Joining of SiC by Al infiltrated TiC tape: Effect of joining parameters on the microstructure and mechanical properties
Source abstract
Abstract
Abstract SiC ceramics were successfully joined by Al infiltrated TiC tapes at 900–1100 °C for 0.5–2 h in vacuum. Phase constituents, microstructure and mechanical strength of the prepared SiC joints were characterized. The prepared SiC joints display dense interlayer and crack-free interface. The interlayer primarily consists of TiC and Al phases, together with small amount of TiAl3 and trace of Al4C3. With increasing the joining temperature or time, the interface layer either thickens or grows to multiple layers. The bending strengths of the SiC joints are higher than 190 MPa as bonded at present conditions, and are closely related with the property of interface and interlayer.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Advanced ceramic materials synthesis · Aluminum Alloys Composites Properties · Advanced materials and composites
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (29)
Show source-provided references
1. High-temperature materials: a general review10.1007/BF00576759 ↗
2. Material properties of a sintered alpha-SiC10.1063/1.556000 ↗
3. Joining of ceramics
4. Joining of engineering ceramics10.1179/174328009X461078 ↗
5. Thermodynamic brazing alloy design for joining silicon-carbide10.1111/j.1151-2916.1991.tb07799.x ↗
6. Advances in brazing of ceramics10.1007/BF01117909 ↗
7. Joining of ZrB2-based ultra-high-temperature ceramic composites using Pd-based braze alloys10.1016/j.scriptamat.2009.03.053 ↗
8. Modified tape casting method for ceramic joining-application to joining of silicon-carbide10.1111/j.1151-2916.1990.tb06760.x ↗
9. Joining of silicon-carbide/silicon-carbide composites and dense silicon-carbide using combustion reactions in the titanium–carbon–nickel system10.1111/j.1151-2916.1992.tb05454.x ↗
10. Joining of SiC to SiC using polyborosiloxane
11. Green state joining of silicon carbide using polycarbosilane10.1111/j.1151-2916.2000.tb01450.x ↗
12. Green state joining of SiC without applied pressure10.1111/j.1151-2916.2001.tb01039.x ↗
13. Effects of joining pressure and deformation on the strength and microstructure of diffusion-bonded silicon carbide10.1111/j.1151-2916.1992.tb07868.x ↗
14. Joining of SiC using reaction bonding methods
15. Reaction-infiltrated, net-shape SiC composites10.1016/0921-5093(94)06512-8 ↗
16. High temperature compressive mechanical behavior of joined biomorphic silicon carbide ceramics10.1016/S0955-2219(02)00138-3 ↗
17. Interfacial reactions between SiC and aluminum during joining10.1007/BF00563067 ↗
18. Survey on wetting of SiC by molten metals10.1016/j.ceramint.2010.01.001 ↗
19. The effect of pore size on the infiltration kinetics of aluminum in titanium carbide preforms10.1016/0956-7151(94)90192-9 ↗
20. Effect of composition and joining parameters on microstructure and mechanical properties of silicon carbide joints10.2109/jcersj2.118.799 ↗
21. Synthesis, microstructure and mechanical properties of reaction-infiltrated TiB2–SiC–Si composites10.1016/j.jallcom.2010.10.053 ↗
22. Image processing with ImageJ
23. In situ synthesis of TiC particulate-reinforced aluminum matrix composites10.1007/BF02670775 ↗
24. Reaction in Al–TiC metal matrix composites10.1016/S0921-5093(01)01228-X ↗
25. Reaction products of Al/TiC composites fabricated by the pressureless infiltration technique10.1007/s11661-005-0125-0 ↗
26. Microstructure and heat-treatment response of Al-2024/TiC composites10.1016/S0921-5093(00)00900-X ↗
27. Microstructural characterization of in situ TiC/Al and TiC/Al–20Si–5Fe–3Cu–1Mg composites prepared by spray deposition10.1016/S1359-6454(03)00292-1 ↗
28. Microstructure and microchemistry of the Al/SiC interface10.1007/BF00575416 ↗
29. Microstructure and interface characteristics of B4C, SiC and Al2O3 reinforced Al matrix composites: a comparative study10.1016/S0924-0136(03)00815-X ↗