journal article·2007-01

A technique for measuring stresses in small spatial regions using cube-corner indentation: Application to tempered glass plates

Rajan Tandon

Publisher page

Abstract

Abstract Vickers indentation cracks have been used to estimate residual stress in materials; however, a high threshold load for cracking limits the smallest spatial region for stress measurement. Cube-corner indenters have a lower included angle, and their sharpness leads to lowered cracking thresholds enabling stress measurement in small spatial regions. Cube-corner indentations on tempered glass plate and on annealed soda-lime-silica glass revealed that crack surface traces on the tempered material were significantly smaller. Cracks were found to be quarter-penny shaped as opposed to half-penny/radial for Vickers indentation. Using an appropriate stress-intensity factor and a stress-intensity factor superposition approach, surface stresses in the tempered plate were calculated. The stresses were in good agreement with those determined using well-established Vickers indentation approach; however, the spatial region sampled is 6–10 times smaller. An estimate of the smallest spatial region at which a particular stress may be measured using this technique is presented.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Metal and Thin Film Mechanics · Advanced Surface Polishing Techniques · Advanced ceramic materials synthesis

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (25)

Show source-provided references
1. Fracture of tempered glass10.1111/j.1151-2916.1968.tb11840.x ↗
2. Finite element analysis of stresses in glass-to-metal foil seals10.1111/j.1151-2916.1978.tb16126.x ↗
3. McKenzie · 1999
4. A mechanical determination of biaxial residual stress in sheet materials10.1063/1.1699913 ↗
5. Determination of residual stress profile using a strain gage technique10.1111/j.1151-2916.1990.tb05276.x ↗
6. Residual stress determination using strain gage measurements10.1111/j.1151-2916.1990.tb06738.x ↗
7. Effects of tensile stress on the Raman spectrum of silica glass10.1016/0022-3093(88)90292-X ↗
8. Indentation technique for measuring stresses in tempered glass surfaces10.1111/j.1151-2916.1977.tb16106.x ↗
9. Measurement of thin layer surface stresses by indentation fracture10.1007/BF00980772 ↗
10. Measurement of residual stresses in coatings on brittle substrates by indentation fracture10.1111/j.1151-2916.1987.tb05006.x ↗
11. Indentation behavior of ion-exchanged glasses10.1111/j.1151-2916.1990.tb05145.x ↗
12. Indentation crack initiation in ion-exchanged aluminosilicate glass10.1023/B:JMSC.0000020002.06117.46 ↗
13. Determination of surface residual stresses in brittle materials by Hertzian indentation: theory and experiment10.1111/j.1151-2916.1999.tb02003.x ↗
14. Measurement of residual stress by load and depth sensing indentation with spherical indenters10.1557/JMR.2001.0286 ↗
15. Pharr · 1993
16. Measurement of mechanical properties by ultra-low load indentation10.1016/S0921-5093(98)00724-2 ↗
17. In situ cube-corner indentation of soda-lime silica glass and fused silica10.1111/j.1551-2916.2004.01494.x ↗
18. Nanoindentation method for measuring residual stress in brittle materials10.1111/j.1151-2916.2003.tb03380.x ↗
19. Tandon, R. and Buchheit, T. E., J. Am. Ceram. Soc., in press.
20. An empirical stress intensity factor equation for the surface crack10.1016/0013-7944(81)90116-8 ↗
21. Stress intensity factors and weight functions for a corner crack in a finite thickness plate10.1016/0013-7944(95)00171-9 ↗
22. A critical evaluation of indentation techniques for measuring fracture toughness: I. Direct crack measurements10.1111/j.1151-2916.1981.tb10320.x ↗
23. Surface stress effects on indentation fracture sequences10.1111/j.1151-2916.1990.tb06737.x ↗
24. The effect of lateral crack growth on the strength of contact flaws in brittle materials10.1557/JMR.1986.0589 ↗
25. Tada · 2000