journal article·2021-02Open access

Low Temperature Degradation and Mechanical Properties of Alumina Reinforced Ceria-Zirconia by Colloidal Processing

D. Tovar-Vargas, B. Ferrari, A.J. Sanchez-Herencia, M. Anglada, E. Jimenez-Pique

Abstract

10Ce-TZP base composites with 2.5, 5, 10 and 15 wt% alumina were fabricated by colloidal processing from slurries with 41 vol% solid load in order to investigate the effects of alumina in the final composites aging and mechanical properties. Alumina particle surface charge was modified with the addition of 3 wt% of PAA. The resulting composites have high relative densities (~ 99%) and homogeneous alumina distribution. The microstructure is refined by the alumina addition resulting in a tetragonal-monoclinic microstructure with monoclinic phase content diminishing with alumina concentration down to 16 vol% in 10Ce-15Al2O3 composite. From the study of hydrothermal aging in autoclave steam at 134 °C and 2 bar pressure, it is concluded that all composites have very high resistance to low temperature degradation. At the same time, mechanical properties were investigated by measuring hardness, elastic modulus, strength and t-m transformation around Vickers and spherical indentations. The t-m transformation extension around imprints prevents the formation of Vickers indentations cracks, which indicates a high level of damage tolerance for all compositions. In particular, for 10Ce-15Al2O3 composite, an excellent combination of hardness (~10 GPa), strength (~1400 MPa), damage tolerance, and resistance to low temperature degradation is achieved.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Advanced ceramic materials synthesis · Advanced materials and composites · Metal and Thin Film Mechanics

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (49)

Show source-provided references
1. The tetragonal-monoclinic transformation in zirconia: Lessons learned and future trends10.1111/j.1551-2916.2009.03278.x ↗
2. Zirconia as a biomaterial10.1016/B978-0-08-055294-1.00017-9 ↗
3. Transformation Toughening in Zirconia-Containing Ceramics10.1111/j.1151-2916.2000.tb01221.x ↗
4. Low-Temperature Degradation of Zirconia and Implications for Biomedical Implants10.1146/annurev.matsci.37.052506.084250 ↗
5. Low‐Temperature Aging of Y‐TZP Ceramics10.1111/j.1151-2916.1999.tb02055.x ↗
6. Effect of Alumina Addition on the Tetragonal‐to‐Monoclinic Phase Transformation in Zirconia–3 mol% Yttria10.1111/j.1151-2916.1991.tb06905.x ↗
7. Phase stability and mechanical properties of zirconia and zirconia composites10.1111/j.1744-7402.2011.02717.x ↗
8. Postsintering Hot Isostatic Pressing of Ceria‐Doped Tetragonal Zirconia/Alumina Composites in an Argon–Oxygen Gas Atmosphere10.1111/j.1151-2916.1989.tb06213.x ↗
9. A comparison of microstructure and mechanical properties of 12Ce-TZP reinforced with alumina and in situ formed strontium- or lanthanum hexaaluminate precipitates10.1016/j.jeurceramsoc.2013.08.037 ↗
10. Zirconia-based composites for biomedical applications: Role of second phases on composition, microstructure and zirconia transformability10.1016/j.jeurceramsoc.2015.04.027 ↗
11. Tough and Strong Ce-TZP/Alumina Nanocomposites Doped with Titania10.1016/S0272-8842(97)00048-5 ↗
12. Introduction to a tough, strong and stable Ce-TZP/MgAl2O4 composite for biomedical applications10.1016/j.jeurceramsoc.2012.02.002 ↗
13. Biaxial flexure strength and low temperature degradation of Ce-TZP/Al2O3nanocomposite and Y-TZP as dental restoratives10.1002/jbm.b.31131 ↗
14. Towards long lasting zirconia-based composites for dental implants: Part I: Innovative synthesis, microstructural characterization and in vitro stability10.1016/j.biomaterials.2015.01.018 ↗
15. Towards long lasting zirconia-based composites for dental implants: Transformation induced plasticity and its consequence on ceramic reliability10.1016/j.actbio.2016.11.040 ↗
16. High‐Toughness Ce‐TZP/Al2O3 Ceramics with Improved Hardness and Strength10.1111/j.1151-2916.1991.tb07315.x ↗
17. Colloidal Processing of Ceramic10.1111/j.1151-2916.2000.tb01560.x ↗
18. Influence of the Dispersant Structure on Properties of Electrostatically Stabilized Aqueous Alumina Suspensions10.1016/S0955-2219(96)00151-3 ↗
19. Optimization of the rheological properties of alumina slurries for ceramic processing applications Part II: Spray-drying10.1016/S0955-2219(00)00232-6 ↗
20. Rheological behavior and slip casting of Al2O3-Ni aqueous suspensions10.1111/j.1551-2916.2006.01045.x ↗
21. Novel colloidal approach for the microstructural improvement in Ti(C,N)/FeNi cermets10.1016/j.jallcom.2017.07.034 ↗
22. Alumina nanocomposites from powder-alkoxide mixtures10.1016/S1359-6454(01)00413-X ↗
23. Slip Casting of Yttria‐Stabilized Tetragonal Zirconia Polycrystals10.1111/j.1151-2916.1988.tb05788.x ↗
24. Aqueous processing of fine ZrO2 particles10.1016/j.colsurfa.2004.12.012 ↗
25. Formation characterization and rheological properties of zirconia and ceria-stabilized zirconia
26. Two-Phase Polycrystalline Ceramics
27. Phase Analysis in Zirconia Systems10.1111/j.1151-2916.1972.tb11290.x ↗
28. Calibration Curve for Quantitative Analysis of the Monoclinic‐Tetragonal ZrO2 System by X‐Ray Diffraction10.1111/j.1151-2916.1984.tb19614.x ↗
29. On the Vickers Indentation Fracture Toughness Test10.1111/j.1551-2916.2006.01482.x ↗
30. Contact damage in a Ce-TZP/Al2O3nanocomposite10.1016/j.jeurceramsoc.2011.05.022 ↗
31. Simple Expressions for the Evaluation of Stresses in Sphere-Loaded Disks Under Biaxial Flexure
32. Effect of calcia co-doping on ceria-stabilized zirconia10.1016/j.jeurceramsoc.2017.12.053 ↗
33. An improved technique for determining hardness and elastic modulus using load and displacement sensing indentation experiments10.1557/JMR.1992.1564 ↗
34. A Mechanism for Non‐Newtonian Flow in Suspensions of Rigid Spheres10.1122/1.548848 ↗
35. Rheology of non-Newtonian fluids: A new flow equation for pseudoplastic systems10.1016/0095-8522(65)90022-X ↗
36. Influence of sintering conditions on low-temperature degradation of dental zirconia10.1016/j.dental.2014.03.005 ↗
37. Suspension stability and sintering influence on yttria-stabilized zirconia fabricated by colloidal processing10.1016/j.ceramint.2013.10.123 ↗
38. Quantitative analysis of monoclinic phase in 3Y-TZP by Raman spectroscopy10.1111/j.1551-2916.2010.03635.x ↗
39. Interest of Raman spectroscopy for the study of dental material: The zirconia material example10.1016/j.irbm.2010.10.004 ↗
40. Low temperature degradation of laser patterned 3Y-TZP: Enhancement of resistance after thermal treatment10.1016/j.jeurceramsoc.2017.10.044 ↗
41. Critical influence of alumina content on the low temperature degradation of 2-3mol% yttria-stabilized TZP for dental restorations10.1016/j.jeurceramsoc.2014.09.018 ↗
42. Enhancement of mechanical properties of ceria-calcia stabilized zirconia by alumina reinforcement10.1016/j.jeurceramsoc.2020.02.002 ↗
43. Metastability of the Martensitic Transformation in a 12mol% Ceria-Zriconia Alloy - I Deformation and Fracture Observations10.1111/j.1151-2916.1989.tb07652.x ↗
44. A fracture mechanics analysis of indentation-induced Palmqvist crack in ceramics10.1007/BF00725625 ↗
45. Fatigue Crack Propagation in Ceria‐Partially‐Stabilized Zirconia (Ce‐TZP)‐Alumina Composites10.1111/j.1151-2916.1990.tb06706.x ↗
46. Ce-TZP/Al2O3 nanocomposites as a bearing material in total joint replacement10.1002/jbm.10182 ↗
47. Fracture toughness of dental zirconia before and after autoclaving10.2109/jcersj2.118.406 ↗
48. Fracture toughness, strength and slow crack growth in a ceria stabilized zirconia-alumina nanocomposite for medical applications10.1016/j.biomaterials.2008.05.021 ↗
49. Transformation Zone Shape Effects on Crack Shielding in Ceria-Partially-Stabilized Zirconia (Ce-TZP)-Alumina Composites10.1111/j.1151-2916.1992.tb04376.x ↗