Abstract In this study, silicon carbide fibre-reinforced Ti3AlC2 matrix composites with a Ti barrier layer were prepared by hot-pressing at 1250 °C and 1300 °C. The microstructure of the composites was characterised by field-emission scanning electron microscopy. During consolidation, reactions of Ti with the fibres and the matrix led to the formation of an interfacial reaction zone between the fibres and the matrix and a matrix reaction zone within the matrix. Quantitative elemental distribution maps of both reaction zones were collected using energy-dispersive spectroscopy. The results revealed that the Ti layer effectively hindered the inward diffusion of Al from the matrix. In addition, the flexural strength of the composite was significantly improved with the addition of the Ti layer. Furthermore, noncatastrophic fracture behaviour was observed for the composites. The improvement of their mechanical behaviour is attributed to the added Ti layer, which prevented strength degradation of the fibres via a severe interface reaction.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: MXene and MAX Phase Materials · Aluminum Alloys Composites Properties · Advanced ceramic materials synthesis

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (36)

Show source-provided references
1. The MN+1AXN phases: a new class of solids; thermodynamically stable nanolaminates10.1016/S0079-6786(00)00006-6 ↗
2. The MAX phases: unique new carbide and nitride materials10.1511/2001.28.736 ↗
3. Progress in research and development on MAX phases: a family of layered ternary compounds10.1179/1743280410Y.0000000001 ↗
4. Layered machinable ceramics for high temperature applications10.1016/S1359-6462(96)00418-6 ↗
5. Preparation of high strength Ti3AlC2 by spark plasma sintering10.1111/ijac.12254 ↗
6. Shell-like nanolayered Nb4AlC3 ceramic with high strength and toughness10.1016/j.scriptamat.2010.12.045 ↗
7. Ab initio study of irradiation tolerance for different M(n+1)AX(n) phase: Ti3SiC2 and Ti3AlC210.1063/1.4861384 ↗
8. Preparation and microwave absorption properties of Ti3AlC2 synthesized by pressureless sintering TiC/Ti/Al10.1111/ijac.12275 ↗
9. Fabrication, mechanical properties and tribological behaviours of Ti3Al0. 8Sn0. 4C2 solid solution by two-time hot-pressing method10.1111/ijac.12265 ↗
10. Synthesis and characterization of Ti3AlC210.1111/j.1151-2916.2000.tb01281.x ↗
11. Mechanical properties of the MAX phases
12. In situ synthesis and properties of Ti3AlC2/TiB2 composites10.1111/j.1551-2916.2007.01954.x ↗
13. Effect of Al2O3 on the microstructure and mechanical properties of Ti3AlC2/Al2O3 in situ composites synthesized by reactive hot pressing10.1016/j.ceramint.2012.03.060 ↗
14. In situ processing and high-temperature properties of Ti3Si(Al)C2/SiC composites10.1111/j.1744-7402.2006.02057.x ↗
15. In situ reaction synthesis, electrical and thermal, and mechanical properties of Nb4AlC310.1111/j.1551-2916.2008.02424.x ↗
16. Mechanical properties of Cr2AlC ceramics10.1111/j.1551-2916.2007.01634.x ↗
17. Crystal structure of V4AlC3: a new layered ternary carbide10.1111/j.1551-2916.2007.02136.x ↗
18. Concept for a damage-tolerant ceramic composite with a strong interfaces10.1111/j.1151-2916.1996.tb08138.x ↗
19. Damage and failure in unidirectional ceramic–matrix composites10.1111/j.1151-2916.1992.tb05495.x ↗
20. Phase evaluation in Al2O3 fibre-reinforced Ti2AlC during sintering in the 1300°C–1500°C temperature range10.1111/j.1551-2916.2011.04612.x ↗
21. The reactivity of Ti2AlC and Ti3SiC2 with SiC fibres and powders up to temperatures of 1550°C10.1111/j.1551-2916.2010.04332.x ↗
22. SiC(SCS-6) fibre-reinforced Ti3AlC2 matrix composites: interfacial characterization and mechanical behaviour10.1016/j.jeurceramsoc.2014.11.034 ↗
23. The microstructure of SCS-6 SiC fibre10.1557/JMR.1991.2234 ↗
24. Microstructure and role of outermost coating for tensile strength of SiC fibre10.1016/S1359-6454(98)00181-5 ↗
25. Continuous silicon carbide fibre MMCs
26. S.Q. Guo, SiC fibres-containing hybrid composites and their fabrication method, Japan Patent No. 2015-167721. (JapanesePatent pending).
27. Thermal stability of Ti3AlC2/Al2O3 composites in high vacuum10.1016/j.matchemphys.2007.02.091 ↗
28. In situ high temperature diffraction study of the thermal dissociation of Ti3AlC2 in vacuum10.1111/j.1551-2916.2010.03764.x ↗
29. Stability and selective oxidation of aluminum in nano-laminate Ti3AlC2 upon heating in argon10.1021/cm030022v ↗
30. Fibre-matrix reaction zone growth kinetics in SiC-reinforced Ti-6Al-4V as studied by transmission electron microscopy
31. Ti-6Al-4V-2Ni as a matrix material for a SiC-reinforced composite10.1007/BF02647087 ↗
32. Fibre/matrix interface reactions in SiC reinforced titanium alloys
33. Microstructural characterization of interface in SiC fibre-reinforced Ti-15-3 matrix composite10.1016/S0921-5093(97)00737-5 ↗
34. Phase formation during ball milling and subsequent thermal decomposition of Ti–Al–Si powder blends10.1016/S0925-8388(96)02720-X ↗
35. Studies of titanium aluminide composites containing metallic fibre/matrix interface layer
36. Residual stresses, strength and toughness of laminates with different layer thickness ratios10.1016/j.actamat.2006.06.008 ↗