journal article·2020-04Open access

Thermal stability enhancement of Cr2AlC coatings on Zr by utilizing a double layer diffusion barrier

Stanislav Mráz, Miléna Tyra, Moritz to Baben, Marcus Hans, Xiang Chen, Friederike Herrig, Konstantina Lambrinou, Jochen M. Schneider

Abstract

Decomposition of Cr2AlC deposited onto a Zr substrate and vacuum-annealed is observed at 800 °C as Al diffuses from the MAX phase into the Zr substrate. A double layer of ZrN and AlN has been predicted by CALPHAD calculations to act as diffusion barrier between the Zr substrate and Cr2AlC. Experimental thermal stability investigations corroborate this prediction by confirming that the proposed double layer diffusion barrier coatings suppress the decomposition of Cr2AlC for one hour at temperatures of up to 1000 °C.
Source: openalex_inverted_index · Quality: baseline

Research context

OpenAlex topics: MXene and MAX Phase Materials · Aluminum Alloys Composites Properties · Advanced materials and composites

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (27)

Show source-provided references
1. Barsoum · 2013
2. The MN+1AXN phases: a new class of solids; thermodynamically stable nanolaminates10.1016/S0079-6786(00)00006-6 ↗
3. Elastic and mechanical properties of the MAX phases10.1146/annurev-matsci-062910-100448 ↗
4. The Mn+1AXn phases: materials science and thin-film processing10.1016/j.tsf.2009.07.184 ↗
5. Towards large area deposition of Cr2AlC on steel10.1016/j.tsf.2005.12.219 ↗
6. Comparison of thermal stability in MAX 211 and 312 phases
7. Synthesis and thermal stability of Cr2AlC10.1016/j.jeurceramsoc.2011.01.009 ↗
8. Oxidation of Cr2AlC at 1300°C in air10.1016/j.corsci.2007.03.044 ↗
9. High-temperature oxidation and hot corrosion of Cr2AlC10.1016/j.actamat.2007.07.024 ↗
10. Oxidation behavior of Cr2AlC ceramics at 1100 and 1250°C10.1007/s10853-008-2516-2 ↗
11. A critical review of the oxidation of Ti2AlC, Ti3AlC2, and Cr2AlC in air10.1080/21663831.2013.806364 ↗
12. Long-time oxidation of Cr2AlC between 700 and 1000°C in air10.1007/s11085-012-9285-7 ↗
13. Cyclic oxidation of Cr2AlC between 1000 and 1300°C in air10.1016/j.jallcom.2007.10.018 ↗
14. Influence of grain size on high temperature oxidation behavior of Cr2AlC ceramics10.1016/j.ceramint.2012.09.039 ↗
15. Short-term oxidation resistance and degradation of Cr2AlC coating on M38G superalloy at 900-1000°C10.1016/j.corsci.2011.07.032 ↗
16. Fabrication and oxidation behavior of Cr2AlC coating on Ti6242 alloy10.1016/j.surfcoat.2010.01.002 ↗
17. Oxide-scale growth on Cr2AlC ceramic and its consequence for self-healing10.1016/j.scriptamat.2013.04.013 ↗
18. Oxidation and crack healing behavior of a fine-grained Cr2AlC ceramic10.1111/jace.12170 ↗
19. Crack healing of Cr2AlC MAX phase studied by X-ray tomography10.1016/j.jeurceramsoc.2016.07.018 ↗
20. Thermal and chemical stability of Cr2AlC in contact with α-Al2O3 and NiAl10.3139/146.110439 ↗
21. Bonding and oxidation protection of Ti2AlC and Cr2AlC for a Ni-based superalloy10.1016/j.jeurceramsoc.2018.10.019 ↗
22. On the chemical compatibility between Zr-4 substrate and well-bonded Cr2AlC coating10.1016/j.jmst.2018.09.005 ↗
23. FactSage thermochemical software and databases, 2010-201610.1016/j.calphad.2016.05.002 ↗
24. Ab initio guided temperature synthesis strategy for smooth face-centered cubic FeMn thin films10.3390/met8060384 ↗
25. Fiji: an open-source platform for biological-image analysis10.1038/nmeth.2019 ↗
26. oxidation of Cr2AlC coatings in the temperature range of 1230 to 1410°C10.1016/j.surfcoat.2011.03.086 ↗
27. http://www.crct.polymtl.ca/fact/phase_diagram.php?file=NZr.jpg&dir=SpMCBN.