02148.x ↗
11. Notched fracture behavior of an oxide/oxide ceramic-matrix composite10.1111/j.1151-2916.1999.tb02207.x ↗
12. Evaluation of damage evolution in ceramic-matrix composites using thermoelastic stress analysis10.1111/j.1151-2916.2000.tb01195.x ↗
13. Jurf, R. A. and Butner, S. C., Advances in oxide–oxide CMC. In: Proc. Int. Gas Turbine and Aeroengine Congress and Exhibition, Indianapolis, IN, 1999.10.1115/99-GT-190 ↗
14. Personal Communication with E. Carelli, Siemens Westinghouse, Pittsburgh, PA.
15. Microstructural stability and room temperature mechanical properties of the Nextel 720 fibre10.1016/S0955-2219(00)00249-1 ↗
16. Mechanical and microstructural properties of Nextel™ 720 relating to its suitability for high temperature application in CMCs10.1002/9780470294567.ch23 ↗
17. The effect of thermal exposures on the strengths of Nextel™ 550 and 720 filaments10.1111/j.1151-2916.1999.tb02159.x ↗
18. Savin · 1961
19. Young · 1989
20. Finite width correction factor for anisotropic plate containing a central opening10.1177/002199838802201105 ↗
21. Macroscopic fracture mechanics of advanced composite materials10.1177/002199837100500402 ↗
22. Stress fracture criteria for laminated composites containing stress concentrations10.1177/002199837400800303 ↗
23. Notch ductile-to-brittle transition due to localized inelastic band10.1115/1.2904225 ↗
24. Babushkin, O., unpublished work.
25. Analysis of damage evolution in continuous fiber-reinforced oxide/oxide composites under cyclic loading, using infra-red thermography10.1002/9780470294680.ch82 ↗
26. Microstructure and high temperature properties of Nextel 720 fibres10.1002/9780470314784.ch44 ↗
27. Al2O3-SiO2 system in the mullite region10.1111/j.1151-2916.1987.tb04875.x ↗
28. Fabrication of sapphire fibre reinforced ceramic matrix composite
29. Polymorphism of silica10.1023/A:1018636920023 ↗