journal article·2006-01

Possibility of enhanced strength and self-recovery of surface damages of ceramics composites under oxidative conditions

Osami Abe, Yoshitaka Ohwa, Yo-ichiro Kuranobu

Publisher page

Abstract

Abstract Oxidation of NiAl/α-Al2O3 composites provides the metamorphic surface layers consisting of boundary NiAl2O4 and Al2O3 grains with compressive stress. Strengthening and toughening from 515 MPa and 4 MPa m1/2 (sintered) to ∼655 MPa and ∼6 MPa m1/2 (oxidized) are enabled by a controlled development of the metamorphic layers at 1200–1300 °C. The reactivity of an oxidation product, NiO, with the matrix-Al2O3 and the rapid diffusion along the grain boundary repairs the damages on surfaces by filling and re-bonding the defects and cracks. The oxidation further progresses via the repaired defects to develop the metamorphic layers supporting them to enhance the recovery of the strength. The degraded strength of the material with defects, 150 MPa, is recovered to 531 MPa by the reparation against the limited recovery to 343 MPa by a thermal healing in Ar.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Advanced ceramic materials synthesis · Advanced materials and composites · Aluminum Alloys Composites Properties

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (8)

Show source-provided references
1. Toughening of NiAl–alumina composites by self-constructed compressive surface layers under oxidation10.1016/S0955-2219(03)00201-2 ↗
2. Oxidation of NiAl/Al2O3 composites for controlled development of surface layers and toughening10.1016/j.ssi.2004.02.062 ↗
3. Strengthening of silicon carbide ceramics by surface nitridation during hot isostatic pressing10.1111/j.1151-2916.1992.tb05616.x ↗
4. Measurement of residual stress in oxide-ZrO2 three layer composites
5. Damage-resistant SiC–AlN layered composites with surface compressive stress10.1111/j.1151-2916.1992.tb05550.x ↗
6. Preparation of NiAl/Al2O3 composites10.4028/www.scientific.net/KEM.159-160.319 ↗
7. Intelligent alumina–NiAl material having sensitivity to oxidation damages
8. Crack healing in silicon carbide10.1111/j.1551-2916.2004.00490.x ↗