journal article·2019-04Open access

Transient and steady states of Gd2Zr2O7 and 2ZrO2∙Y2O3 (ss) interactions with calcium magnesium aluminium silicates

Sandrine Duluard, Elodie Delon, Jean-Pierre Bonino, André Malié, Aurélien Joulia, Luc Bianchi, Philippe Gomez, Florence Ansart

Publisher page

Abstract

Reactions between calcium magnesium aluminium silicates (CMAS) and Gd2Zr2O7 or 2ZrO2∙Y2O3 (ss) are investigated within a temperature range of 1200–1300 °C and for durations of 1 h–100 h. The evolution of CMAS penetration depth in Gd2Zr2O7 and 2ZrO2∙Y2O3 (ss) pellets varies considerably depending on the interaction time. A quantitative analysis of the nature and composition of phases observed in stationary conditions (powder/powder interaction) is performed by SEM-FEG coupled with WDS analyses using micro-agglomerated nanoparticles of Gd2Zr2O7 and 2ZrO2∙Y2O3. Faster kinetics of the gadolinium-based system are illustrated through an analysis of the morphology of the reaction area and of the resulting CMAS tightness of reaction products. The compositions and quantities of reaction products observed at equilibrium are very similar for the two systems, but transient states are significantly different.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Advanced ceramic materials synthesis · Nuclear materials and radiation effects · Magnesium Oxide Properties and Applications

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (59)

Show source-provided references
1. Some recent trends in research and technology of advanced thermal barrier coatings10.1016/S1270-9638(02)00003-2 ↗
2. EB-PVD thermal barrier coatings for aeroengines and gas turbines10.1002/1527-2648(200104)3:4<193::AID-ADEM193>3.0.CO;2-U ↗
3. Corrosion mechanisms of ZrO2-Y2O3 thermal barrier coatings in the presence of molten middle-east sand
4. Degradation of thermal-barrier coatings at very high temperatures10.1557/S0883769400048223 ↗
5. Role of environment deposits and operating surface temperature in spallation of air plasma sprayed thermal barrier coatings10.1016/S0257-8972(96)02994-5 ↗
6. Novel thermal barrier coatings that are resistant to high-temperature attack by glassy deposits10.1016/j.actamat.2007.08.028 ↗
7. Environmental stability of the YSZ layer and the YSZ/TGO interface of an in-service EB-PVD coated high-pressure turbine blade10.1007/s10853-008-3215-8 ↗
8. Microstructural characterization of the interaction between 8YPSZ (EB-PVD) thermal barrier coatings and a synthetic CAS10.1016/j.surfcoat.2013.11.014 ↗
9. Calcium-magnesium-alumino-silicate (CMAS) degradation of EB-PVD thermal barrier coatings: characterization of CMAS damage on ex-service high pressure blade TBCs10.1016/j.surfcoat.2012.07.074 ↗
10. Thermochemical interaction of thermal barrier coatings with molten CaO-MgO-Al2O3 -SiO2 (CMAS) deposits10.1111/j.1551-2916.2006.01209.x ↗
11. Mechanisms of cracking and delamination within thick thermal barrier systems in aero-engines subject to calcium-magnesium-alumino-silicate (CMAS) penetration10.1016/j.msea.2008.01.006 ↗
12. A delamination mechanism for thermal barrier coatings subject to calcium–magnesium–alumino-silicate (CMAS) infiltration10.1016/j.actamat.2004.11.028 ↗
13. Degradation of La2Zr2O7 and other novel EB-PVD thermal barrier coatings by CMAS (CaO–MgO–Al2O3–SiO2) and volcanic ash deposits10.1016/j.surfcoat.2013.07.029 ↗
14. Characterization of Eyjafjallajökull volcanic ash particles and a protocol for rapid risk assessment10.1073/pnas.1015053108 ↗
15. April-May 2010 Eyjafjallajökull volcanic fallout over Rimini, Italy10.1016/j.atmosenv.2011.05.018 ↗
16. Volcanic ash over Europe during the eruption of Eyjafjallajökull on Iceland, April-May 201010.1016/j.atmosenv.2011.03.054 ↗
17. Chellah · 2013
18. Step-by-step investigation of degradation mechanisms induced by CMAS attack on YSZ materials for TBC applications10.1016/j.surfcoat.2013.08.055 ↗
19. Gadolinium oxide solubility in molten silicate: dissolution mechanism and stability of Ca2Gd8(SiO4)6O2 and Ca3Gd2(Si3O9)2 silicate phases10.1016/j.jeurceramsoc.2017.02.022 ↗
20. Zirconates as new materials for thermal barrier coatings10.1111/j.1151-2916.2000.tb01506.x ↗
21. 2ZrO2 Y2O3 thermal barrier coatings resistant to degradation by molten CMAS: part I, optical basicity considerations and processing10.1111/jace.13210 ↗
22. Low-thermal-conductivity rare-earth zirconates for potential thermal-barrier-coating applications10.1111/j.1151-2916.2002.tb00574.x ↗
23. 2ZrO2∙Y2O3 (ss). (YZ)-pyrochlore based oxide as an electrolyte material for intermediate temperature solid oxide fuel cells (ITSOFCs)—Influence of Mn addition on YZ10.1016/j.matchemphys.2007.09.010 ↗
24. Phase relationships in the Y2O3-ZrO2 system10.1007/BF00908375 ↗
25. Thermal barrier coating materials10.1016/S1369-7021(05)70934-2 ↗
26. Equilibrium relationships between thermal barrier oxides and silicate melts10.1016/j.actamat.2016.08.077 ↗
27. 2ZrO2 Y2 O3 thermal barrier coatings resistant to degradation by molten CMAS: part II, interactions with sand and fly ash10.1111/jace.13209 ↗
28. Calcium-magnesium alumino-silicate interaction with yttrium monosilicate environmental barrier coatings: YMS interaction with YMS EBCs10.1111/j.1551-2916.2010.03916.x ↗
29. Effect of CMAS deposits on MOCVD coatings in the system Y2O3 -ZrO2 : phase relationships10.1111/jace.12502 ↗
30. Air plasma-sprayed yttria and yttria-stabilized zirconia thermal barrier coatings subjected to calcium-magnesium-alumino-silicate (CMAS)10.1007/s11666-014-0107-0 ↗
31. Phase equilibria and crystal chemistry in the calcia–silica–yttria system10.1016/j.jeurceramsoc.2016.01.046 ↗
32. Wang · 2016 · 151
33. CaO-MgO-Al2O3-SiO2 (CMAS) corrosion of Gd2Zr2O7 and Sm2Zr2O710.1149/2.0301610jes ↗
34. Phase equilibria in the calcia-gadolinia-silica system10.1016/j.jallcom.2016.10.263 ↗
35. Infiltration-inhibiting reaction of gadolinium zirconate thermal barrier coatings with CMAS melts10.1111/j.1551-2916.2007.02175.x ↗
36. Drexler · 2011
37. Composition effects of thermal barrier coating ceramics on their interaction with molten Ca-Mg-Al-silicate (CMAS) glass10.1016/j.actamat.2012.06.053 ↗
38. Comparison of oxidation behavior of YSZ and Gd2Zr2O7 thermal barrier coatings (TBCs)10.1016/j.surfcoat.2016.12.078 ↗
39. Zaleski · 2013
40. Evolution of hot corrosion resistance of YSZ, Gd2Zr2O7, and Gd2Zr2O7+YSZ composite thermal barrier coatings in Na2SO4+V2O5 at 1050°C10.1016/j.jeurceramsoc.2012.01.006 ↗
41. Effect of CMAS composition on hot corrosion behavior of gadolinium zirconate thermal barrier coating materials10.1149/2.0531709jes ↗
42. Characterization of microstructure and thermal properties of Gd2Zr2O7-type thermal barrier coating10.1016/j.jeurceramsoc.2011.11.043 ↗
43. Effect of changing the rare earth cation type on the structure and crystallization behavior of an aluminoborosilicate glass
44. Melting and crystallization of silicate systems relevant to thermal barrier coating damage10.1111/jace.13478 ↗
45. Interaction between ceramic powder and molten calcia-magnesia-alumino-silicate (CMAS) glass, and its implication on CMAS-resistant thermal barrier coatings10.1016/j.scriptamat.2015.09.027 ↗
46. CMAS corrosion of EB PVD TBCs: identifying the minimum level to initiate damage10.1016/j.ijrmhm.2009.07.005 ↗
47. Mohan · 2010
48. Pujol · 2014
49. Pouchou · Recherche Aerospatiale · 1984 · 3 · 167
50. Characterization of anion disorder in zirconate A2B2O7 compounds by Raman spectroscopy10.1111/j.1151-2916.1979.tb19107.x ↗
51. Does local disorder occur in the pyrochlore zirconates?10.1021/ic301677b ↗
52. Order-disorder transition in the Nd2-yYyZr2O7 system: probed by X-ray diffraction and Raman spectroscopy10.1016/j.jssc.2009.10.010 ↗
53. Order-disorder transition in Nd2-yGdyZr2O7 pyrochlore solid solution: an X-ray diffraction and Raman spectroscopic study10.1016/j.jssc.2007.07.007 ↗
54. Preparation and fluorite-pyrochlore phase transformation in Gd2Zr2O710.1016/j.jallcom.2009.08.021 ↗
55. Ab initio investigation of phase stability of Y2Ti2O7 and Y2Zr2O7 under high pressure10.1103/PhysRevB.80.212102 ↗
56. Volcanic ash-induced decomposition of EB-PVD Gd2Zr2O7 thermal barrier coatings to Gd-oxyapatite, zircon, and Gd, Fe-zirconolite
57. Effects of cation substitution and temperature on the interaction between thermal barrier oxides and molten CMAS10.1016/j.jeurceramsoc.2014.09.006 ↗
58. Stability and CMAS resistance of ytterbium-silicate/hafnate EBCs/TBC for SiC composites10.1111/jace.13262 ↗
59. Environmental degradation of thermal-barrier coatings by molten deposits10.1557/mrs.2012.230 ↗