Influence of carbon sources on nitriding process, microstructures and mechanical properties of Si3N4 bonded SiC refractories
Source abstract
Abstract
Abstract The incomplete nitriding and heterogeneity structure of large-size Si 3 N 4 -bonded SiC refractories limited its application in refractories industry. The objective of this work was to provide a way that adding carbon in matrix with the expectations of carbon could reacted with free-Si and transformed into SiC after nitridation. The effects of carbon sources on the bonded morphologies and nitridation process of Si 3 N 4 bonded SiC refractories were investigated. Results indicated the strength and Young’s-modulus of specimen with carbon black increased to 39.4 MPa and 103.89 GPa from 29.8 MPa and 73.43 GPa, respectively. The residual Young’s-modulus also improved from 44.13 GPa to 62.9 GPa after 9-quenching cycles. For specimen with graphite, residual graphite after nitridation resulted in a definite strength decline, but residual strength after quenching was improved. Moreover, analysis results on N-elements indicated surprisingly improvement in the nitriding degree for specimen with carbon black. The microstructure evolution and mechanism associating with the enhanced nitriding process was discussed.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Advanced ceramic materials synthesis · Advanced materials and composites · Aluminum Alloys Composites Properties
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (38)
Show source-provided references
1. Bond developments in silicon carbide blast furnace refractories during the 1980’s
2. William E. Lee, W. Mark Rainforth, Ceramic microstructures, property control by processing, Printed in Great Britain at University Press, Cambridge, 1994, P. 492–495, ISBN 0–412-431408.
3. Chemical degradation of si3N4-bonded SiC sidelining materials in aluminium electrolysis cells10.1111/j.1551-2916.2009.03020.x ↗
4. Thermal conductivity of porous Si3N4-bonded SiC sidewall materials in aluminum electrolysis cells10.1111/j.1551-2916.2011.04973.x ↗
5. Physico-chemical characterisation of silicon carbide refractories10.1016/j.jeurceramsoc.2005.08.009 ↗
6. Phase transformation, microstructure and mechanical properties of Si3N4/SiC composite10.1016/S0955-2219(01)00193-5 ↗
7. Silicon nitride and related materials10.1111/j.1151-2916.2000.tb01182.x ↗
8. Silicon nitride for high-temperature applications10.1111/j.1551-2916.2010.03839.x ↗
9. Influence of additives on microstructural changes in nitride bonded SiC refractories10.1016/j.jeurceramsoc.2005.03.238 ↗
10. Reaction-bonded silicon carbide refractories10.1016/S0254-0584(01)00502-8 ↗
11. Influence of sintering and sintering additives on the mechanical and microstructural characteristics of Si3N4/SiC wood cutting tools10.1016/j.jeurceramsoc.2010.04.007 ↗
12. Catalytic effects of metals on direct nitridation of silicon10.1111/j.1151-2916.2001.tb00897.x ↗
13. Synthesis of porous Si3N4/SiC ceramics with rapid nitridation of silicon10.1016/j.jeurceramsoc.2015.06.028 ↗
14. Sintering of Si3N4 under high nitrogen pressure10.1111/j.1151-2916.1977.tb16102.x ↗
15. Microstructure and thermomechanical behaviour of a SiC-based refractory
16. Influence of porosity on the high temperature oxidation of a SiC-reinforced Si3N4 ceramic composite10.1023/A:1026746927762 ↗
17. Manufacture and examination of C/Si3N4 nanocomposites10.1016/j.jeurceramsoc.2003.10.021 ↗
18. Microstructure and fracture-mechanical properties of carbon derived Si3N4+SiC nanomaterials10.1016/j.msec.2005.09.032 ↗
19. Some tribological properties of a carbon-derived Si3N4/SiC nanocomposite10.1016/j.jeurceramsoc.2003.10.029 ↗
20. SiC ceramic-bonded carbon fabricated with Si3N4 and carbon powders10.1111/j.1744-7402.2011.02677.x ↗
21. Fabrication of low shrinkage, porous silicon nitride ceramics by addition of a small amount of carbon10.1111/j.1151-2916.2001.tb00890.x ↗
22. Creep behavior of a carbon-derived Si3N4/SiC nanocomposite10.1016/j.jeurceramsoc.2003.10.046 ↗
23. Young’s modulus of elasticity of carbon-bonded alumina materials up to 1450°C10.1111/jace.12526 ↗
24. High temperature behaviour of spinel castables-impact on microstructural changes
25. Oxidation mechanism of Si3N4-bonded SiC ceramics by CO, CO2 and steam10.1023/A:1004354415867 ↗
26. Thermodynamic calculation of the Si-N-O system
27. Yamaguchi · 2016 · 60
28. Creep mechanisms in multiphase ceramic materials10.1111/j.1151-2916.1998.tb02333.x ↗
29. Decomposition of ZrW2O8 in Al matrix and the influence of heat treatment on ZrW2O8/Al-Si thermal expansion10.1016/j.scriptamat.2014.10.014 ↗
30. Reactivity between liquid Si or Si alloys and graphite10.1016/j.jeurceramsoc.2012.05.020 ↗
31. Nitrogen solubility in liquid silicon10.2320/matertrans1989.35.821 ↗
32. Synthesis and microwave absorption properties of SiC nanowires reinforced SiOC ceramic10.1016/j.jeurceramsoc.2013.08.029 ↗
33. Combustion synthesis of SiC/Si3N4-NW composite powders: the influence of catalysts and gases10.1016/j.ceramint.2012.02.032 ↗
34. Growth and characterization of nanostructured β-SiC via carbothermal reduction of SiO2 xerogels containing carbon nanoparticles10.1016/S0022-0248(99)00435-2 ↗
35. Optical and electrical transport properties in silicon carbide nanowires10.1063/1.1781749 ↗
36. Effect of ferrosilicon additive and sintering condition on microstructural evolution and mechanical properties of reaction-bonded SiC refractories10.1016/j.ceramint.2016.08.081 ↗
37. Synthesis of silicon carbide whiskers using reactive graphite as template10.1016/j.ceramint.2013.07.032 ↗
38. Production of SiC and Si3N4 whiskers in C+SiO2 solid mixtures10.1016/S0254-0584(01)00332-7 ↗