High-temperature corrosion of spark plasma sintered Gd2SiO5 with volcanic ash for environmental barrier coatings
Source abstract
Abstract
Abstract Hot corrosion behavior was evaluated by gadolinium monosilicate (Gd2SiO5) with volcanic ash for environmental barrier coatings (EBCs). Sintered Gd2SiO5 was prepared by the spark plasma sintering (SPS) method at 1400 °C for 20 min, and high-temperature corrosion resistance against of volcanic ash was evaluated at 1400 °C for 2 h, 12 h, and 48 h. The surface region of sintered Gd2SiO5 was partially dissolved in molten volcanic ash, creating a chemically reacted area. The formation of the elongated morphology of Ca2Gd8(SiO4)6O2 grains observed in the reaction area is thicker with increasing heat-treatment time as the volcanic ash dissolves. In addition, high-temperature X-ray diffraction was carried out to identify the dynamics of phase evaluation in the volcanic ash and Gd2SiO5. According to the results, corrosion occurs due to reaction of the Gd2SiO5 phase and the Ca component of volcanic ash at 1300 °C, and the Ca2Gd8(SiO4)6O2 phase is generated.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Advanced ceramic materials synthesis · Nuclear materials and radiation effects · Advanced materials and composites
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (24)
Show source-provided references
1. Environmental durability of slurry based mullite–gadolinium silicate EBCs on silicon carbide10.1016/j.jeurceramsoc.2010.12.015 ↗
2. Corrosion characteristics of silicon carbide and silicon nitride10.6028/jres.098.040 ↗
3. Rare earth silicate environmental barrier coatings for SiC/SiC composites and Si3N4 ceramics10.1016/j.jeurceramsoc.2004.12.013 ↗
4. Thermophysical properties of porous SiC ceramics fabricated by pressureless sintering
5. Influence of microstructure on the thermophysical properties of sintered SiC ceramics10.1016/j.jallcom.2007.09.055 ↗
6. Tensile fatigue behavior of plain-weave reinforced Cf/C-SiC composites10.1016/j.ceramint.2016.01.068 ↗
7. CMC jackets for metallic pipes—a novel approach to prevent the creep deformation of thermo-mechanically loaded metals10.1016/j.jeurceramsoc.2018.01.018 ↗
8. Microstructural and thermal properties of plasma sprayed mullite coatings10.1016/j.ceramint.2010.02.007 ↗
9. Hydrothermal synthesis of ytterbium silicate nanoparticles10.1021/ic9023585 ↗
10. High‐temperature corrosion of EB‐PVD yttria partially stabilized zirconia thermal barrier coatings with an artificial volcanic ash overlay10.1111/j.1551-2916.2010.04166.x ↗
11. Volcanic ash‐induced decomposition of EB ‐PVD Gd2Zr2O7 thermal barrier coatings to Gd ‐oxyapatite, zircon, and Gd, Fe ‐zirconolite10.1111/jace.12251 ↗
12. Corrosion behavior of volcanic ash on sintered mullite for environmental barrier coatings10.1016/j.ceramint.2016.10.147 ↗
13. Thermal behavior and mechanical properties of Y2SiO5 environmental barrier coatings after isothermal heat treatment10.1016/j.surfcoat.2016.09.088 ↗
14. Water vapour corrosion of rare earth monosilicates for environmental barrier coating application10.1016/j.ceramint.2017.02.123 ↗
15. High temperature water vapour corrosion of rare earth disilicates (Y, Yb, Lu)2Si2O7 in the presence of Al(OH)3 impurities10.1016/j.jeurceramsoc.2006.09.013 ↗
16. Degradation of La2Zr2O7 and other novel EB-PVD thermal barrier coatings by CMAS (CaO–MgO–Al2O3–SiO2) and volcanic ash deposits10.1016/j.surfcoat.2013.07.029 ↗
17. Mechanisms and mitigation of volcanic ash attack on yttria stabilized zirconia thermal barrier coatings10.1016/j.surfcoat.2014.09.015 ↗
18. Hot corrosion behavior of plasma sprayed 4 mol% Y2O3- ZrO2 thermal barrier coatings with volcanic ash10.4191/kcers.2013.50.6.353 ↗
19. Hot corrosion of γ-Y2Si2O7 in strongly basic Na2CO3 molten salt environmentJ10.1016/j.jeurceramsoc.2007.05.011 ↗
20. CMAS degradation of environmental barrier coatings
21. Corrosion behavior of volcanic ash and calcium magnesium aluminosilicate on Yb2SiO5 environmental barrier coatings10.2109/jcersj2.16211 ↗
22. Hot corrosion of RE2SiO5 with different cation substitution under calcium–magnesium–aluminosilicate attack10.1016/j.ceramint.2017.04.045 ↗
23. High temperature corrosion of ZrO2-4mol%Y2O3 thermal barrier coatings with volcanic ash
24. Influence of rare earth oxides on kinetics and reaction mechanisms in CMAS silicate melts10.1016/j.jeurceramsoc.2019.06.036 ↗