journal article·2017-02

Mechanical properties of nano-grain SiO2 glass prepared by spark plasma sintering

Zhenhua He, Hirokazu Katsui, Takashi Goto

Publisher page

Abstract

Abstract Silicon carbide (SiC) layers were deposited on silica (SiO 2 ) glass powder by rotary chemical vapor deposition (RCVD) to form SiO 2 glass (core)/SiC (shell) powder; this powder was consolidated by spark plasma sintering (SPS). SiO 2 glass powder with a particle size of 250 nm was coated with 5–10-nm-thick SiC layers. The resultant SiO 2 glass (core)/SiC (shell) powder was consolidated to form a nano-grain SiO 2 glass composite at a relative density above 90% by SPS in the sintering temperature range of 1573–1823 K. The Vickers hardness and fracture toughness of the SiO 2 glass composite at 1723 K were found to be 14.2 GPa and 5.4 MPa m 1/2 , respectively.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Advanced ceramic materials synthesis · Diamond and Carbon-based Materials Research · Advanced materials and composites

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (19)

Show source-provided references
1. Bioactive glass ceramics: properties and applications10.1016/0142-9612(91)90194-F ↗
2. A survey of energy and environmental applications of glass10.1016/j.jeurceramsoc.2008.08.011 ↗
3. Preparation of Ni-precipitated hBN powder by rotary chemical vapor deposition and its consolidation by spark plasma sintering10.1016/j.jallcom.2010.04.170 ↗
4. Fabrication and mechanical properties of SiO2 matrix composites reinforced by carbon nanotube10.1016/S0921-5093(03)00256-9 ↗
5. High-hardness and ductile mosaic SiC/SiO2 composite by spark plasma sintering10.1111/jace.12813 ↗
6. Densification of SiO2–cBN composites by using Ni nanoparticle and SiO2 nanolayer coated cBN powder10.1016/j.ceramint.2012.02.090 ↗
7. Synthesis of SiC/SiO2 core-shell powder by rotary chemical vapor deposition and its consolidation by spark plasma sintering10.1016/j.ceramint.2012.09.025 ↗
8. Silicon carbide coating on diamond powder by rotary chemical vapor deposition10.4028/www.scientific.net/KEM.508.65 ↗
9. Surface modification of silicon carbide powder with silica coating by rotary chemical vapor deposition10.4028/www.scientific.net/KEM.616.232 ↗
10. Microstructures and mechanical properties of liquid-phase sintered seeded silicon carbide10.1016/S0254-0584(00)00435-1 ↗
11. Densification, microstructure and mechanical properties of SiO2–cBN composites by spark plasma sintering10.1016/j.ceramint.2011.07.013 ↗
12. Equilibrium penny-like cracks in indentation fracture10.1007/BF00557479 ↗
13. Elastic/plastic indentation hardness and indentation fracture toughness: the inclusion core model10.1007/BF01233154 ↗
14. Direct observation and analysis of indentation cracking in glasses and ceramics10.1111/j.1151-2916.1990.tb05119.x ↗
15. Indentation behavior of soda-lime silica glass fused silica, and single-crystal quartz at liquid nitrogen temperature10.1111/j.1151-2916.1995.tb08241.x ↗
16. Fracture toughness of fused SiO2 and float glass at elevated temperatures10.1111/j.1151-2916.1981.tb09884.x ↗
17. Fracture surface energy of glass10.1111/j.1151-2916.1969.tb13350.x ↗
18. Cone cracks around Vickers indentations in fused silica glass10.1007/BF00589840 ↗
19. Direct observation of indentation deformation and cracking of silicate glasses10.1557/jmr.2015.214 ↗