The structural and mechanical characterization of TiC and TiC/Ti thin films grown by DC magnetron sputtering
Source abstract
Abstract
Abstract The formation of TiC and Ti phases and their influence on their mechanical properties was studied in this work. Thin layers were deposited by DC magnetron sputtering at room temperature in ultrahigh vacuum from Ti and C targets. Cubic TiC phase (c-TiC) was formed from 58 to 86 at.% Ti content. First formation of hexagonal Ti (h-Ti) occurred from 86 at.% Ti content. The c-TiC disappears from 90 at.% Ti content. Films with 86 at.% Ti content the c-TiC structure can transform to h-Ti by sequential stacking faults. Dominance of c-TiC(111) texture with increasing Ti content was observed. The hardness of thin films agree with structural observations. The highest hardness value (∼26 GPa) showed the c-TiC thin film with 67 at% Ti content. The nanohardness values showed decreasing character with increasing Ti content over 70 at.%. The lowest values of nanohardness (∼10 GPa) was observed for thin films with only h-Ti phase.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Metal and Thin Film Mechanics · Advanced materials and composites · Copper Interconnects and Reliability
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (29)
Show source-provided references
1. Nanocomposite TiC/a–C:H hard coatings deposited by reactive PVD10.1016/S0257-8972(00)00888-4 ↗
2. Nanostructural and mechanical properties of nanocomposite nc-TiC/a-C:H films deposited by reactive unbalanced magnetron sputtering10.1063/1.1650898 ↗
3. Evaluation of phase, composition, microstructure and properties in TiC/a-C:H thin films deposited by magnetron sputtering10.1016/j.apsusc.2004.05.278 ↗
4. Microstructure and tribological properties of magnetron sputtered nc-TiC/a-C nanocomposite10.1016/j.surfcoat.2004.10.041 ↗
5. Nanostructured TiC/a-C coatings for low friction and wear resistant applications10.1016/j.surfcoat.2004.10.106 ↗
6. Mechanical and tribological properties of TiC/amorphous hydrogenated carbon composite coatings fabricated by DC magnetron sputtering with and without sample bias10.1016/j.diamond.2006.05.010 ↗
7. Depth profile analyses of nc-TiC/a-C:H coating prepared by balanced magnetron sputtering10.1016/j.surfcoat.2011.02.038 ↗
8. Evaluation of composition, mechanical properties and structure of nc-TiC/a-C:H coatings prepared by balanced magnetron sputtering10.1016/j.surfcoat.2011.09.012 ↗
9. On the effect of the substrate to target position on the properties of titanium carbide/carbon coatings10.1016/j.surfcoat.2017.06.076 ↗
10. Preparation of TiC films by alternate deposition of Ti and C layers using a dual magnetron sputtering source10.1016/S0257-8972(99)00388-6 ↗
11. Deposition of TiC films by dual source dc magnetron sputtering10.1016/S0042-207X(00)00341-9 ↗
12. Effects of residual stress on the mechanical and structural properties of TiC thin films grown by RF sputtering10.1016/j.surfcoat.2004.06.017 ↗
13. Ceramic TiC/a:C protective nanocomposite coatings: structure and composition versus mechanical properties and tribology10.1016/j.ceramint.2016.04.164 ↗
14. Mechanical behavior of bioactive TiC nanocomposite thin films10.4028/www.scientific.net/MSF.729.296 ↗
15. TiC coatings prepared by pulsed laser deposition and magnetron sputtering10.1016/S0257-8972(96)03124-6 ↗
16. Magnetron sputtering of hard nanocomposite coatings and their properties10.1016/S0257-8972(01)01139-2 ↗
17. TiC crystallite formation and the role of interfacial energies on the composition during the deposition process of TiC/a:C thin films10.1016/j.surfcoat.2016.06.047 ↗
18. Examination of nanocrystalline TiC/amorphous C deposited thin films10.1016/j.jeurceramsoc.2013.12.006 ↗
19. Carbon-metal (Ni or Ti) nanocomposite thin films for functional applications10.1016/j.solidstatesciences.2009.05.018 ↗
20. An improved technique for determining hardness and elastic modulus using load and displacement sensing indentation experiments10.1557/JMR.1992.1564 ↗
21. Measurement of hardness and elastic modulus by instrumented indentation: advances in understanding and refinements to methodology10.1557/jmr.2004.19.1.3 ↗
22. Electron diffraction based analysis of phase fractions and texture in nanocrystalline thin films, part I: principles10.1017/S1431927608080380 ↗
23. Electron diffraction based analysis of phase fractions and texture in nanocrystalline thin films, part II: implementation10.1017/S1431927609090023 ↗
24. Electron diffraction based analysis of phase fractions and texture in nanocrystalline thin films, part III: application examples10.1017/S1431927611012803 ↗
25. Advanced mechanical properties of pure titanium with ultrafine grained structure10.1016/S1359-6462(01)01089-2 ↗
26. Structure of metals, third edition: crystallographic methods
27. Tribologically transformed structure of titanium alloy (TiAl6V4) in surface fatigue induced by repeated impacts10.1016/j.msea.2004.10.008 ↗
28. Fundamental structure forming phenomena of polycrystalline films and the structure zone models10.1016/S0040-6090(97)00503-8 ↗
29. Structural evolution and optical properties of TiO2 thin films prepared by thermal oxidation of sputtered Ti films10.1063/1.1309039 ↗