BF slag resistance of β-Si3Al3O3N5 material derived from Al salt cake
Source abstract
Abstract
Abstract In the process of recycling of salt cake from secondary aluminium smelting, it was shown that a significant value addition can be made as β-Si 3 Al 3 O 3 N 5 could be successfully synthesized from the rest product after water-leaching by silicothermal reduction method. In order to evaluate its refractory application, the corrosion behavior in blast furnace slag was investigated under static condition at 1400–1480 °C in the present work. The results show that the β-Si 3 Al 3 O 3 N 5 material has good slag resistance. The apparent activation energy obtained for corrosion process is −388.7 kJ/mol, revealing a more complicated dissolution mechanism. The corrosion process is started with the dissolution of intergranular phase including the iron silicides and glassy phases in the specimens, which is aided by the softening at high temperature and the continuous attack from slag, then followed by the dissolution of β-Si 3 Al 3 O 3 N 5 grains in the slag.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Advanced ceramic materials synthesis · Recycling and utilization of industrial and municipal waste in materials production · Concrete and Cement Materials Research
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (24)
Show source-provided references
1. Gil · 2010 · 258
2. Surface composition, charge and texture of active alumina powders recovered from aluminum dross tailings chemical waste10.1016/S0032-5910(03)00047-0 ↗
3. Osborne · 1995
4. Garret LW. Process for the production of sulfates. US.4337228; 1982.
5. Huckabay DA, Skiathas DA. Aluminium sulfate manufacture from aluminum dross tailings. US.4320098; 1982.
6. Huckabay JA. Method for treatment of aluminum dross oxides. US.4434142; 1984.
7. Oxidation studies of SiAlON/MgAlON ceramics with Fe2O3 and CaO impurities, part II: Phase evolution10.1007/s11663-012-9758-8 ↗
8. Study on the slag corrosion resistance of unfired Al2O3–SiC/β-SiAlON/Ti(C, N)–C refractories10.1016/j.ceramint.2013.07.047 ↗
9. Influence of additives and compositions on the nitridation and formation of SiAlONs produced by reaction bonding and silicothermal reduction10.1016/j.jascer.2013.02.005 ↗
10. Leaching process investigation of secondary aluminium dross: the effect of CO2 on leaching process of salt cake from aluminum remelting process10.1007/s11663-012-9678-7 ↗
11. New heat treatment methods for glass removal from silicon nitride and sialon ceramics10.1023/A:1026782723065 ↗
12. Crystallization of 3M/4X Mg–Si–Al–O–N melts10.1007/BF01114721 ↗
13. Nitride capacities in CaO–SiO2 and CaO–SiO2–Al2O3 melts10.1002/srin.199200459 ↗
14. Nitrogen solubility in CaO–SiO2, CaO–MgO–SiO2 and BaO–MgO–SiO2 melts10.1007/BF02658120 ↗
15. Titration of ammonia in presence of boric acid10.1021/ac50152a031 ↗
16. Meeker · Ind Eng Chem Anal Ed · 1933 · 5 · 39610.1021/ac50086a012 ↗
17. Quantitative description of the microstructure -porosity of sialons and iron silicide inclusions10.1016/j.matchar.2006.01.001 ↗
18. Solid–liquid interactions: the key to microstructural evolution in ceramic10.1016/j.jeurceramsoc.2007.12.010 ↗
19. Corrosion of refractory and ceramic
20. Slag corrosion of gamma aluminum oxynitride10.1002/srin.200200179 ↗
21. Dissolution rate of silicon nitride ceramics into molten CaO–SiO2–Al2O3 slags10.2320/jinstmet1952.59.5_540 ↗
22. Crank · 1975 · 21
23. Dissolution rate of silicon nitride ceramics into molten CaO–Al2O3–SiO2 slags10.1111/j.1151-2916.1997.tb02923.x ↗
24. The equilibrium solubility of nitrogen in aluminosilicate melts10.1007/BF02814918 ↗