Abstract The reaction-bonding method is used to fabricate a dense SiC sintered body by filling a SiC preformed structure with a molten Si. Reaction-bonded SiC has both excellent mechanical strength and high-temperature corrosion resistance; however, a low fracture toughness and low melting point of the residual Si constitute major drawbacks of this material. Therefore, in this study, in order to improve the mechanical properties of the reaction-bonded SiC, the composition of the matrix phase was modified by using a preform that is composed of TiC powder. Two types of matrix phases (TiSi 2 and Ti 3 SiC 2 ) were developed, depending on the amounts of reacted TiC and Si. Ti 3 SiC 2 was formed at a TiC to Si molar ratio of 3:2, and TiSi 2 was obtained with increasing amount of Si. The fracture toughness (7.4 MPa√m) of reaction-bonded SiC consisting of the Ti 3 SiC 2 matrix phase was higher than that (3.0 MPa√m) of the the conventional reaction-bonded SiC. However, the resistance to high-temperature steam oxidation at 1200 °C decreased when TiSi 2 and Ti 3 SiC 2 were substituted for Si as the matrix phase.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Advanced ceramic materials synthesis · MXene and MAX Phase Materials · Aluminum Alloys Composites Properties

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (25)

Show source-provided references
1. Kinetics and mechanisms of high-temperature creep in silicon carbide: I, reaction-bonded10.1111/j.1151-2916.1984.tb19726.x ↗
2. Mechanism of deformation of silicon nitride and silicon carbide at high temperature10.1016/S0955-2219(99)00121-1 ↗
3. Behavior of SiC at high temperature under helium with low oxygen partial pressure10.1016/j.jeurceramsoc.2008.04.032 ↗
4. Handbook of SiC properties for fuel performance modeling10.1016/j.jnucmat.2007.05.016 ↗
5. Stability of SiC and its composites at high neutron fluence10.1016/j.jnucmat.2010.12.088 ↗
6. Fabrication and material issues for the application of SiC composites to LWR fuel cladding10.5516/NET.07.2012.084 ↗
7. Development of high-strength reaction-sintered silicon carbide10.1016/S0925-9635(03)00066-9 ↗
8. The effect of SiC powder size at reaction bonded SiC composite fabricated by a molten Si infiltration method10.4191/KCERS.2008.45.8.486 ↗
9. Influence of resin content and compaction pressure on the mechanical properties of SiC-Si composites with sub-micron SiC microstructures10.1016/S0955-2219(00)00281-8 ↗
10. Formation of dense silicon carbide by liquid silicon infiltration of carbon with engineered structure10.1557/JMR.2008.0167 ↗
11. Preparation of reaction bonded silicon carbide (RBSC) using boron carbide as an alternative source of carbon10.1016/j.jeurceramsoc.2010.11.032 ↗
12. Microstructure and mechanical properties of RB-SiC/MoSi2 composite10.1007/BF01168987 ↗
13. Liquid-phase reaction-bonding of silicon carbide using alloyed silicon-molybdenum melts10.1111/j.1151-2916.1990.tb05179.x ↗
14. Reaction-formed silicon carbide10.1016/0921-5093(91)90210-E ↗
15. High-temperature compressive strength of reaction-formed silicon carbide (RFSC) ceramics10.1016/S0955-2219(97)00107-6 ↗
16. Microstructure and mechanical properties of in situ produced SiC/TiSi2 nanocomposites10.1016/S0955-2219(99)00157-0 ↗
17. Synthesis of Ti3SiC2/SiC and TiSi2/SiC composites using displacement reactions in the Ti–Si–C system10.1016/1359-6462(95)00663-X ↗
18. Effect of the amounts of silicon on the in situ synthesis of Ti3SiC2 based composites made from TiC/Si powder mixtures10.1016/j.ceramint.2009.07.029 ↗
19. Three-dimensional printing of Ti3SiC2-based ceramics10.1111/j.1551-2916.2010.04257.x ↗
20. Fatigue-crack growth and fracture properties of coarse and fine-grained Ti3SiC210.1016/S1359-6462(99)00427-3 ↗
21. Ti3SiC2: a damage tolerant ceramic studied with nano-indentations and transmission electron microscopy10.1016/S1359-6454(03)00091-0 ↗
22. Oxidation kinetics of Zircaloy-4 and Zr-1Nb-1Sn-0.1Fe at temperatures of 700–1200°C10.1016/j.jnucmat.2004.08.007 ↗
23. A fracture mechanics analysis of indentation-induced Palmqvist crack in ceramics10.1007/BF00725625 ↗
24. Dense WSi2 and WSi2-20 vol.% ZrO2 composite synthesized by pressure-assisted field-activated combustion10.1016/S0925-8388(01)01167-7 ↗
25. High temperature oxidation behavior of Ti3SiC2-based material in air10.1016/S1359-6454(01)00247-6 ↗