Preparation and corrosion resistance of nonstoichiometric lanthanum zirconate coatings
Source abstract
Abstract
Abstract Lanthanum zirconate is a promising thermal barrier coating material owing to its excellent thermophysical properties and La plays the key role in its corrosion resistance. Here, an amorphous precursor is used as raw feedstock material so as to synthesize lanthanum zirconate coatings with tailorable composition by atmospheric plasma spray (APS). Three lanthanum zirconate coatings of La1.7Zr2.3O7.15, La2.0Zr2.0O7.0 and La2.3Zr1.7O6.85 are fabricated. Furthermore, the corrosion resistance of the as-sprayed coatings against CaO-MgO-Al2O3-SiO2 at 1250℃ is investigated. The increased La content promotes the formation of a sealing layer of the crystalline Ca2La8(SiO4)6O2 apatite, which slows down the penetration of molten CaO-MgO-Al2O3-SiO2. Therefore, the infiltration rate of the La2.3Zr1.7O6.85 coating decreased up to 42.6 % compared with the other two coatings. This work develops a feasible preparation strategy to control the La composition for the improved corrosion resistance, which is expected to guide the future coating design and synthesis for the materials with big composition changes during the APS process.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: High-Temperature Coating Behaviors · Nuclear materials and radiation effects · Nuclear Materials and Properties
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (40)
Show source-provided references
1. Thermal-barrier coatings for more efficient gas-turbine engines10.1557/mrs.2012.232 ↗
2. Advanced structural ceramics in aerospace propulsion10.1038/nmat4687 ↗
3. Advances on strategies for searching for next generation thermal barrier coating materials10.1016/j.jmst.2018.11.016 ↗
4. Role of environmental deposits and operating surface temperature in spallation of air plasma sprayed thermal barrier coatings10.1016/S0257-8972(96)02994-5 ↗
5. Zirconates as new materials for thermal barrier coatings10.1111/j.1151-2916.2000.tb01506.x ↗
6. Thermochemical interaction of thermal barrier coatings with molten CaO-MgO-Al2O3-SiO2(CMAS) deposits10.1111/j.1551-2916.2006.01209.x ↗
7. Jet engine coatings for resisting volcanic ash damage10.1002/adma.201004783 ↗
8. Thermal stability of lanthanum zirconate plasma-sprayed coating10.1111/j.1151-2916.2001.tb00962.x ↗
9. Theoretical elastic stiffness, structural stability and thermal conductivity of La2T2O7 (T=Ge, Ti, Sn, Zr, Hf) pyrochlore10.1016/j.actamat.2010.04.031 ↗
10. Ceramic materials for thermal barrier coatings10.1016/S0955-2219(03)00129-8 ↗
11. Thermal conductivity of rare earth zirconate pyrochlore from first principles10.1016/j.scriptamat.2013.01.010 ↗
12. Theoretical elastic stiffness, structure stability and thermal conductivity of La2Zr2O7 pyrochlore10.1016/j.actamat.2006.12.035 ↗
13. Composition‐dependent intrinsic defect structures in pyroclore RE2B2O7 (RE =La, Nd, Gd; B = Sn, Hf, Zr)10.1111/jace.16705 ↗
14. Composition dependent intrinsic defect structures in ASnO3 (A = Ca, Sr, Ba)10.1016/j.jmst.2019.10.015 ↗
15. Recent progress in thermal/environmental barrier coatings and their corrosion resistance
16. Infiltration-inhibiting reaction of gadolinium zirconate thermal barrier coatings with CMAS melts10.1111/j.1551-2916.2007.02175.x ↗
17. Plasma-sprayed La2Ce2O7 thermal barrier coatings against calcium-magnesium-alumina-silicate penetration10.1016/j.jeurceramsoc.2014.02.031 ↗
18. Degradation of La2Zr2O7 and other novel EB-PVD thermal barrier coatings by CMAS (CaO-MgO-Al2O3-SiO2) and volcanic ash deposits10.1016/j.surfcoat.2013.07.029 ↗
19. Hot corrosion behaviour of La2(Zr0.7Ce0.3)2O7 thermal barrier coating ceramics exposed to molten calcium magnesium aluminosilicate at different temperatures10.1016/j.corsci.2015.08.031 ↗
20. Improved resistance of lanthanum zirconate coatings to calcium-magnesium-alumina-silicate corrosion through composition tailoring10.1016/j.ceramint.2018.04.239 ↗
21. Preparation of lanthanum zirconate films with a widely controllable La/Zr ratio by LCVD10.1016/j.ceramint.2018.03.088 ↗
22. Influence of composition on molten sulfate-vanadate salt corrosion resistance of lanthanum zirconate coatings10.1016/j.ceramint.2018.09.086 ↗
23. Laser chemical vapour deposition: materials, modelling, and process control10.1179/095066001771048727 ↗
24. Contribution a l’etude des systemes zircone-oxydes des lanthanides au voisinage de la fusion
25. Energie Electrostatique des reseaux pyrochlore10.1016/S0022-3697(73)80163-5 ↗
26. 1967
27. Plasma spraying of ceramics with particular difficulties in processing
28. Effect of non-stoichiometry and synthesis temperature on the structure and conductivity of Ln2+xM2−xO7−x/2 (Ln=Sm–Gd; M=Zr, Hf; x=0-0.286)10.1016/j.ssi.2006.11.001 ↗
29. Improving atmospheric plasma spraying of zirconate thermal barrier coatings based on particle diagnostics
30. CaO-MgO-Al2O3-SiO2 corrosion behavior of air-plasma-sprayed (LaxYb1-x)2Zr2O710.1111/jace.16044 ↗
31. Preparation and thermophysical properties of La2Zr2O7 coatings by thermal spraying of an amorphous precursor10.1007/s11666-011-9667-4 ↗
32. Melting and oxidation behavior of in-flight particles in plasma spray process10.1016/j.ijheatmasstransfer.2005.07.019 ↗
33. Fundamental studies associated with the plasma spray process10.1016/0257-8972(88)90083-7 ↗
34. Plasma spraying modeling: particle injection in a time-fluctuating plasma jet10.1016/j.surfcoat.2008.04.028 ↗
35. Study by Raman spectroscopy of order-disorder phenomena occurring in some Binary oxides with fluorite-related structures10.1002/jrs.1250050208 ↗
36. Characterization of anion disorder in zirconate A2B2O7 compounds by Raman spectroscopy10.1111/j.1151-2916.1979.tb19107.x ↗
37. Structural properties and the fluorite–pyrochlore phase transition in La2Zr2O7: The role of oxygen to induce local disordered states10.1016/j.jallcom.2016.05.347 ↗
38. G.V. Subba Rao, Oxide pyrochlores—a review10.1016/0079-6786(83)90001-8 ↗
39. Plasma sprayed gadolinium zirconate thermal barrier coatings that are resistant to damage by molten Ca–Mg–Al–silicate glass10.1016/j.surfcoat.2012.03.051 ↗
40. Mitigation of damage from molten fly ash to air-plasma-sprayed thermal barrier coatings10.1016/j.msea.2011.06.041 ↗