journal article·2018-04

Joining and testing of alumina fibre reinforced YAG-ZrO2 matrix composites

Muhammad Yasir Akram, Monica Ferraris, Valentina Casalegno, Milena Salvo, Georg Puchas, Stefan Knohl, Walter Krenkel

Publisher page

Abstract

Abstract Alumina (Nextel™ 610) fibre reinforced YAG-ZrO2 matrix composites were successfully joined by using different brazing alloys, metallic interlayers and a glass-ceramic. All joints were mechanically stable and free of cracks. Three commercial brazing alloys and a new alloy based on Ti/Cu/Al interlayers were selected to join these composites for applications in a non-oxidizing environment. A glass-ceramic based on SiO2-Al2O3-CaO-MgO was developed in case the joined component needs to be oxidation resistant. To evaluate the thermal stability, all joined composites were aged up to 100 h in air at 550 °C for brazing joints or 850 °C and 930 °C for glass-ceramic joints. The mechanical strength was measured using single lap and four point bending tests before and after ageing. Four point bending tests on glass-ceramic joined samples showed an average joint strength of about 70 MPa which is 35% of as-received composites.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Advanced ceramic materials synthesis · Intermetallics and Advanced Alloy Properties · Advanced materials and composites

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (53)

Show source-provided references
1. Creep of Nextel 610 fiber at 1100C in air and in steam10.1111/j.1744-7402.2012.02831.x ↗
2. Developments in oxide fiber composites10.1111/j.1551-2916.2006.01342.x ↗
3. Advances in oxide CMC10.1115/1.483195 ↗
4. Novel oxide fiber composites by freeze casting10.1016/j.jeurceramsoc.2014.06.015 ↗
5. Aluminosilicate fiber/mullite matrix composites with favorable high-temperature properties10.1016/S0955-2219(99)00260-5 ↗
6. Novel high temperature wound oxide ceramic matrix composites manufactured via freeze gelation
7. Durability of Oxide/Oxide CMCs in gas turbine combustors10.1115/1.4007978 ↗
8. Assessment of three oxide/oxide ceramic matrix composites: mechanical performance and effects of heat treatments10.1016/j.compositesa.2014.09.013 ↗
9. Oxide/oxide ceramic matrix composite (CMC) exhaust mixer development in the NASA environmentally responsible aviation (ERA) project
10. Improvement of oxide/oxide cmc and development of combustor and turbine components in the hipoc program
11. Anisotropic damage of alumina/alumina CFCCs under long term high temperature exposure: investigations by ultrasonic stiffness measurements and quasi-static tests10.1016/j.compscitech.2005.07.006 ↗
12. Ashcraft · 2011 · 1
13. Singh · 1999
14. Joining of machined SiC/SiC composites for thermonuclear fusion reactors10.1016/j.jnucmat.2008.02.020 ↗
15. Reaction of SiC/SiC composites with a zinc borate glass10.1111/j.1151-2916.1995.tb08872.x ↗
16. Flexural strength and shear strength of silicon carbide to silicon carbide joints fabricated by a molybdenum diffusion bonding technique10.1111/j.1551-2916.2005.00381.x ↗
17. Joining of SiC/SiCf ceramic matrix composites for fusion reactor blanket applications10.1016/S0022-3115(99)00268-8 ↗
18. Radiation-tolerant joining technologies for silicon carbide ceramics and composites10.1016/j.jnucmat.2013.10.002 ↗
19. Joining of zirconium diboride-based ultra high-temperature ceramic composites using metallic glass interlayers10.1016/j.msea.2007.01.015 ↗
20. Joining of SiC ceramic-based materials with ternary carbide Ti 3SiC210.1016/j.mseb.2010.09.002 ↗
21. Joining of C/SiC composites by spark plasma sintering technique10.1016/j.jeurceramsoc.2013.10.028 ↗
22. Secure tightening of a CMC fastener for the heat shield of re-entry vehicles10.1016/j.compstruct.2009.07.002 ↗
23. Characterization of furnace sintered mullite and oxide ceramic matrix composites (O-CMC) by using glass solders10.4028/www.scientific.net/AST.88.162 ↗
24. Corrosion of selected ceramic materials in hot gas environment10.1016/j.jeurceramsoc.2006.01.015 ↗
25. Norton · 2013
26. Reactive wetting of alumina by Ti-rich Ni–Ti–Zr alloys10.1007/s10853-015-9684-7 ↗
27. Actively brazed alumina to alumina joints using CuTi, CuZr and eutectic AgCuTi filler alloys10.1016/j.ceramint.2010.07.029 ↗
28. Wettability of transparent YAG (Y3Al5O12) by molten Ag-Cu-Ti alloys10.1016/j.jeurceramsoc.2015.03.036 ↗
29. Oxidation behavior of silver and copper based brazing filler metals for silicon nitride/metal joints10.1111/j.1151-2916.1989.tb06151.x ↗
30. Oxidation behaviour of titanium-containing brazing filler metals10.1007/BF02402948 ↗
31. Sealing technology for solid oxide fuel cells10.1111/j.1744-7402.2007.02128.x ↗
32. The state-of-the-art in sealing technology for solid oxide fuel cells10.1007/s11837-006-0052-6 ↗
33. An alkali-free barium borosilicate viscous sealing glass for solid oxide fuel cells10.1016/j.jpowsour.2014.07.088 ↗
34. Interfacial interactions between an alkali-free borosilicate viscous sealing glass and aluminized ferritic stainless steel10.1016/j.jpowsour.2013.11.018 ↗
35. Joining of porous alumina with a CaO-AlO3−SiO2 glass-ceramic10.1111/jace.12310 ↗
36. Microstructure and strength of Al2O3/Al2O3 joints bonded with ZnO-Al2O3-B2O3-SiO2 glass-ceramic10.1016/j.jmst.2014.01.011 ↗
37. High performance oxide fibers for metal and ceramic composites10.1016/S1359-835X(00)00176-7 ↗
38. Improvement in oxidation resistance of Cu-Al dilute alloys by pre-annealing in H2 and Ar atmospheres10.2320/matertrans.46.167 ↗
39. Brazing ceramics to titanium using amorphous filler metal
40. Light metal system part 2-AlCuTi
41. Glass forming ability criterion10.4028/www.scientific.net/MSF.19-20.11 ↗
42. Glass structure and glass properties
43. Study of calcium-magnesium-aluminum-silicate (CMAS) glass and glass-ceramic sealant for solid oxide fuel cells10.1016/j.jpowsour.2012.12.055 ↗
44. Crystallization kinetics of a solid oxide fuel cell seal glass by differential thermal analysis10.1016/j.jpowsour.2005.01.010 ↗
45. Kinetic study on Non-Isothermal crystallization
46. Kinetics of non-isothermal crystallization10.1016/0032-3861(71)90041-3 ↗
47. Glass-ceramic sealant for solid oxide fuel cells application: characterization and performance in dual atmosphere10.1016/j.jpowsour.2016.08.010 ↗
48. Crystallization behaviour of glass-ceramic sealant for solid oxide fuel cells10.1016/j.matlet.2014.11.128 ↗
49. Flexural strength and Weibull analysis of a microhybrid and a nanofill composite evaluated by 3- and 4-point bending tests10.1016/j.dental.2007.05.013 ↗
50. High-temperature mechanical properties of a glass sealant for solid oxide fuel cell10.1016/j.jpowsour.2008.12.102 ↗
51. Flexural strength and viscosity of glass ceramic sealants for solid oxide fuel cell stacks10.1002/fuce.201100116 ↗
52. Novel glass-ceramic composition as sealant for SOFCs10.1111/jace.13219 ↗
53. High temperature mechanical properties of a crystallized BaO-B2O3-Al2O3-SiO2 Glass ceramic for sofc