Abstract 3D SiCf/BN–SiC/SiBCN composites were fabricated via precursor impregnation and polymer infiltration pyrolysis (PIP). Oxidation behavior of the composites heated in air at 800 °C, 1000 °C and 1200 °C for 50 h was investigated. Following the oxidation treatment, it was found that the bending strength of the composites at different oxidation temperatures was degraded. The weight loss of the composites decreased gradually over the range of oxidation times of 1–50 h. In order to clarify the oxidation mechanism of the composites, reconstructed images, microstructures, phase compositions, the oxide layer formed on the composites and main chemical reactions were all analyzed. It was revealed that the degradation in the fracture strength of the composites was closely related to the oxidation of SiBCN matrix and BN-SiC interphase, whereas there was no signs of oxidation products about SiC fiber, which indicated that SiC fiber could be protected from oxygen by SiBCN matrix at 800−1200 °C in air.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Advanced ceramic materials synthesis · Advanced materials and composites · Aluminum Alloys Composites Properties

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (41)

Show source-provided references
1. Synthesis, pyrolysis of novel liquid SiBCN ceramic precursor and its application in ceramic matrix composites10.1016/j.jeurceramsoc.2016.11.009 ↗
2. High-temperature mechanical properties of Si-B-C-N-precursor-derived amorphous ceramics and the applicability of deformation models developed for metallic glasses10.1111/j.1151-2916.2000.tb01678.x ↗
3. Oxidation and corrosion of ceramics and ceramic matrix composites
4. Thermal stability, phase evolution, and crystallization in Si-B-C-N ceramics derived from a polyborosilazane precursor10.1111/j.1151-2916.2002.tb00357.x ↗
5. Crystallization and creep behavior of Si-B-C-N10.1016/j.actamat.2005.06.011 ↗
6. Amorphous silicoboron carbonitride ceramic with very high viscosity at temperatures above 1500 °C10.1111/j.1151-2916.1998.tb02780.x ↗
7. Progress of a novel non-oxide Si-B-C-N ceramic and its matrix composites10.1007/s40145-012-0017-x ↗
8. Fiber-reinforced composites with polymer-derived matrix: processing, matrix formation and properties
9. Fabrication of fiber-reinforced ceramic composites by the modified slurry infiltration technique10.1111/j.1551-2916.2007.01795.x ↗
10. The physics and mechanics of fibre-reinforced brittle matrix composites10.1007/BF00355946 ↗
11. Processing and properties of C/Si–B–C–N fiber-reinforced ceramic matrix composites prepared by precursor impregnation and pyrolysis10.1016/j.actamat.2007.12.001 ↗
12. Cfiber/SiCfiller/Si–B–C–Nmatrix composites with extremely high thermal stability10.1016/j.actamat.2009.05.033 ↗
13. Synthesis, pyrolysis of a novel liquid SiBCN ceramic precursor and its application in ceramic matrix composites10.1016/j.jeurceramsoc.2016.11.009 ↗
14. Oxidation protection for carbon fiber composites10.1016/0008-6223(89)90204-2 ↗
15. Oxidation protection for carbon fibre composites10.1007/BF00357844 ↗
16. Key developments in high temperature structural silicides10.1016/S0921-5093(98)01043-0 ↗
17. Oxidation behavior of SiC–SiBCN ceramics10.1016/j.ceramint.2014.09.025 ↗
18. A silicoboron carbonitride ceramic stable to 2,000°C10.1038/382796a0 ↗
19. Precursor-derived Si-B-C-N ceramics: oxidation kinetics10.1111/j.1151-2916.2001.tb00985.x ↗
20. Ablation mechanism and properties of SiCf/SiBCN ceramic composites under an oxyacetylene torch environment10.1016/j.corsci.2014.01.006 ↗
21. Studies on SiBN(C)-ceramics: oxidation and crystallization behavior lead the way to applications10.1557/PROC-346-617 ↗
22. Amorphous silicoboron carbonitride monoliths resistant to flowing air up to 1800℃10.1016/j.corsci.2016.03.026 ↗
23. Mechanical and microstructural characterisation of SiC- and SiBNC-fibre reinforced CMCs manufactured via PIP method before and after exposure ro air10.1016/j.jeurceramsoc.2012.05.028 ↗
24. Oxidation behavior of a 2D-SiCf/BN/SiBCN composite at 1350–1650°C in air10.1002/maco.201810070 ↗
25. Wet oxidation behavior of SiC/(SiC-SiBCN)x composites prepared by CVI combined with PIOP process10.1111/jace.16497 ↗
26. Modelling of dimensional changes during polymer-ceramic conversion for bulk component fabrication10.1007/BF01197660 ↗
27. Synthesis and pyrolysis mechanism of a novel polymeric precursor for SiBN ternary ceramic fibers10.1016/j.ceramint.2019.06.286 ↗
28. The role of the fiber/matrix interface in the first matrix cracking of fiber-reinforced brittle-matrix composites10.1016/0266-3538(94)90197-X ↗
29. Role of interface properties on the toughness of brittle matrix composites reinforced with ductile fibers10.1557/JMR.1992.3132 ↗
30. The role of interfaces in fiber-reinforced brittle matrix composites10.1016/0266-3538(91)90010-M ↗
31. The effect of defect locations on the stress distribution and crack initiation in monolithic aluminum vs. GLARE hybrid composite10.4028/www.scientific.net/MSF.486-487.354 ↗
32. The toughening and strengthening of ceramic materials through discontinuous reinforcement10.1007/BF01171532 ↗
33. Fabrication, mechanical properties and thermal stability of a novel glass matrix composite material reinforced by short oxycarbide fibres10.1023/A:1020664905937 ↗
34. Oxidation behavior from room temperature to 1500°C of 3D-C/SiC composites with different coatings10.1111/j.1151-2916.2002.tb00205.x ↗
35. Spectroscopic and calorimetric investigation of short and intermediate-range structures and energetics of amorphous SiCO, SiCN, and SiBCN polymer-derived ceramics
36. FACTSAGE thermochemical software and databases10.1016/S0364-5916(02)00035-4 ↗
37. Ablation behavior of graphene reinforced SiBCN ceramics in an oxyacetylene combustion flame10.1016/j.corsci.2015.07.006 ↗
38. Ablation of C/SiC, C/SiC–ZrO2 and C/SiC–ZrB2 composites in dry air and air mixed with water vapor10.1016/j.ceramint.2013.10.009 ↗
39. Ablation behavior and mechanism of SiCf/Cf/SiBCN ceramic composites with improved thermal shock resistance under oxyacetylene combustion flow10.1016/j.ceramint.2015.03.144 ↗
40. High-temperature oxidation of boron nitride: II, Boron nitride layers in composites10.1111/j.1151-2916.1999.tb01944.x ↗
41. High-temperature oxidation of boron nitride10.1016/S0272-8842(86)80006-2 ↗