Delayed failure of ceramic matrix composites in tension at elevated temperatures
Source abstract
Abstract
Abstract Ultimate tensile strength of five different continuous fiber-reinforced ceramic matrix composites (CMCs), including SiCf/BSAS (two dimensional (2D), 2 types), SiCf/MAS (2D), SiCf/SiC (2D), and Cf/SiC (2D, 2 types), was determined as a function of test rate at 1100–1200 °C in air. All five CMCs exhibited a significant dependency of ultimate tensile strength on test rate such that the ultimate tensile strength decreased with decreasing test rate. The dependency of ultimate tensile strength on test rate, the applicability of preload technique, and the predictability of life from one loading configuration (constant stress-rate loading) to another (constant stress loading) all suggested that the overall, phenomenological delayed failure of the CMCs would be governed by a power-law type of slow crack growth.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Advanced ceramic materials synthesis · Advanced materials and composites · Concrete and Cement Materials Research
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (19)
Show source-provided references
1. Effect of load rate on tensile strength of various CFCCs at elevated temperatures: an approach to life-prediction testing10.1002/9780470294680.ch69 ↗
2. Fabrication of fiber-reinforced celsian matrix composites10.1016/S1359-835X(00)00169-X ↗
3. Worthem, D. W., Thermomechanical Fatigue Behavior of Three CFCC’s, NASA CR-195441. NASA Glenn Research Center, Cleveland, OH, 1995.
4. Stress/life behavior of a C/SiC composite in a low partial pressure of oxygen environment: I—Static strength and stress rupture database10.1002/9780470294741.ch51 ↗
5. ASTM C 1359, Standard test method for monotonic tensile strength testing of continuous fiber-reinforced advanced ceramics with solid rectangular cross-section specimens at elevated temperatures. In Annual Book of ASTM Standards (Vol 15.01). ASTM, West Conshohocken, PA, 2001.
6. Fatigue strength as a function of preloading in dynamic fatigue testing of glass and ceramics10.1115/1.2817011 ↗
7. Effect of preloading on fatigue strength in dynamic fatigue testing of ceramic materials at elevated temperatures10.1002/9780470314715.ch8 ↗
8. The influence of temperature, stress, and environment on the oxidation and life of C/SiC composites10.1002/9780470294741.ch49 ↗
9. Stress/life behavior of C/SiC composites in a low partial pressure of oxygen environment. II—Stress rupture life and residual strength relationship10.1002/9780470294741.ch52 ↗
10. Slow crack growth in brittle materials under dynamic loading conditions10.1007/BF00113930 ↗
11. ASTM C 1368, Standard test method for determination of slow crack growth parameters of advanced ceramics by constant stress-rate flexural testing at ambient temperature. In Annual Book of ASTM Standards (Vol 15.01). ASTM, West Conshohocken, PA, 2001.
12. ASTM C 1465, Standard test method for determination of slow crack growth parameters of advanced ceramics by constant stress-rate flexural testing at elevated temperatures. In Annual Book of ASTM Standards (Vol 15.01). ASTM, West Conshohocken, PA, 2001.
13. Ultra-fast fracture strength of advanced structural ceramics at elevated temperatures: an approach to high-temperature “inert” strength
14. Modeling the oxidation of carbon fibres in a C/SiC composite under stressed oxidation10.1002/9780470294741.ch50 ↗
15. Effect of loading rate on the monotonic tensile behavior of a continuous-fiber-reinforced glass–ceramic matrix composite10.1111/j.1151-2916.1996.tb08122.x ↗
16. Curtin, W. A. and Halverson, H. G., High Temperature Deformation and Failure in Oxide/oxide Composites, HITEMP Review 1999: Advanced High Temperature Engine Materials Technology Project (NASA/CP—1999-208915/Vol 2, Paper 48). NASA Glenn Research Center, Cleveland, OH, 1999.
17. Environmentally induced time-dependent failure mechanisms in CFCCs at elevated temperatures10.1002/9780470294499.ch2 ↗
18. Subcritical crack growth in CVI silicon-carbide reinforced with Nicalon fibers—experiment and model10.1111/j.1151-2916.1994.tb04609.x ↗
19. Stress–corrosion cracking in a unidirectional ceramic-matrix composite10.1111/j.1151-2916.1994.tb07030.x ↗