Abstract
Abstract A higher manganese silicide (HMS) thermoelectric, with composition MnSi1.74, densified by spark plasma sintering, was successfully coated with a glass-ceramic, in order to be used at temperatures higher than 500 °C. Compositional changes in both the HMS substrate and the glass-ceramic coating are reviewed and discussed with respect to the electrical properties of the uncoated and coated HMS before and after thermal cycles from RT to 600 °C in air. The formation of a Si-deficient layer (MnSi) on the uncoated HMS surface is due to the reaction between the HMS and oxygen at 600 °C, thus contributing to a lower power factor in comparison with the as-sintered HMS. Coated HMS samples (after thermal cycles RT-600 °C) show a lower electrical resistivity and a significantly higher power factor in comparison with the uncoated ones. The glass-ceramic coating is self-reparable at 600 °C, as demonstrated by the complete sealing of an induced scratch on its surface.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Advanced Thermoelectric Materials and Devices · Semiconductor materials and interfaces · Chalcogenide Semiconductor Thin Films
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (19)
Show source-provided references
1. Complex thermoelectric materials10.1038/nmat2090 ↗
2. New and old concepts in thermoelectric materials10.1002/anie.200900598 ↗
3. Physical, mechanical, and structural properties of highly efficient nanostructured n- and p-silicides for practical thermoelectric applications10.1007/s11664-013-2848-9 ↗
4. High performance n-type PbTe-based materials for thermoelectric applications
5. Encapsulated thermoelectric modules for advanced thermoelectric systems10.1007/s11664-013-2926-z ↗
6. Thermal to electrical energy conversion of skutterudite-based thermoelectric modules10.1007/s11664-012-2261-9 ↗
7. Multilayered thin films for oxidation protection of Mg2Si thermoelectric material at middle–high temperatures10.1016/j.tsf.2012.10.114 ↗
8. Protective properties of magnetron-sputtered Cr–Si layers on CoSb310.1007/s11085-010-9209-3 ↗
9. Oxidation suppression characteristics of the YSZ coating on Mg2Si thermoelectric legs10.1016/j.ceramint.2016.03.161 ↗
10. Thermal stability of Mg2Si0.4Sn0.6 in inert gases and atomic-layer-deposited Al2O3 thin film as a protective coating10.1039/C6TA07611D ↗
11. Oxidation protective glass-ceramic coating for higher manganese silicide thermoelectrics10.1007/s10853-016-0192-1 ↗
12. Protective enamel coating for n- and p-type skutterudite thermoelectric materials10.1007/s10853-014-8711-4 ↗
13. Enhancement of oxidation resistance of CoSb3 thermoelectric material by glass coating10.1016/j.matdes.2017.01.055 ↗
14. Improved oxidation resistance of thermoelectric skutterudites coated with composite glass10.1016/j.ceramint.2012.11.051 ↗
15. Durability of silicide-based thermoelectric modules at high temperatures in air10.1007/s11664-015-3784-7 ↗
16. Effect of thermal cycling on commercial thermoelectric modules
17. Durable glass-ceramic coatings for foam glass10.1111/j.2041-1294.2011.00071.x ↗
18. Sealing technology for solid oxide fuel cells (SOFC)10.1111/j.1744-7402.2007.02128.x ↗
19. Vitreous and glass-ceramics materials in the SiO2-Al2O3-MeO-M2O type system