Diffusion study of rare-earth oxides into silica layer for environmental barrier coating applications
Source abstract
Abstract
Abstract The effect of exposure temperature and time on the diffusion rate of rare-earth oxides applied on silicon carbide fiber-reinforced SiC ceramic matrix composites (SiC/SiC CMCs) have been investigated. Knowledge on diffusion mechanism between the deposited rare-earth (RE) slurry and silica layer is necessary to understand the process governing EBCs formation and their properties. SEM/EDS analysis were used to study the effect of microstructure on diffusivity. The diffusion coefficient increases with increasing sintering temperature and time. The measured diffusion coefficients of the RE-coating into silica layer were in the order of 10−15-10-17 m2/s revealing an overall good adhesion on the SiC/SiC CMCs.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Advanced ceramic materials synthesis · Magnesium Oxide Properties and Applications · Recycling and utilization of industrial and municipal waste in materials production
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (30)
Show source-provided references
1. 4.4.2 protective coatings for gas turbines
2. Rare earth silicate environmental barrier coatings for SiC/SiC composites and Si3N4 ceramics10.1016/j.jeurceramsoc.2004.12.013 ↗
3. Corrosion of silicon‐based ceramics in combustion environments10.1111/j.1151-2916.1993.tb03684.x ↗
4. Spitsberg · 2013
5. Alumina base coatings for protection of SiC ceramics10.1007/BF02834067 ↗
6. New generation of plasma-sprayed mullite coatings on Silicon Carbide10.1111/j.1151-2916.1995.tb08236.x ↗
7. Upper temperature limit of environmental barrier coatings based on mullite and BSAS10.1111/j.1151-2916.2003.tb03466.x ↗
8. Elastic Modulus evolution and behavior of Si/Mullite/BSAS-Based environmental barrier coatings exposed to high temperature in water vapor environment
9. Thermal properties of rare-earth monosilicates for EBC on Si-Based ceramic composites10.1111/jace.13982 ↗
10. Modeling of thermal residual stress in environmental barrier coated Fiber reinforced ceramic matrix composite10.1177/0021998311414950 ↗
11. Design of thermally reliable environmental barrier coating for a SiC/SiC ceramic matrix composites
12. Study of silver diffusion in silicon carbide10.1016/j.jnucmat.2009.02.022 ↗
13. Silver diffusion in coated fuel particles10.1111/j.1551-2916.2010.04055.x ↗
14. Maclean · 2004
15. Diffusion of fission products and radiation damage in SiC
16. Silver diffusion in silicon carbide coatings10.1111/j.1551-2916.2011.04544.x ↗
17. Grain boundary diffusion of Ag through polycrystalline SiC in TRISO fuel particles10.1016/j.jnucmat.2015.09.054 ↗
18. Preliminary results of post-irradiation examination of the AGR-1 TRISO fuel compacts
19. First elevated-temperature performance testing of coated particle fuel compacts from the AGR-1 irradiation experiment10.1016/j.nucengdes.2013.11.021 ↗
20. Comparison of diffusion coefficients and activation energies for Ag diffusion in Silicon Carbide10.1016/j.net.2015.05.004 ↗
21. Microstructure of TRISO coated particles from the AGR-1 experiment: SiC grain size and grain boundary character10.1016/j.jnucmat.2012.08.052 ↗
22. Shewmon · 1989
23. Ag diffusion in cubic silicon carbide10.1016/j.jnucmat.2010.10.088 ↗
24. Silver and cesium diffusion dynamics at the β‐SiC Σ5 grain boundary investigated with density functional theory molecular dynamics and metadynamics10.1021/jp411156c ↗
25. Diffusion of Ag along 3 grain boundaries in 3C-SiC10.1103/PhysRevB.84.214104 ↗
26. Grain boundary excess free volume - direct thermodynamic measurement10.1007/s10853-006-0563-0 ↗
27. Oxidation behaviour of SiC/SiC ceramic matrix composites in air10.1016/j.jeurceramsoc.2016.05.051 ↗
28. Al Nasiri · 2017
29. Interaction of yttrium disilicate environmental barrier coatings with calcium-magnesium-iron alumino-silicate melts10.1016/j.actamat.2017.12.004 ↗
30. Evaluation of silver transport through SiC during the German HTR fuel program10.1016/j.jnucmat.2009.09.024 ↗