Enhancing the spark-plasma sinterability of B4C nanopowders via room-temperature methylation induced purification
Source abstract
Abstract
Abstract B 4 C nanopowders were subjected to room-temperature methylation to assess its possible beneficial effect on single-step cycle spark-plasma sinterability. It was found that methylation removes the oxidic impurities, thus chemically purifying the B 4 C nanopowders without nanoparticle growth. Next, it was determined that the temperature of spark-plasma sintering optimizing the microstructure and mechanical properties is ∼1500 °C, below which there is insufficient densification and above which there is marked grain growth, scenarios both detrimental for the hardness of these B 4 C ceramics. It was also found that the so-purified nanopowders are more sinterable than the as-received nanopowders, and also than the same nanopowders purified by annealing under an inert atmosphere. This greater sinterability resulting from the elimination of the oxidic impurities is attributable to the enhanced grain-boundary diffusion favouring the densification. Thanks to the methylation, dense, nano-grained, superhard B 4 C ceramics can thus be fabricated with greater energy efficiency. Implications of interest for the ceramics community are discussed.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Advanced ceramic materials synthesis · Boron and Carbon Nanomaterials Research · Advanced materials and composites
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (31)
Show source-provided references
1. Nanoindentation and Raman spectroscopy studies of boron carbide single crystals10.1063/1.1521580 ↗
2. Shock-induced localized amorphization in boron carbide10.1126/science.1080819 ↗
3. Density- and hardness-optimized pressureless sintered and post-hIPed B4C10.1557/JMR.2005.0260 ↗
4. Dynamic indentation response of fine-grained boron carbide10.1111/j.1551-2916.2007.01652.x ↗
5. Static and dynamic mechanical properties of boron carbide processed by spark plasma sintering10.1016/j.jeurceramsoc.2009.07.007 ↗
6. Sintering behavior and mechanical properties of B4C ceramics fabricated by spark plasma sintering
7. Synthesis and consolidation of boron carbide: a review10.1179/095066009X12506721665211 ↗
8. Microstructural characterization of spark plasma sintered boron carbide ceramics10.1016/j.ceramint.2009.09.004 ↗
9. Boron carbide: structure, properties, and stability under stress10.1111/j.1551-2916.2011.04865.x ↗
10. Enhanced mechanical properties of nanocrystalline boron carbide by nanoporosiy and interface phases10.1038/ncomms2047 ↗
11. Effect of spark plasma sintering parameters on microstructure and room-temperature hardness and toughness of fine-grained boron carbide (B4C)10.1016/j.jeurceramsoc.2012.08.028 ↗
12. High-temperature creep deformation of coarse-grained boron carbide ceramics10.1016/j.jeurceramsoc.2014.11.001 ↗
13. High-temperature deformation of fully-dense fine-grained boron carbide ceramics: experimental facts and modeling10.1016/j.matdes.2015.08.134 ↗
14. High-temperature plastic deformation of spark plasma sintered boron carbide-based composites: the case study of B4C–SiC10.1016/j.jeurceramsoc.2015.12.016 ↗
15. Grain size dependence of hardness and fracture toughness in pure near fully-dense boron carbide ceramics10.1016/j.jeurceramsoc.2016.01.017 ↗
16. Opportunities for advanced ceramics and composites in the nuclear sector10.1111/jace.12406 ↗
17. Toughening of super-hard ultra-fine grained B4C densified by spark-plasma sintering via SiC addition10.1016/j.jeurceramsoc.2013.01.018 ↗
18. Additive-free superhard B4C with ultrafine-grained dense microstructures10.1016/j.jeurceramsoc.2013.10.006 ↗
19. Densification of B4C nanopowder with nanograin retention by spark-plasma sintering10.1016/j.jeurceramsoc.2014.12.021 ↗
20. Hardness–grain size relations in ceramics10.1111/j.1151-2916.1994.tb04641.x ↗
21. Cho · 2006
22. Sintering of boron carbide heat-treated with hydrogen10.1111/j.1151-2916.2002.tb00420.x ↗
23. Aqueous dispersion and slip casting of boron carbide powder: effect of pH and oxygen content10.1111/j.1151-2916.1991.tb07147.x ↗
24. Densification of carbon-rich boron carbide nanopowder compacts10.1557/jmr.2007.0155 ↗
25. Green · 1998
26. A critical evaluation of indentation techniques for measuring fracture toughness: I direct crack measurements10.1111/j.1151-2916.1981.tb10320.x ↗
27. Defects in boron carbide before and after neutron irradiation10.1016/0001-6160(71)90040-X ↗
28. Haynes · 2015
29. Powder processing effects on the rapid low-temperature densification of ZrB210.1111/j.1551-2916.2011.04873.x ↗
30. German · 1996
31. Theory of normal and abnormal grain growth10.1016/0001-6160(65)90200-2 ↗