Abstract

Abstract Oxidization of diamond in the sintering process of diamond/glass composites results in thermal degradation of diamond and uncontrolled expansion of the bulk composites with many irregular pores, causing low bending strength of the composites. In this paper, Ti powder was used as oxygen getter due to its excellent affinity with oxygen. The results showed the diamond grits got good protection from oxidation during sintering due to the prior reaction of Ti powder with oxygen. As a result, expansion phenomenon was inhibited and bending strength was improved for the composites due to the Ti additives. TiO 2 , as oxidization product of Ti, could enter into the glass network. The maximum bending strength and minimum volume expansion values were obtained for the composites with 6 wt.% Ti powder. This content resulted in a decrease of volume expansion from 22.78% to −25.0%, and an increase in bending strength from 28.49 MPa to 100.54 MPa.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Tunneling and Rock Mechanics · Diamond and Carbon-based Materials Research · Advanced materials and composites

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (18)

Show source-provided references
1. Diamond tool bits with iron alloys as the binding matrices10.1016/S0254-0584(01)00419-9 ↗
2. Diamond tools in stone and civil engineering industry: cutting principles, wear and applications10.1016/S0925-9635(01)00561-1 ↗
3. Interfacial characterization of Cu/diamond composites prepared by powder metallurgy for heat sink applications10.1016/j.scriptamat.2007.10.011 ↗
4. High-performance grinding—a review10.1016/j.jmatprotec.2005.04.010 ↗
5. Sintering parameters and wear performances of vitrified bond diamond grinding wheels10.1016/j.ijrmhm.2005.11.002 ↗
6. Grinding wheels for manufacturing of silicon wafers: a literature review10.1016/j.ijmachtools.2006.02.003 ↗
7. Study of the wettability between diamond abrasive and vitrified bond with low melting point and high strength10.4028/www.scientific.net/KEM.359-360.11 ↗
8. Influence of vitrified bond structure on radial wear of cBN grinding wheels10.1016/j.jmatprotec.2009.03.013 ↗
9. Appropriate conditioning strategies increase the performance capabilities of vitrified-bond CBN grinding wheels10.1016/S0007-8506(07)62331-2 ↗
10. Highly porous vitrified bonded abrasives by the selective extraction of butyl carbamate from green grinding wheels with supercritical CO210.1111/j.1551-2916.2005.00276.x ↗
11. Temperatures and energy partition for grinding with vitrified CBN wheels10.1016/S0007-8506(07)63176-X ↗
12. W. Hu, L. Wan, X. Liu, Q. Li, Z. Wang. Effect of TiO2/Al2O3 film coated diamond abrasive particles by sol–gel technique. doi:10.1016/j.apsusc.2011.01.101.10.1016/j.apsusc.2011.01.101 ↗
13. Effects of nano-AlN on phase transformation of low temperature vitrified bond during sintering process10.1016/S1003-6326(10)60136-7 ↗
14. Effect of Si coating on prevention of diamond degradation in diamond/glass composite10.1016/j.surfcoat.2010.02.068 ↗
15. Thermal residual stress analysis of coated diamond grits10.1016/S1674-4799(09)60036-4 ↗
16. Growth mechanism of nanometer-sized SiC and oxidation resistance of SiC-coated diamond particles10.1111/j.1551-2916.2004.00809.x ↗
17. Wettability and reactivity in diamond–borosilicate glass system10.1016/j.ijrmhm.2009.10.008 ↗
18. Effects of titanium coating on property of diamond10.1016/S1003-6326(07)60162-9 ↗