Oxidation resistance of B6O-materials with different additives
Source abstract
Abstract
Abstract The oxidation resistance of B6O materials with and without Y2O3/Al2O3 additives and a typical cBN material were analysed in dry and wet air using TG measurements for up to 10 h and static experiments in a muffle furnace for up to 50 h. The results showed that the oxidation of the materials is sensitive to the composition of the atmosphere. In wet air with 17 vol.% H2O a weight loss was measured for all materials. In dry air a parabolic increase of the mass and a formation of a glassy surface layer were observed for the B6O materials whereas the cBN-material is characterized by the formation of a mostly crystalline layer. The oxidation resistance is the lowest for the pure B6O and the highest for the investigated cBN material.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Advanced ceramic materials synthesis · Advanced materials and composites · Aluminum Alloys Composites Properties
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (25)
Show source-provided references
1. Boron suboxide: as hard as cubic boron nitride10.1063/1.1494860 ↗
2. Pressing on: the legacy of Percy W. Bridgman10.1038/nmat1488 ↗
3. X-Ray study of the synthesis of boron oxides at high pressure: phase diagram and equation of state10.1103/PhysRevB.70.214108 ↗
4. High-pressure, high-temperature synthesis and characterization of boron suboxide (B6O)10.1021/cm970433+ ↗
5. High pressure consolidation of B6O-diamond mixtures10.1023/A:1012499214307 ↗
6. Microstructure and mechanical properties of B6O–B4C sintered composites prepared under high pressure10.1023/A:1004753116816 ↗
7. B6O-cBN composites prepared by high-pressure sintering10.1111/j.1151-2916.2000.tb01224.x ↗
8. Ellison-Hayashi C, Zandi M, Shetty DK, Kuo P, Yeckley R, Csillag F. Boron suboxide material and method for its preparation. 1992, US Patent 5,135,895.
9. Goosey BF, Anderson SC. Method of fabricating boron suboxide articles. 1974, US Patent 3,816,586.
10. Hot pressing of boron suboxide B12O210.1016/0022-5088(86)90003-2 ↗
11. Liquid phase assisted hot pressing of boron suboxide materials10.1016/j.jeurceramsoc.2007.10.011 ↗
12. B6O: a correlation between mechanical properties and microstructure evolution upon Al2O3 addition during hot-pressing10.1111/j.1551-2916.2007.02167.x ↗
13. Liquid phase assisted densification of superhard B6O-materials10.1016/j.jeurceramsoc.2009.03.002 ↗
14. Hard and tough boron suboxide based composites10.4028/www.scientific.net/AST.45.1745 ↗
15. Field-assisted densification of superhard B6O materials with Y2O3/Al2O3 addition10.1111/j.1551-2916.2009.03197.x ↗
16. Andrews A. Development of boron suboxide composites with improved thoughness. PhD-Thesis, Wits; 2008
17. High pressure sintering of B6O powder and properties of the sintered compact10.2472/jsms.47.1000 ↗
18. Herrmann M, Swarnakar AK, Thiele M, Van der Biest O, Sigalas I. High temperature properties of B6O-materials. J. Eur. Ceram. Soc., submitted.
19. Interaction of boron suboxide with compacted graphite cast iron10.1016/j.ceramint.2010.10.011 ↗
20. FactSage thermochemical software and databases10.1016/S0364-5916(02)00035-4 ↗
21. Uzgur · 1996 · 85
22. Baiburt · Vopr. Radioelektron. Ser. 4: Tekhnol. Proizv. Oborud. · 1963 · 64
23. Silicon nitride for high-temperature applications10.1111/j.1551-2916.2010.03839.x ↗
24. High-temperature oxidation of boron nitride: I. monolithic boron nitride10.1111/j.1551-2916.1999.tb20075.x ↗
25. High-temperature oxidation of boron nitride10.1016/S0272-8842(86)80006-2 ↗