journal article·2002-12

Apparent activation energy of fused silica optical fibers in static fatigue in aqueous environments

Y.S. Shiue, M.J. Matthewson

Publisher page

Abstract

Static fatigue of fused silica optical fiber is known to be caused by stress assisted reaction of silica with ambient moisture. Past studies have often been conducted in hot water to accelerate experiments compared with cooler vapor environment. However, changes in the pH of water with temperature has an important influence on the fatigue rate, but has been ignored in the literature. To study the effect of pH, static fatigue of fused silica fibers has been characterized over a range of temperatures in both distilled water and pH 7 buffer solution. The apparent activation energies were then obtained for the different environments. The silica fibers were found to fatigue faster in pH 7 buffer solution than in distilled water, and the apparent activation energy for fatigue was higher in pH 7 buffer. The difference in the results for the two environments can be understood in terms of the difference in their pH and how the pH varies with temperature.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Advanced Fiber Optic Sensors · Glass properties and applications · Photonic Crystal and Fiber Optics

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (27)

Show source-provided references
1. Static fatigue of glass I10.1063/1.1722991 ↗
2. A molecular mechanism for stress corrosion in vitreous silica10.1111/j.1151-2916.1983.tb15715.x ↗
3. The effect of environment on the strength of optical fiber
4. Charles, R. J. and Hillig, W. B. The Kinetics of Glass failure by stress corrosion. Proc. Symp. sur la Resistance Mechanique du verre at le Moyens d l'Ameliorer, Union Sciences Continentale du Verre, Charleroi Belgium, 1962 pp. 1–17
5. Stress corrosion and static fatigue of glass10.1111/j.1151-2916.1970.tb15962.x ↗
6. Chemical kinetics models for the fatigue behavior of fused silica optical fiber10.1557/PROC-531-143 ↗
7. Dynamic Fatigue of Glass10.1063/1.1723019 ↗
8. Slow crack growth in brittle materials under dynamic loading conditions10.1007/BF00113930 ↗
9. An atomistic model of kinetic crack growth in brittle solids10.1007/BF00543692 ↗
10. Dependency of fatigue predictions on the form of the crack velocity equation10.1111/j.1151-2916.1981.tb10305.x ↗
11. Optical fiber reliability models
12. Summary of stress-dependent activation energy for lightguide fibers10.1111/j.1151-2916.1992.tb04456.x ↗
13. Pearson · 1981
14. A chemical interpretation of static fatigue10.1111/j.1151-2916.1972.tb11215.x ↗
15. Temperature dependence of the transition in static fatigue of fused silica optical fiber10.1111/j.1551-2916.1988.tb00183.x ↗
16. Molecular mechanisms for corrosion of silica and silicate glasses10.1016/0022-3093(94)90708-0 ↗
17. Effect of pH on the strength and fatigue behavior of fused silica optical fiber 47th Int
18. Activation energy for strength degradation of fused silica optical fibers10.1557/PROC-531-175 ↗
19. Environmental effects on the static fatigue of silica optical fiber10.1111/j.1151-2916.1988.tb05025.x ↗
20. Technique for the static fatigue testing of fibers10.1111/j.1151-2916.1987.tb04986.x ↗
21. Static fatigue of optical fibers in bending10.1111/j.1151-2916.1987.tb05736.x ↗
22. Acid stripping of fused silica optical fibers without strength degradation10.1109/50.557565 ↗
23. The effect of diffusion rates in optical fiber polymer coatings on aging10.1117/12.372786 ↗
24. Yuce, H. H., Varachi J. P. Jr., Kilmer, J. P., Kurkjian, C. R. and Matthewson, M. J., Optical fiber corrosion: coating contribution to zero-stress aging OFC'92 Tech. Digest, 1992, PD21 395–399.10.1364/OFC.1992.PD21 ↗
25. Lawn · 1993
26. Optical fibre and cables
27. Temperature dependence of static fatigue of optical fibers coated with a UV-curable polyurethane acrylate10.1111/j.1151-2916.1982.tb10389.x ↗