journal article·2014-12

Arc jet testing and evaluation of Mo–Si–B coated Mo and SiC–ZrB2 ceramics

P.J. Ritt, P.A. Williams, S.C. Splinter, J.H. Perepezko

Publisher page

Abstract

Abstract The transition from blunt leading edges to sharp leading edges on re-entry aircrafts is necessary to increase both maneuverability and safety. However, the oxidation resistance of current materials is inadequate for the extreme conditions experienced by sharp leading edge re-entry vehicles. The Mo–Si–B alloy system has been utilized to design a multilayer coating that has the ability to protect from 800 to 1700 °C. Substrates of Mo and ZrB 2 –50 vol% SiC with a flat profile were coated with the Mo–Si–B based coating and evaluated using arc jet testing performed at NASA Langley Research Center. Heat fluxes of 2.5 to nearly 3.5 MW/m 2 and surface temperatures of 1500–1650 °C were achieved during the 20-min tests. The samples presented in this study showed
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Advanced ceramic materials synthesis · Advanced materials and composites · Diamond and Carbon-based Materials Research

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (59)

Show source-provided references
1. Thermal shielding of a reentry vehicle by ultra-high-temperature ceramic materials10.2514/1.17947 ↗
2. High speed propulsion: performance advantage of advanced materials10.1023/B:JMSC.0000041687.37448.06 ↗
3. Fifty years of hypersonics: where we’ve been, where we’re going10.1016/S0376-0421(03)00079-4 ↗
4. Oxidation of ultra-high temperature transition metal diboride ceramics10.1179/1743280411Y.0000000012 ↗
5. Degradation behavior of 4D carbon/carbon composites under supersonic oxidative air plasma10.1016/j.ceramint.2013.02.056 ↗
6. Experimental investigation of passive/active oxidation behavior of SiC based ceramic thermal protection materials exposed to high enthalpy plasma10.1016/j.jeurceramsoc.2012.09.002 ↗
7. Oxidation and ablation of 3d carbon–carbon composite at up to 3000-degrees-C10.1016/0008-6223(94)00172-V ↗
8. Oxidation microstructure studies of reinforced carbon/carbon10.1016/j.carbon.2005.11.013 ↗
9. Microstructure and ablation performances of dual-matrix carbon/carbon composites10.1016/j.carbon.2006.01.017 ↗
10. Oxidation behavior and protection of carbon/carbon composites10.1016/0008-6223(87)90197-7 ↗
11. Oxidation-resistant carbon–carbon composites up to 1700-degrees-C10.1016/0008-6223(94)00173-W ↗
12. Active oxidation of SiC10.1007/s11085-010-9216-4 ↗
13. Oxidation of carbon fiber-reinforced silicon carbide matrix composites at reduced oxygen partial pressures10.1111/j.1551-2916.2010.04376.x ↗
14. Thermal and environmental barrier coatings for SiC/SiC CMCs in aircraft engine applications10.1111/j.1744-7402.2004.tb00181.x ↗
15. Corrosion of silicon-based ceramics in combustion environments10.1111/j.1151-2916.1993.tb03684.x ↗
16. Structural evolution and ablation mechanism of a hafnium carbide coating on a C/C composite in an oxyacetylene torch environment10.1016/j.corsci.2012.04.033 ↗
17. Ablation behavior of HfC protective coatings for carbon/carbon composites in an oxyacetylene combustion flame10.1016/j.corsci.2012.08.064 ↗
18. Microstructure and ablation behavior of hafnium carbide coating for carbon/carbon composites10.1016/j.surfcoat.2011.12.001 ↗
19. Oxygen diffusion in atomic layer deposited ZrO2 and HfO2 thin films on Si(100)10.1063/1.1753080 ↗
20. Oxidation-based materials selection for 2000 degrees C plus hypersonic aerosurfaces: theoretical considerations and historical experience10.1023/B:JMSC.0000041686.21788.77 ↗
21. Toward oxidation-resistant ZrB2–SiC ultra high temperature ceramics10.1007/s11661-010-0540-8 ↗
22. Oxidation behavior of a Zr-0.5y alloy10.1007/BF00613535 ↗
23. Oxygen diffusion in ultrafine grained monoclinic ZrO210.1063/1.370567 ↗
24. Oxidation of ZrB2–SiC ultra-high temperature composites over a wide range of SiC content10.1016/j.jeurceramsoc.2012.05.021 ↗
25. Space shuttle thermal protection system
26. Ablation behavior of ZrB2–SiC ultra high temperature ceramics under simulated atmospheric re-entry conditions10.1016/j.compscitech.2008.02.009 ↗
27. Stability of ultra-high-temperature ZrB2–SiC ceramics under simulated atmospheric re-entry conditions10.1016/j.jeurceramsoc.2007.02.201 ↗
28. Arc-jet testing of ultra-high-temperature-ceramics10.1016/j.ast.2009.12.004 ↗
29. Dynamic oxidation of ultra-high temperature ZrB2–SiC under high enthalpy supersonic flows10.1016/j.corsci.2010.11.018 ↗
30. Oxidation of ZrB2–SiC ceramics under atmospheric and reentry conditions
31. Arc-jet testing on HfB2 and HfC-based ultra-high temperature ceramic materials10.1016/j.jeurceramsoc.2007.11.021 ↗
32. Processing, properties and arc jet oxidation of hafnium diboride/silicon carbide ultra high temperature ceramics10.1023/B:JMSC.0000041689.90456.af ↗
33. ZrB2–SiC sharp leading edges in high enthalpy supersonic flows10.1111/j.1551-2916.2012.05226.x ↗
34. Thermal and oxidation response of UHTC leading edge samples exposed to simulated hypersonic flight conditions10.1111/jace.12180 ↗
35. Oxidation-resistant coatings for ultra-high-temperature refractory Mo-based alloys10.1007/s11837-010-0148-x ↗
36. Phase stability and structural defects in high-temperature Mo–Si–B alloys10.1016/j.actamat.2008.07.015 ↗
37. Liquidus projection for the Mo-rich portion of the Mo–Si–B ternary system10.1016/S0966-9795(99)00088-6 ↗
38. Boron-doped molybdenum silicides10.1002/adma.19960080118 ↗
39. Oxide scale formation and isothermal oxidation behavior of Mo–Si–B intermetallics at 600–1000 degrees C10.1016/S0966-9795(98)00058-2 ↗
40. Boron-doped molybdenum silicides for structural applications10.1016/S0921-5093(98)01045-4 ↗
41. Diffusion structures in Mo vs. Si solid–solid diffusion couples10.1016/S1359-6462(98)00111-0 ↗
42. Microstructure and growth kinetics of the Mo5Si3 and Mo3Si layers in MoSi2/Mo diffusion couple10.1016/S0966-9795(03)00068-2 ↗
43. Synthesis of oxidation resistant silicide coatings on Mo–Si–B alloys10.1016/j.scriptamat.2005.05.015 ↗
44. Coating designs for oxidation control of Mo–Si–B alloys10.1016/S1359-6462(02)00070-2 ↗
45. Characterization and oxidation behavior of silicide coating on multiphase Mo–Si–B alloy10.1016/j.intermet.2008.06.014 ↗
46. Oxidation behaviour of the Mo–Si–B and Mo–Si–B-Al alloys in the temperature range of 700–1300 degrees C10.1016/j.intermet.2007.02.012 ↗
47. Mo–Si–B based coating for oxidation protection of SiC–C composites10.1016/j.surfcoat.2012.04.016 ↗
48. Comparative measurements of earth and martian entry environments in the NASA Langley HYMETS Facility
49. Silicon-carbide/boron-containing coatings for the oxidation protection of graphite10.1016/0008-6223(94)00178-3 ↗
50. Interdiffusion kinetics in the Mo5SiB2 (T-2) phase10.1007/BF02736562 ↗
51. Mechanical, thermal, and oxidation properties of refractory hafnium and zirconium compounds10.1016/S0955-2219(99)00129-6 ↗
52. Oxygen diffusion through Al-doped amorphous SiO210.1007/BF02736571 ↗
53. Oxidation of zirconium diboride-silicon carbide ceramics under an oxygen partial pressure of 200Pa: formation of zircon10.1016/j.corsci.2010.06.004 ↗
54. Thermal stability of zircon (ZrSiO4)10.1016/j.jeurceramsoc.2007.12.040 ↗
55. Active oxidation of a UHTC-based CMC
56. Temperature jump phenomenon during plasmatron testing of ZrB2–SiC ultrahigh-temperature ceramics10.2514/1.T3798 ↗
57. Modeling oxidation kinetics of SiC-containing refractory diborides10.1111/j.1551-2916.2011.04927.x ↗
58. Oxidation kinetics of hot-pressed ZrB2–SiC ceramic matrix composites10.1016/j.ceramint.2012.09.091 ↗
59. Transient oxidation of Mo–Si–B alloys: effect of the microstructure size scale10.1016/j.actamat.2009.06.036 ↗