Abstract Many ceramic structural applications involve a combination of tensile (mode I) and shear (mode II) loading conditions. Quantitative fractography was performed on monolithic and R -curve materials. Soda-lime-silica glass was selected as the monolithic material. A mica glass ceramic was selected to represent R -curve materials. Mixed-mode fracture surfaces in both materials were characterized by an absence of the mist region. For the mica glass ceramic, crack-to-mirror size ratios were found to be a function of the crack length and mode mixity. Hackle markings on mixed-mode fracture surfaces appear as lances and differ from those observed on surfaces failed in pure Mode I. Atomic force microscopy showed that the features in different regions on the mixed-mode fracture surfaces are similar and differ only by scale. The practical implications of these observations are that forensic analyses can be used without a priori knowledge of the loading conditions.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Rock Mechanics and Modeling · Geophysical Methods and Applications · Ultrasonics and Acoustic Wave Propagation

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (43)

Show source-provided references
1. Mixed mode cracking in layered materials10.1016/S0065-2156(08)70164-9 ↗
2. Comparison of DBEM and FEM crack path predictions in a notched shaft under torsion10.1016/j.engfracmech.2010.03.012 ↗
3. Numerical and experimental investigation of mixed-mode fracture parameter on silicon nitride using the Brazilian disc test10.1111/j.1460-2695.2010.01457.x ↗
4. Microcrack model and its significance to hydraulic fracturing and fracture toughness testing
5. Edge chipping of hard materials10.1016/S0263-4368(01)00030-0 ↗
6. Mixed-mode fracture in soda lime glass10.1111/j.1151-2916.1979.tb19055.x ↗
7. Mechanisms of failure from surface flaws in mixed-mode loading10.1111/j.1151-2916.1984.tb09626.x ↗
8. Mixed mode fracture in soda lime glass analyzed by using the generalized MTS criterion10.1016/j.ijsolstr.2008.08.035 ↗
9. Fractography of mixed-mode fracture in soda lime silica glass10.1111/j.1551-2916.2012.05431.x ↗
10. Fracture under complex stress – the angled crack problem10.1007/BF00191106 ↗
11. Fracture toughness of polycrystalline ceramics in combined mode I and mode II loading10.1111/j.1151-2916.1989.tb05957.x ↗
12. Mixed-mode fracture in biaxial stress state: application of the diametral-compression (Brazilian disk) test10.1016/0013-7944(87)90032-4 ↗
13. Corning, Inc., Brochure for Macor.
14. Mechanical properties of mica glass ceramics10.1111/j.1151-2916.1995.tb08472.x ↗
15. Deformation and fracture of mica containing glass ceramics in Hertzian contacts10.1557/JMR.1994.0762 ↗
16. Mixed-mode fracture in an R-curve material10.1016/j.engfracmech.2011.11.019 ↗
17. Effect of flaw shape on strength of ceramics10.1111/j.1151-2916.1976.tb09406.x ↗
18. Effect of grinding on flaw geometry and fracture of glass10.1111/j.1151-2916.1977.tb15484.x ↗
19. Randall · 1967 · 88
20. A study of the rupture of glass
21. Breaking stress of glass determined from dimensions of fracture mirrors10.1111/j.1151-2916.1959.tb13560.x ↗
22. Comparison of the stress–intensity and Johnson-and-Holloway criteria for crack branching in rectangular bars10.1111/j.1151-2916.1987.tb05707.x ↗
23. Mecholsky · 1994
24. Fracture of ceramics10.1002/adem.200700347 ↗
25. Estimation of fracture energy from the work of fracture and fracture surface area: I. Stable crack growth10.1007/s10704-009-9350-7 ↗
26. Scanning tunneling microscope observations of the mirror region of silicate glass fracture surfaces10.1557/JMR.1994.0476 ↗
27. Fracture mechanics description of fracture mirror formation in single crystals10.1007/BF00035717 ↗
28. Mecholsky · 2002
29. Relation of stresses near a crack to the crack extension force
30. Brittleness dependence of crack branching in ceramics10.1111/j.1151-2916.1986.tb04743.x ↗
31. Mixed-mode fracture of hot pressed Si3N410.1111/j.1151-2916.1985.tb15238.x ↗
32. Stress intensity factors for semicircular cracks II10.1115/1.3607862 ↗
33. Three dimensional stress distribution around an elliptical crack under arbitrary loadings10.1115/1.3625127 ↗
34. A critical review of crack tip stress intensity factors for semi elliptic cracks10.1111/j.1460-2695.1981.tb01127.x ↗
35. Smith · 1974
36. Hussain · 1974 · 2
37. On the crack extension in plates under plane loading and transverse shear10.1115/1.3656897 ↗
38. Mixed mode fracture from controlled surface flaws in hot pressed silicon nitride10.1111/j.1151-2916.1976.tb09458.x ↗
39. Strain energy density factor applied to mixed mode crack problems10.1007/BF00035493 ↗
40. Formation of fracture ‘lances’ in glass10.1016/0013-7944(69)90010-1 ↗
41. Helical crack-front instability in mixed-mode fracture10.1038/nature08862 ↗
42. Rice · 1984
43. Quinn GD. Fractography of ceramics and glasses. NIST Special Publication 960-16: 8–14, 8–17; 2007.