Hydrothermal corrosion of zirconia-toughened alumina (ZTA) at 200°C
Source abstract
Abstract
Abstract To investigate the corrosion behaviour of zirconia-toughened alumina (ZTA) under hydrothermal corrosion, a commercial material was compared with materials of similar composition, but fabricated using different processing methods and pure alumina. The specimens were corroded at a temperature of 200 °C in deionised water. Generally, linear corrosion kinetics were found. Pure alumina shows the lowest mass loss and the smallest rate constants. The reduction of the four-point bending strength does not correlate with the mass loss. The main parameter for the degradation is the cubic/tetragonal to monoclinic transformation of zirconia. Investigation of the corrosion of polished surfaces reveals spallation of Al2O3 grains or groups of grains surrounded by zirconia as the main mechanism. A decrease in the size of zirconia grains helps to reduce the strength degradation.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Advanced ceramic materials synthesis · Advanced materials and composites · Nuclear materials and radiation effects
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (15)
Show source-provided references
1. Hydrothermal corrosion of alumina ceramics10.1111/j.1151-2916.1997.tb03258.x ↗
2. Corrosion of aluminium oxide in acids and caustic solutions
3. Corrosion behaviour of alumina ceramics in caustic alkaline solutions at high temperatures10.1111/j.1151-2916.1991.tb04304.x ↗
4. The corrosion behaviour of ceramic materials in caustic alkaline solutions at high temperature10.1016/0010-938X(92)90207-J ↗
5. Environmental degradation of zirconia ceramics10.1016/0955-2219(95)00035-S ↗
6. Corrosion of zirconia ceramics in acidic solutions at high pressures and temperatures10.1016/S0955-2219(98)00244-1 ↗
7. Aging behaviour of Y-TZP
8. Effects of liquid environments on zirconia-toughened alumina. Part II: mechanical properties10.1007/BF00540711 ↗
9. Examining the corrosion behaviour of Al2O3+10% ZrO2 in aqueous solutions
10. Keramische Wälzlager für Anwendungen in korrosiven Medien
11. Krell, A. and Blank, P., Hartstoffverstärkte stabilisierte ZrO2Keramik mit mechanischer Stabilität unter hydrothermaler Beanspruchung. Patent DE 19733700, 1999.
12. Processing of high-density submicrometer Al2O3 for new applications10.1111/j.1151-2916.2003.tb03339.x ↗
13. Seipel, B., Korrosion von Siliciumnitrid und Zirkonoxidverstärktem Aluminiumoxid in wässriger Lösung unter Durchflussbedingungen. Dissertation thesis, University Tuebingen, 2003.
14. 1993 · Vol 5
15. Corrosion behaviour of different technical ceramics in acids, basic solutions and under hydrothermal conditions10.4028/www.scientific.net/KEM.264-268.877 ↗