Influence of subcritical crack growth on the determination of fracture toughness in brittle materials
Source abstract
Abstract
Abstract The strength of materials suffering from subcritical crack growth (SCCG) can be affected by the loading conditions and environment. This crack growth can also occur during the measurement of the material’s fracture toughness, K Ic , yielding lower measured (apparent) values. In this work the K Ic measurements of two different brittle materials was compared in different environments ( i.e., water, ambient air and argon) using three testing methods: (i) Single Edge V-Notch Beam, (ii) Chevron Notch Beam, and (iii) Ball-on-three-Balls-KIc. A strong effect of the environment was found on the measured K Ic values using all three methods. Low “ K Ic values” were measured in water, i.e., ∼1.3–1.7 MPa m 1/2 depending on the material, whereas higher “toughness values” were obtained in argon, i.e., ∼2.0–2.3 MPa m 1/2 . This is explained with a model accounting for the SCCG during the fracture toughness experiment. Recommendations on the assessment of fracture toughness in brittle materials are given.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Concrete and Cement Materials Research · Hydrogen embrittlement and corrosion behaviors in metals · Advanced ceramic materials synthesis
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (24)
Show source-provided references
1. Delayed fracture in glass10.1088/0959-5309/59/2/302 ↗
2. Influence of water vapour on crack propagation in soda-lime glass10.1111/j.1151-2916.1967.tb15145.x ↗
3. Subcritical crack growth in ceramics
4. Thermally activated crack propagation in brittle materials10.1007/BF00012548 ↗
5. Sub-critical crack growth in ceramics
6. Subcritical crack propagation in 3Y-TZP ceramics: static and cyclic fatigue10.1111/j.1151-2916.1999.tb02213.x ↗
7. Influence of the temperature on the strength and the subcritical crack growth rate of alumina10.1016/j.msea.2004.02.090 ↗
8. Environmentally enhanced fracture of glass: a historical perspective10.1111/j.1551-2916.2009.03097.x ↗
9. R-curve and subcritical crack growth in lead zirconate titanate ceramics10.1016/j.msea.2008.09.016 ↗
10. Effect of microstructure and grain boundary chemistry on slow crack growth in silicon carbide at ambient conditions10.1016/j.jeurceramsoc.2015.02.020 ↗
11. Ceramic-filled-glass composite sintering
12. Lifetime prediction for mechanically stressed low temperature co-fired ceramics10.1016/j.jeurceramsoc.2003.07.010 ↗
13. Sub-critical crack growth behavior of a low-temperature co-fired ceramic10.1111/j.1551-2916.2007.01626.x ↗
14. Strength reliability of 3D low temperature co-fired multilayer ceramics under biaxial loading10.1016/j.jeurceramsoc.2010.11.031 ↗
15. Subcritical crack growth in low temperature co-fired ceramics under biaxial loading10.1016/j.engfracmech.2012.12.004 ↗
16. Influence of temperature and humidity on the strength of low temperature co-fired ceramics10.1016/j.jeurceramsoc.2014.12.031 ↗
17. ISO 23146, Fine ceramics (advanced ceramics, advanced technical ceramics) – Test methods for fracture toughness of monolithic ceramics – Single-edge V-notch beam (SEVNB) method (2008).
18. ASTM C 1421-01b, Standard Test Methods for Determination of Fracture Toughness of Advanced Ceramics at Ambient Temperature (2001).
19. On measuring fracture toughness under load control in the presence of slow crack growth10.1016/j.jeurceramsoc.2015.04.004 ↗
20. Lifetime prediction of ceramics: importance of the test method10.1016/0272-8842(94)90069-8 ↗
21. Influence of relative humidity on mechanical properties of alumina, PZT and zirconia10.4028/www.scientific.net/KEM.206-213.751 ↗
22. Biaxial tensile strength test for brittle rectangular plates10.2109/jcersj.114.1054 ↗
23. Slice synthesis of a three dimensional work of fracture specimen10.1016/0013-7944(75)90059-4 ↗
24. Fracture toughness testing of small ceramic discs and plates10.1016/j.jeurceramsoc.2013.12.021 ↗