journal article·2017-08Open access

Enhanced oxidation resistance of SiC/SiC minicomposites via slurry infiltration of oxide layers

Jianyu Zhou, Amjad S. Almansour, George G. Chase, Gregory N. Morscher

Abstract

SiC based composite materials commonly have protective silica surface in air. Under humid environments at high temperatures, like occur in jet engines, the silica surface layer reacts with water molecules to form volatile silicon hydroxide (Si(OH)4) and the protection is reduced which cause jet engine degradation. An alternative approach to protect SiC based composites would be to infiltrate the SiC matrix via slurry with an oxide material that is resistant to the high-temperature and humid environment. As proof of concept, aqueous based mullite particle slurries were infiltrated by pressurized flow and by capillarity of the wetting slurry on the external surface of the porous SiC matrix of single-fiber-tow SiC/SiC minicomposites. Minicomposites were precracked at room temperature during tensile tests then tested in tensile creep in air at 1200 °C to study the degree of protection that the infiltrated mullite provided at high temperatures. Next, fracture surfaces were examined using SEM.
Source: europepmc · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Advanced ceramic materials synthesis · Aluminum Alloys Composites Properties · Advanced materials and composites

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (21)

Show source-provided references
1. Prediction of permeability for chemical vapor infiltration10.1111/jace.12456 ↗
2. Upper temperature limit of environmental barrier coatings based on mullite and BSAS10.1111/j.1151-2916.2003.tb03466.x ↗
3. Paralinear oxidation of silicon nitride in a water-vapor/oxygen environment10.1111/j.1151-2916.2003.tb03461.x ↗
4. Oxidation and corrosion of ceramics and ceramic matrix composites10.1016/S1359-0286(01)00009-2 ↗
5. Oxidation behavior of silicon carbide at 1200C in both air and water–vapor-rich environments10.1016/j.corsci.2014.07.052 ↗
6. Paralinear oxidation of silicon nitride in a water-vapor/oxygen environment10.1111/j.1151-2916.2003.tb03461.x ↗
7. Rare earth silicate environmental barrier coatings for SiC/SiC composites and Si3N4 ceramics10.1016/j.jeurceramsoc.2004.12.013 ↗
8. Plasma spray-physical vapor deposition (PS-PVD) of ceramics for protective coatings
9. Effect of fiber content on single tow SiC minicomposite mechanical and damage properties using acoustic emission10.1016/j.jeurceramsoc.2015.06.001 ↗
10. Tensile creep and rupture behavior of different fiber content and type single tow SIC/SIC minicomposites
11. Microcomposite test procedure for evaluating the interface properties of ceramic matrix composites10.1111/j.1151-2916.1995.tb08814.x ↗
12. Room and elevated temperature tensile properties of single tow Hi-Nicalon, carbon interphase, CVI SiC matrix minicomposites10.1016/S0955-2219(00)00138-2 ↗
13. Compressive creep of mullite ceramics10.1007/BF00724757 ↗
14. Mechanical properties of mullite materials10.1016/0955-2219(95)00133-6 ↗
15. Mullite+ CAS bond coat for environmental barrier coatings for Si-Based ceramics
16. EBC development for hot-pressed Y2O3/Al2O3 doped silicon nitride ceramics10.1016/j.msea.2010.05.067 ↗
17. Slurry based multilayer environmental barrier coatings for silicon carbide and silicon nitride ceramics—I. Processing10.1016/j.surfcoat.2010.06.029 ↗
18. Slurry based multilayer environmental barrier coatings for silicon carbide and silicon nitride ceramics—II. Oxidation resistance10.1016/j.surfcoat.2010.07.048 ↗
19. Fiber effects on minicomposite mechanical properties for several silicon carbide fiber-chemically vapor-Infiltrated silicon carbide matrix systems10.1111/j.1151-2916.1999.tb01734.x ↗
20. Lange's handbook of chemistry10.1080/10426919008953291 ↗
21. Bank · 2010