Novel fabrication of injection-moulded ceramic parts with large section via partially water-debinding method
Source abstract
Abstract
Abstract In this work, we adopt a combination of low molecular weight PEG (L-PEG) and high molecular weight PEG (H-PEG) as water-soluble binder to fabricate injection-moulded ceramic parts with large section. The mechanism of the combination of PEGs removal was proposed for the first time. Defect-free near gear parts with large-sized-section (thickness – 16 mm) were successfully fabricated through water extraction (15 h) followed by rapid thermal pyrolysis (4.5 h). It solves the difficulty of fabricating injection-moulded ceramic parts with large section and our approach is energy saving and high-efficiency as compared with conventional thermal debinding. The results demonstrate that our approach of partially water-debinding followed by rapid thermal pyrolysis could solve the problems of conventional thermal debinding, providing an effective route for the production of injection moulded ceramic parts with large section.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Injection Molding Process and Properties · Additive Manufacturing and 3D Printing Technologies · Advanced materials and composites
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (20)
Show source-provided references
1. Fabrication of injection moulded translucent alumina ceramics via pressureless sintering10.1179/1743676111Y.0000000005 ↗
2. Injection molding of surface modified powders with high solid loadings: a case for fabrication of translucent alumina ceramics10.1016/j.jeurceramsoc.2011.03.003 ↗
3. Surface modification mechanism of stearic acid to zirconia powders induced by ball milling for water-based injection molding10.1111/j.1551-2916.2011.04475.x ↗
4. In situ evaluation of dimensional variations during water extraction from alumina injection-moulded parts10.1016/S0955-2219(99)00221-6 ↗
5. Injection-molded ceramics: critical aspects of the binder removal process and component fabrication10.1016/0955-2219(93)90055-V ↗
6. Thermal debinding of powder injection molded parts – observations and mechanisms10.1007/BF02651756 ↗
7. Properties of ceramic injection-molding formulations. 3: polymer removal10.1007/BF01148795 ↗
8. Residual stresses and cracking in large ceramic injection mouldings subjected to different solidification schedules10.1016/S0955-2219(00)00120-5 ↗
9. Aetiology of defects in large ceramic moldings10.1111/j.1151-2916.1999.tb02046.x ↗
10. Rivers RD, Kokomo, Inventor; Cabot Corporation, Assignee. Method of injection molding powder metal parts. United States Patent US 4113480 (1978) Sep 2.
11. Solvent debinding mechanism for alumina injection molded compacts with water-soluble binders10.1016/S0272-8842(02)00226-2 ↗
12. Dynamics of water debinding in ceramic injection moulding10.1179/174367608X362430 ↗
13. Solvent debinding mechanism for alumina injection molded compacts with water-soluble binders10.1016/S0272-8842(02)00226-2 ↗
14. Solvent debinding kinetics of alumina green bodies by powder injection-molding10.1016/0272-8842(95)99791-9 ↗
15. Pore structure evolution during solvent extraction and wicking10.1016/0272-8842(95)00025-9 ↗
16. Effective length scale for predicting solvent-debinding times of components produced by powder injection molding10.1111/j.1151-2916.1999.tb01888.x ↗
17. A model for PEG removal from alumina injection moulded parts by solvent debinding10.1016/j.jmatprotec.2006.08.004 ↗
18. Injection moulding of alumina with partially water soluble binder system and solvent debinding kinetics10.1179/174328407X161196 ↗
19. Water-soluble binder of cellulose acetate butyrate/poly(ethylene glycol) blend for powder injection molding10.1023/A:1012579010171 ↗
20. Preparation and evaluation of Al2O3 plastic forming feedstock with partially water soluble polymer as a binder10.1016/S0924-0136(02)01099-3 ↗