Archaeological ceramic amphorae from underwater marine environments: Influence of firing temperature on salt crystallization decay
Source abstract
Abstract
Non-desalinated and desalinated fragments of Iberian, Italic and Tarraconensian amphorae sherds, found in different underwater marine environments, were compared to determine the decay caused by salt crystallization. Polarizing light and fluorescence optical microscopy, scanning electron microscopy coupled to energy dispersive X-ray spectroscopy, X-ray diffraction, ion chromatography and mercury intrusion porosimetry tests were conducted on the samples. Non-desalinated samples exhibit a variety of signs of degradation, especially those samples fired at lower temperature. Sherds fired at higher temperatures have a lower surface area and less connected porosity, which entail a lower absorption of soluble salts containing water and eventually less decay than those fired at lower temperatures. The composition and texture reached with the firing temperature is a key factor on salt crystallization decay and hence on the durability of these artefacts. This should be taken into account during desalination procedures that have to be optimized in order to be successful.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Building materials and conservation · Cultural Heritage Materials Analysis · Conservation Techniques and Studies
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (61)
Show source-provided references
1. Clay products
2. Winkler · 1994
3. Salt-induced decay in calcareous stone monuments and buildings in a marine environment in SW France10.1016/S0950-0618(02)00104-6 ↗
4. Analysis of calcium acetate efflorescences formed on ceramic tiles in a museum environment10.1016/j.culher.2006.09.004 ↗
5. Further studies of the thermal decomposition of clays
6. Las sales solubles en el deterioro de rocas monumentales10.3989/mc.1994.v44.i235.579 ↗
7. Thermodynamic modelling of changes induced by salt pressure crystallisation in porous media of stone10.1016/S0022-0248(99)00163-3 ↗
8. Role of pore structure in salt crystallisation in unsaturated porous stone10.1016/j.jcrysgro.2003.09.004 ↗
9. Soluble salt minerals from pigeon droppings as potential contributors to the decay of stone based cultural heritage10.1127/0935-1221/2004/0016-0505 ↗
10. Las sales y su incidencia en la conservación de la cerámica arqueológica
11. An experimental study of the effects of salt erosion on pottery10.1016/0305-4403(90)90004-O ↗
12. Kingery · 1976
13. Rice · 1987
14. El entorno marino de los restos arqueológicos
15. Magnesium sulfate salts and historic building materials: experimental simulation of limestone flaking by relative humidity cycling and crystallization of salts10.3989/mc.2008.v58.i289-290.77 ↗
16. Preservation strategies for avoidance of salt crystallization in El Paular Monastery cloister, Madrid, Spain10.1007/s12665-010-0733-x ↗
17. El Centre d’Arqueologia subaquàtica de Catalunya (CASC) i l’arqueologia subaquàtica a Catalunya
18. Tchernia · 1999 · 159
19. Vivar · 2007 · vol. 1 · 22
20. Residues and linnings in ancient Mediterranean transport amphoras
21. Fourier transform infrared spectroscopy as a suitable technique in the study of the materials used in waterproofing of archaeological amphorae10.1016/j.aca.2007.07.021 ↗
22. Wine and olive oil permeation in pitched and non-pitched ceramics: relation with results from archaeological amphorae from Sagalassos10.1016/j.jas.2008.11.024 ↗
23. Waterproofing materials used in Betic, Italic and Tarraconensian archaeological anphorae
24. Dissolution of salts crystallized in building materials using ultrasound: an alternative to NORMAL (1983) standard methodology10.1016/S1350-4177(00)00062-6 ↗
25. Hematite nucleation and growth in the firing of carbonate-rich clay for pottery production10.1016/j.jeurceramsoc.2007.03.031 ↗
26. Some notes on the firing colour of clay bricks10.1016/0169-1317(87)90007-X ↗
27. Bricks in historical buildings of Toledo City: characterization and restoration10.1016/S1044-5803(03)00101-3 ↗
28. Mineralogical applications of the analytical SEM in archaeology10.1180/minmag.1987.051.359.03 ↗
29. An approach to the dynamics of clay firing10.1016/S0169-1317(99)00032-0 ↗
30. Mineralogical and chemical composition of transport amphorae excavated at Locri Epizephiri (southern Italy)10.1016/S1296-2074(01)01120-7 ↗
31. Barker · 1998
32. Bard · 1986
33. Deer · 1963
34. The influence of temper shape on the mechanical properties of archaeological ceramics10.1016/j.jeurceramsoc.2010.04.039 ↗
35. Vernon · 2004 · 594
36. Naotake · 2003
37. Hydrotermal alteration and its relationship to ore fluid alteration
38. Thermal analysis as a method of characterizing ancient ceramic technologies10.1016/0040-6031(95)02570-7 ↗
39. Moessbauer study of the effect of calcium content on iron oxide transformations in fired clays10.1111/j.1151-2916.1981.tb09599.x ↗
40. Gehlenite-Akermanite series-(Melilite Group) in slags of high kiln
41. Weathering traces in ancient bricks from historical buildings10.1016/j.buildenv.2004.08.027 ↗
42. Mineralogical transformations of calcareous rich clays with firing: a comparative study between calcite and dolomite rich clays from Algarve, Portugal10.1016/j.clay.2008.02.008 ↗
43. Mineralogical changes during firing of calcium-rich bricks clays
44. High temperature reactions and use of Bronze Age pottery from La Mancha, Central Spain
45. Carbonate silicate phase reactions during ceramic firing10.1127/0935-1221/2001/0013-0621 ↗
46. Durability improvement of ancient bricks by cementation of porous media10.1111/j.1551-2916.2005.00466.x ↗
47. Contribution of analytical techniques to determining the technologies used in the ceramic materials from the Former Workers Hospital of Maudes, Madrid (Spain)10.1016/j.jeurceramsoc.2012.09.007 ↗
48. Modern techniques of analysis applied to ancient ceramics
49. DOE · 1994
50. Weast · 1985
51. Sulfur and iron speciation in recently recovered timbers of the Mary Rose revealed via X-ray absorption spectroscopy10.1016/j.jas.2007.09.007 ↗
52. Effect of humidity on pyrite oxidation
53. Sulfur and iron analyses of marine archaeological wood in shipwrecks from the Baltic Sea and Scandinavian waters10.1016/j.jas.2012.03.006 ↗
54. Formation of coral concretions on marine iron international10.1111/j.1095-9270.1976.tb00969.x ↗
55. Conservation of waterlogged timbers from the Batavia 1629
56. Deterioration of the seventeenth-century warship Vasa by internal formation of sulphuric acid10.1038/415893a ↗
57. Sandström · 2003 · vol. 19
58. Warren · 1999
59. Influence of mineralogy and firing temperature on the porosity of bricks10.1016/S0955-2219(03)00249-8 ↗
60. Influence of firing temperature and mineralogical composition on bending strength and porosity of ceramic tile bodies10.1016/j.clay.2008.01.005 ↗
61. Durability estimation of porous building stones from pore structure and strength10.1016/j.enggeo.2004.03.005 ↗