Effect of binding system on the compressive behaviour of refractory mortars
Source abstract
Abstract
Abstract In refractory masonry lining of industrial furnaces the compressibility of mortars is critical for the thermo-mechanical integrity of the structure. Compressive stress–strain behaviour of refractory mortars has been measured during drying at room temperature and in the service temperature range of 300–1400 °C. The results have been explained using fractographic analysis and distinct element method computer modelling. The mortar failure has been shown to occur due to formation of shear bands of micro-cracks. The propagation of cracks preferably follows the shortest path between larger pores and is influenced by grain cohesion and interlocking. Tests with mortars featuring calcium aluminate cement, mono aluminium phosphate, water glass and bentonite clay binders have indicated that besides increasing the cohesion between the grains the binder reduces the internal friction that promotes higher compressibility. It has been found that the mortar with clay has the highest compressibility. The mortar with cement shows the most stable behaviour.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Concrete and Cement Materials Research · Building materials and conservation · Rock Mechanics and Modeling
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (28)
Show source-provided references
1. Banerjee · 1998
2. Shinohara · 1998
3. Schacht · 1995
4. Green and early age compressive strength of extruded cement mortar monitored with compression tests and ultrasonic techniques10.1016/j.cemconres.2005.09.005 ↗
5. Brandt · 2009
6. Experimental analysis of compaction of concrete and mortar10.1002/nag.178 ↗
7. Role of porosity in controlling the mechanical and impact behaviours of cement-based materials10.1016/j.ijimpeng.2007.01.002 ↗
8. Relationship between porosity, permeability and ultrasonic parameters in sound and damaged mortar
9. Compression of granular materials10.1139/T08-123 ↗
10. Failure of cemented granular materials under simple compression: experiments and numerical simulations10.1007/s00707-009-0160-9 ↗
11. A plasticity model for powder compaction process incorporating particle deformation and rearrangement10.1016/j.ijsolstr.2007.11.021 ↗
12. Effect of elevated temperatures on the residual mechanical properties of high-performance mortar10.1016/S0008-8846(02)00709-3 ↗
13. Castro Olivera · 2003
14. Mechanics of masonry in compression10.1061/(ASCE)0733-9445(1985)111:4(857) ↗
15. Dosification of a cement-talc-chamotte refractory mortar subjected to thermal shock10.1016/0008-8846(92)90096-E ↗
16. Alumino-silicate mortars with phosphate bond
17. Verruijt · 2012
18. http://www.itascacg.com.
19. DEM analysis of bonded granular geomaterials10.1002/nag.728 ↗
20. In situ X-ray diffraction and Young's modulus measurement during heat treatment of high-alumina cement castables10.1111/j.1151-2916.2001.tb00702.x ↗
21. Castable refractory concretes10.1179/095066001101528439 ↗
22. Sodium silicate glass as an inorganic binder in foundry industry
23. Contributions to the mechanism of water glass hardening by using thermal analysis methods and X-ray diffractometry10.1007/BF02055939 ↗
24. Dehydration and hydration of montmorillonite at elevated temperatures and pressures monitored using synchrotron radiation
25. Routschka · 2007
26. Montmorillonite: high temperature reactions and classification
27. Improvement of the temperature resistance of aluminium-matrix composites using an acid phosphate binder10.1007/BF00363335 ↗
28. Nowak · 2005