Abstract
Abstract Silicon carbide fibers combine structural and refractory properties making them good candidates for ceramic matrix composite reinforcement, driving their ultimate failure. The fractographic observation after tensile tests of various silicon carbide fibers, belonging to first, second or third generations, reveals the critical flaw location i.e. internal or surface. An etching treatment under pure chlorine at 500–850 °C can be used to transform the fibers surface on hundreds of nanometers and alter the surface-located flaw population. This way, first-generation SiC-based fibers successfully show an asymptotic improvement of tensile strength (up to 60%) and Weibull modulus (up to twice), when etched on 0.3–1 μm depth range. The lifetime of bundles, under static fatigue conditions at intermediate temperature, is consequently multiplied by a factor ranging from 10 to 40 with a narrower dispersion. Nevertheless, the tensile strength could neither be increased on second-generation Hi-Nicalon nor dramatically dropped on third-generation Hi-Nicalon-S fiber.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Advanced ceramic materials synthesis · Silicon Nanostructures and Photoluminescence · Advanced Surface Polishing Techniques
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (29)
Show source-provided references
1. The design of the fibre-matrix interfacial zone in ceramic matrix composites10.1016/S1359-835X(97)00128-0 ↗
2. Delayed failure at intermediate temperature (600°–700°C) in air in silicon carbide multifilament tows10.1111/j.1551-2916.2004.00888.x ↗
3. Damage and failure in ceramic–matrix minicomposites: experimental study and model10.1016/S1359-6454(96)00224-8 ↗
4. Failure of fibres bundles10.1016/j.compscitech.2003.07.003 ↗
5. Delayed failure of Hi-Nicalon and Hi-Nicalon S multifilament tows and single filaments at intermediate temperatures (500°–800°C)10.1111/j.1551-2916.2009.02924.x ↗
6. Reinforcement of ceramic matrix composites: properties of SiC-based filaments and tows
7. Recent developments of the SiC fiber Nicalon and its composites, including properties of the SiC fiber Hi-Nicalon for ultra-high temperature10.1016/0266-3538(94)90184-8 ↗
8. A review of the development of three generations of small diameter silicon carbide fibres10.1007/s10853-006-6566-z ↗
9. High temperature strength and oxidation resistance of newly developed SiC fibers
10. Fabrication and mechanical properties of new improved Si-M-C-(O) Tyranno fiber10.1002/9780470294482.ch8 ↗
11. Statistical analysis of failure of SiC fibres in the presence of bimodal flaw populations10.1023/A:1018600119250 ↗
12. Mazerat · 2012
13. Crack branching and fracture mirror data of glasses and advanced ceramics
14. Contribution to the understanding of the microstructure of first generation Si-C-O fibers
15. Bias in the Weibull strength estimation of a SiC fiber for the small gauge length case
16. Characterization of Nicalon fibres with varying diameters part I strength and fracture studies10.1023/A:1004343608115 ↗
17. Advances in ceramic-matrix composites III
18. Strength and fracture properties of advanced SiC-based fibers10.1007/s11029-006-0063-y ↗
19. Tensile strength and fracture surface characterization of Hi-Nicalon SiC fibers10.1016/S0022-3115(00)00675-9 ↗
20. Carbon coatings on silicon carbide by reaction with chlorine-containing gases10.1039/a701126a ↗
21. Formation of carbon coating on SiC fibers by selective etching in halogens and supercritical water10.1002/9780470294482.ch10 ↗
22. Conversion of silicon carbide to crystalline diamond-structured carbon at ambient pressure10.1038/35077031 ↗
23. Kinetics of conversion of silicon carbide to carbide derived carbon10.1088/0953-8984/18/32/S07 ↗
24. Carbide derived carbon (CDC) coatings for Tyranno ZMI SiC fibers10.1002/9780470294802.ch8 ↗
25. In-situ processing of carbon coating on the surface of SiC-based fibers10.1016/j.surfcoat.2010.07.060 ↗
26. Delcamp · 2008
27. Composition and reactivity of various silicon carbide fibers10.1002/9781118932995.ch13 ↗
28. Study of Nicalon-based ceramic fibres and powders by EXAFS spectrometry, X-ray diffractometry and some additional methods10.1007/BF02397093 ↗
29. Evidence of silicon oxycarbide phase in the Nicalon silicon fiber10.1007/BF00660966 ↗