Abstract

Abstract α- and α/β-SiAlON compositions, doped with Y 2 O 3 or Nd 2 O 3 , were densified by gas pressure sintering (GPS). The wear and mechanical properties of the materials were investigated and compared to β-Si 3 N 4 materials. Microstructure evolution and its change with composition as well as the influence of the microstructural changes on the mechanical and tribological properties were reported. Wear tests were performed using a tribometer with ball-on-plate geometry in reciprocating sliding contact under dry condition. It was observed that α/β-SiAlON compositions, doped with Y 2 O 3 , have better wear properties in comparison to α-SiAlON and β-Si 3 N 4 samples. Field emission scanning electron microscopy (FESEM) was used to analyse the worn surfaces after wear tests. The results showed that α/β-SiAlON and β-Si 3 N 4 materials have different wear behaviour.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Advanced ceramic materials synthesis · Advanced materials and composites · Ferroelectric and Piezoelectric Materials

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (29)

Show source-provided references
1. Silicon nitride and related materials10.1111/j.1151-2916.2000.tb01182.x ↗
2. α-SiAlON ceramics10.1038/274880a0 ↗
3. Optimizing mechanical properties and thermal stability of Ln-α-β-sialon by using duplex Ln elements (Dy and Sm)10.1016/S0955-2219(98)00174-5 ↗
4. Tribological behavior of Dy–sialon ceramics sliding against Si3N4 under lubrication of fluorine-containing oils10.1016/S0043-1648(02)00040-6 ↗
5. Ceramic–ceramic composite materials with improved friction and wear properties10.1016/0301-679X(92)90122-4 ↗
6. Materials-based concepts for an oil-free engine
7. The transition of wear mode during the running-in process of silicon nitride sliding in water10.1016/S0043-1648(96)07283-3 ↗
8. The effect of surface roughness on friction of ceramics sliding in water10.1016/S0043-1648(98)00208-7 ↗
9. Sliding friction and wear up to 600°C of high speed steels and silicon nitrides for gas turbine bearings10.1016/0043-1648(93)90091-Y ↗
10. Unlubricated sliding wear mechanism of fine ceramic Si3N4 against high-chromium cast iron10.1016/0301-679X(94)90029-9 ↗
11. Sliding friction and wear of ceramics at elevated temperatures up to 1000°C
12. Unlubricated sliding wear of ceramics against graphitized cast irons10.1016/0043-1648(94)90355-7 ↗
13. Friction and wear behaviour of hot-pressed SiAlON-steel ball tribopair under reciprocating sliding conditions
14. Limitations on the use of ceramics in unlubricated sliding applications due to transfer layer formation10.1016/0043-1648(94)90162-7 ↗
15. The combined effect of speed and humidity on the wear and friction of silicon nitride10.1016/0043-1648(93)90506-H ↗
16. Tribological properties of AlN–CeO2–Si3N4 cutting materials in unlubricated sliding against tool steel and cast iron10.1016/0921-5093(95)10154-3 ↗
17. Tribo-oxidational effects on friction and wear behaviour of silicon nitride/tool steel and silicon nitride/gray cast iron contacts10.1111/j.1151-2916.1999.tb01859.x ↗
18. State of the art review on friction and wear mechanisms of ceramics
19. Friction and wear of silicon nitride at 150°C to 800°C10.1080/05698198608981711 ↗
20. Wear transition diagram for silicon nitride10.1016/0043-1648(93)90332-G ↗
21. Friction and wear of silicon nitride exposed to moisture at high temperatures
22. Tribological behavior of silicon nitride materials under unlubricated sliding between 22°C and 1000°C
23. Ceramic–ceramic composites for dry sliding in closed tribosystems
24. The friction and wear of ceramic/ceramic and ceramic/metal combinations in sliding contact
25. High temperature friction and wear testing of silicon nitride ceramics10.1016/0301-679X(95)00020-5 ↗
26. Taut, T. and Bergmann, J., Rietveld-Analyse mit dem Programmsystem Refine ++, Handbuch der Version 1.1, 1998.
27. Amin · 1991 · 4
28. Influence of rare-earth additives on wear properties of hot-pressed silicon nitride ceramics under dry sliding conditions10.1111/j.1551-2916.2004.01683.x ↗
29. Dopant-dependent oxidation behaviour of α-SiAlON ceramics10.1023/B:JMSC.0000035325.94289.b8 ↗