The effects of fiber orientation on failure behaviors of 2D C/SiC torque tube
Source abstract
Abstract
Abstract Different failure behaviors were observed in the 2D C/SiC torque tubes which were fabricated by chemical vapor infiltration (CVI) with different fiber orientations (0°/90° and ±45°). CT test was implemented to characterize the density heterogeneity of the ceramic matrix composite (CMC) torque tubes. With the density value measured by Archimedes drainage method, FEM software was implemented to simulate the stress distribution of the ceramic matrix composite torque tubes and calculate the failure stress. Torsional tests were conducted using special attachments to a universal material test machine. Different torsional behaviors of CMC torque tubes with two different fiber orientations were presented in the stress-strain curves. The fracture morphologies were observed by SEM, and the predominant factors of failure were analyzed. CMC torque tubes with fiber orientation of ±45° have a higher torque capacity and modulus. In failure analysis, we found that ±45° fiber orientation CMC torque tubes have reasonable fracture morphologies.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Advanced ceramic materials synthesis · Aluminum Alloys Composites Properties · Advanced materials and composites
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (17)
Show source-provided references
1. C/C-SiC composites for space applications and advanced friction systems10.1016/j.msea.2005.08.204 ↗
2. Advanced ceramic matrix composite materials for current and future propulsion technology applications10.1016/j.actaastro.2004.05.052 ↗
3. Vapor-phase fabrication and properties of continuous filament ceramic composites10.1126/science.253.5024.1104 ↗
4. Simulated three-dimensional transient temperature field during aircraft braking for C/SiC composite brake disc10.1016/j.matdes.2011.01.041 ↗
5. Operational limits for reusable space transportation systems due to physical boundaries of C/SiC materials10.1016/S1270-9638(03)00054-3 ↗
6. Technologies for thermal protection systems applied on re-usable launcher10.1016/j.actaastro.2004.05.034 ↗
7. The effects of Z-stitching density on thermophysical properties of plain woven carbon fiber reinforced silicon carbide composites10.1016/j.ceramint.2014.08.070 ↗
8. Prediction of the torsional strength of the hybrid aluminum/composite drive shaft10.1016/j.matdes.2008.05.024 ↗
9. An axial/torsional test method for ceramic matrix composite tubular specimens
10. Carter · 2001 · 1
11. Design, preparation and properties of non-oxide CMCs for application in engines and nuclear reactors: an overview10.1016/S0266-3538(03)00230-6 ↗
12. Microstructure and mechanical properties of three-dimensional carbon/silicon carbide composites fabricated by chemical vapor infiltration10.1016/S0008-6223(98)00076-1 ↗
13. FEM calculation about tensile strength of 2D-C/SiC composites with circular holes
14. Ceramic matrix composite material in highly loaded journal bearings
15. Compression strength of porous sintered alumina and zirconia10.1111/j.1151-2916.1953.tb12837.x ↗
16. Failure criteria for non-metallic materials part II: ceramic matrix composites
17. Damage characteristics and constitutive modeling of the 2D C/SiC composite: part I—experiment and analysis10.1016/j.cja.2014.10.026 ↗