Manufacturing of electrical discharge machinable ZTA-TiC - hot pressing vs. spark plasma sintering
Source abstract
Abstract
Abstract Hot pressing and spark plasma sintering were applied to manufacture electrical discharge machinable ZTA-TiC ceramics containing 17 vol.% zirconia (1.5Y) and 24 vol.% titanium carbide in an alumina matrix. Sintering was carried out at 1450–1600 °C and 40 MPa pressure with 2 h dwell for HP and 10 min for SPS. The influence of sintering conditions on mechanical properties, microstructure, phase composition and electrical conductivity was investigated. Both sintering technologies lead to fully densified samples with similar strength and toughness. Hardness was generally lower for SPS. SPS samples develop a finer microstructure. HP samples the TiC grains tend to merge at high sintering so that HP materials reach significantly higher conductivities. Productivity and energy consumption per piece can be significantly decreased by shifting to SPS. Both types of material were ED-machinable. Hot pressed ceramics showed better cutting performance and improved surface quality in trimming operations.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Advanced ceramic materials synthesis · Advanced materials and composites · MXene and MAX Phase Materials
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (39)
Show source-provided references
1. Fracture toughness of Al2O3 with an unstabilized ZrO2 dispersed phase10.1111/j.1151-2916.1976.tb09386.x ↗
2. Review zirconia-toughened alumina (ZTA) ceramics10.1007/BF02385721 ↗
3. The influence of stabilizer concentration on the mechanical properties of alumina – 17 vol% zirconia (0.6Y-2Y) composites
4. High strength and toughness alumina matrix composites by transformation toughening and ‘in situ’ platelet reinforcement (ZPTA) – the new generation of bioceramics
5. EDM-future steps towards the machining of ceramics10.1016/S0007-8506(07)60759-8 ↗
6. A study on the electrical discharge machining of conductiveCeramics10.1016/j.jmatprotec.2004.04.197 ↗
7. Microstructure and tool electrode erosion in EDMed of TiN/Si3N4 composites10.1016/S0921-5093(03)00630-0 ↗
8. Electrical discharge machining of ZrO2 toughened WC composites10.1016/j.matchemphys.2010.03.069 ↗
9. Development of electrical discharge machinable ZTA ceramics with 24 vol% of TiC, TiN, TiCN, TiB2 and WC as electrically conductive phase10.1111/j.1744-7402.2012.02756.x ↗
10. Wire-EDM of ZTA-TiC composites with variable content of electrically conductive phase10.4028/www.scientific.net/KEM.504-506.1165 ↗
11. Machinability of ZTA-TiC ceramics by electrical discharge drilling10.1016/j.procir.2013.03.022 ↗
12. The effect of electric field and pressure on the synthesis and consolidation of materials: A review of the spark plasma sintering method10.1007/s10853-006-6555-2 ↗
13. Thermodynamics analysis of diffusion in spark plasma sintering welding Cr3C2 and ni10.1063/1.4978366 ↗
14. Y2O3 and Nd2O3 co-stabilized ZrO2-WC composites10.1007/s10853-008-2899-0 ↗
15. Pulsed electric current sintering of electrically conductive ceramics10.1007/s10853-008-2631-0 ↗
16. Development of ZrO2–WC composites by pulsed electric current sintering10.1016/j.jeurceramsoc.2006.11.079 ↗
17. Electroconductive Alumina–TiC–Ni nanocomposites obtained by spark plasma sintering10.1016/j.ceramint.2011.01.033 ↗
18. Electrical discharge machining of metal doped Y-TZP/TiC nanocomposites10.1016/j.jeurceramsoc.2015.05.008 ↗
19. Wire electrical discharge machining of 3Y-TZP/Ta ceramic-metal composites10.1016/j.jallcom.2017.12.221 ↗
20. Microstructure and mechanical properties of TiN/Si3N4 nanocomposites by spark plasma sintering (SPS)10.1016/j.jallcom.2010.08.116 ↗
21. Hardness and flexural strength of single-walled carbon nanotube/alumina composites10.1007/s10853-014-8419-5 ↗
22. Electrically conductive CNT-dispersed silicon nitride ceramics10.1111/j.1551-2916.2005.00539.x ↗
23. Electrically conductor black zirconia ceramic by SPS using graphene oxide10.1007/s10832-017-0076-z ↗
24. A critical evaluation of indentation techniques for measuring fracture toughness: II, strength method10.1111/j.1151-2916.1981.tb10321.x ↗
25. Calibration curve for quantitative analysis of the monoclinic-tetragonal ZrO2 system by X-Ray diffraction10.1111/j.1151-2916.1984.tb19715.x ↗
26. X-Ray determination of transformation depths in ceramics containing tetragonal ZrO210.1111/j.1151-2916.1981.tb10285.x ↗
27. Mechanics of transformation-toughening in brittle materials10.1111/j.1151-2916.1982.tb10426.x ↗
28. Average grain size in polycrystalline ceramics10.1111/j.1151-2916.1969.tb11975.x ↗
29. Mechanical properties of zirconia toughened alumina with 10–24vol.% 1.5mol% Y-TZP reinforcement10.1016/j.jeurceramsoc.2012.02.057 ↗
30. Mechanical properties of zirconia toughened alumina with 10–24vol.% 1Y-TZP reinforcement10.1016/j.jeurceramsoc.2012.06.019 ↗
31. The influence of stabilizer concentration on the mechanical properties of alumina – 17 vol% zirconia (0.6Y-2Y) composites properties of alumina – 17 vol% zirconia (0.6Y-2Y) composites
32. Landfried · 2014
33. Percolation and tunneling in composite materials10.1142/S0217979204025336 ↗
34. Piezo-spectroscopic analysis of the residual stresses in zirconia-toughened alumina ceramics: the influence of the tetragonal-to-monoclinic transformation10.1016/S0921-5093(99)00383-4 ↗
35. Toughening of a particulate-reinforced ceramic-matrix composite by thermal residual stress10.1111/j.1151-2916.1990.tb05209.x ↗
36. Landfried · 2014
37. Crack propagation behavior of alumina with different grain sizes under static and cyclic fatigue10.4028/www.scientific.net/KEM.317-318.449 ↗
38. Model for toughness curves in two-phase ceramics: II, microstructural variables10.1111/j.1151-2916.1993.tb07760.x ↗
39. Grigull · 1990