Fabrication of porous SiC ceramics having pores shaped with Si grain templates
Source abstract
Abstract
Abstract SiC porous ceramics were prepared by heating mixtures of Si powder and carbon black at 900 °C for 24 h in Na vapor. The grains of the Si powder were not only the source of Si for SiC but also served as templates for the pores in the SiC porous ceramics. Angular-shaped pores with sizes of 2–10, 10–150 and 50–150 μm were formed by angular Si grains with sizes of ≤10, ≤50 and ≤150 μm, respectively. The porosity of the SiC porous ceramics was around 55–59%. Spherical pores were also formed when spherical Si grains were used. A bending strength of 14 MPa was measured for the SiC porous ceramics prepared with the Si grains (≤50 μm).
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Advanced ceramic materials synthesis · Aluminum Alloys Composites Properties · Advanced materials and composites
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (22)
Show source-provided references
1. Processing routes to macroporous ceramics: a review10.1111/j.1551-2916.2006.01044.x ↗
2. Fabrication and characterization of cordierite-bonded porous SiC ceramics10.1016/j.ceramint.2008.01.025 ↗
3. Effect of template size on microstructure and strength of porous silicon carbide ceramics10.2109/jcersj2.116.1159 ↗
4. Processing and properties of polysiloxane-derived porous silicon carbide ceramics using hollow microspheres as templates10.1016/j.jeurceramsoc.2007.09.009 ↗
5. Porosity control of porous silicon carbide ceramics10.1016/j.jeurceramsoc.2009.03.027 ↗
6. Sintering behavior of porous SiC ceramics10.1016/j.ceramint.2003.10.006 ↗
7. Microstructure and properties of porous β-SiC templated from soft woods10.1016/S0955-2219(03)00195-X ↗
8. Porous SiC ceramics fabricated by reactive infiltration of gaseous silicon into charcoal10.1016/j.ceramint.2003.11.001 ↗
9. Biomorphic SiC-ceramic prepared by Si-vapor phase infiltration of wood10.1016/S0955-2219(02)00131-0 ↗
10. Porous silicon carbide ceramics produced by a carbon foam derived from mixtures of mesophase pitch and Si particles10.1111/j.1551-2916.2008.02842.x ↗
11. Wood-derived porous SiC ceramics by sol infiltration and carbothermal reduction10.1111/j.1551-2916.2004.00784.x ↗
12. Preparation of porous SiC ceramic with a woodlike micostructure by sol–gel and carbothermal reduction processing10.1016/j.jeurceramsoc.2003.10.042 ↗
13. Preparation of biomorphic SiC ceramic by carbothermal reduction of oak wood charcoal10.1016/j.msea.2003.11.051 ↗
14. Low-temperature fabrication of porous SiC ceramics by preceramic polymer reaction bonding10.1016/j.matlet.2004.11.003 ↗
15. Low temperature synthesis of β-SiC powder by the Na flux method using fullerene and silicon10.2109/jcersj.115.74 ↗
16. Low-temperature synthesis of biomorphic cellular SiC ceramics from wood by using a Na flux10.2109/jcersj2.116.163 ↗
17. Low-temperature synthesis and mechanical properties of SiC porous granules from activated charcoal with a Na flux10.2320/matertrans.MAW200859 ↗
18. Na–Si binary phase diagram and solution growth of silicon crystals10.1016/j.jallcom.2009.02.036 ↗
19. Low-temperature fabrication of porous β-SiC ceramics in sodium vapor10.1111/j.1551-2916.2007.02021.x ↗
20. Preparation of monosized silicon micro particles by pulsated orifice ejection method10.2497/jjspm.53.346 ↗
21. Thermal expansion of the cubic (3C) polytype of SiC10.1007/BF01106557 ↗
22. Determination of the vapor pressure of sodium10.1021/j150523a012 ↗