Effect of YSZ-incorporated glass-based composite coating on oxidation behavior of K438G superalloy at 1000°C
Source abstract
Abstract
Abstract A glass-based composite coating incorporating YSZ particles was prepared by sintering on K438G superalloy substrates. The YSZ additions increased the cyclic oxidation resistance at 1000 °C, while the formation of zircon resulting from interfacial reactions between YSZ and the glass matrix worked reversely. Besides, the YSZ inclusions changed the crystallization behavior of the glass matrix, and only anorthite precipitated during cyclic oxidation. Due to the synergy of sand-blasting and sealing effect of the glass-based coating, the oxidation behavior of K438G was changed and a layer of alumina instead of chromia formed at the substrate/coating interface. Furthermore, a gahnite layer formed at the alumina/gahnite interface because of interfacial reactions between alumina and the glass matrix, leading to the formation of a bi-layered thermally grown oxide. Thus, the alumina layer was protected from the attack of the active glass matrix. Accordingly, the coated K438G superalloy exhibited satisfactory oxidation resistance at 1000 °C.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: High-Temperature Coating Behaviors · Advanced ceramic materials synthesis · Advanced materials and composites
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (56)
Show source-provided references
1. Progress in coatings for gas turbine airfoils10.1016/S0257-8972(98)00667-7 ↗
2. Coatings for gas turbine materials and long term stability issues10.1016/j.matdes.2004.02.005 ↗
3. High temperature coatings for gas turbine blades: a review10.1016/0257-8972(89)90099-6 ↗
4. Amorphous sol-gel SiO2 film for protection of Ti6Al4V alloy against high temperature oxidation10.1016/j.surfcoat.2006.11.004 ↗
5. Reactive sputter-deposition of alumina films on superalloys and their high-temperature corrosion-resistance10.1016/0257-8972(94)02289-3 ↗
6. Effect of Al2O3 and enamel coatings on 900 (C oxidation and hot corrosion behaviors of gamma-TiAl10.1016/S0921-5093(99)00513-4 ↗
7. Hot corrosion of glass coating on nickel base superalloy10.1016/j.ceramint.2007.03.008 ↗
8. Recent developments in the preparation, characterization and applications of glass- and glass-ceramic-to metal seals and coatings10.1007/s10853-010-5095-y ↗
9. Wetting and sealing of interface between 7056 glass and kovar alloy10.1016/j.matchemphys.2007.04.012 ↗
10. Corrosion resistance and mechanism of steel rebar coated with three types of enamel10.1016/j.corsci.2012.02.024 ↗
11. SiO2-Al2O3-glass composite coating on Ti-6Al-4V alloy: oxidation and interfacial reaction behavior10.1016/j.corsci.2013.05.010 ↗
12. Oxidation protection of gamma-titanium aluminide using glass-ceramic coatings10.1016/j.surfcoat.2008.12.029 ↗
13. Glass-ceramics as oxidation resistant bond coat in thermal barrier coating system10.1016/j.ceramint.2008.07.005 ↗
14. Glass–ceramic coatings on titanium alloys for high temperature oxidation protection: oxidation kinetics and microstructure10.1016/j.corsci.2013.04.041 ↗
15. Metal-glass based composites for novel TBC-systems10.1002/1521-4052(200108)32:8<669::AID-MAWE669>3.0.CO;2-H ↗
16. Comparison between micrometer- and nano-sale glass composites for sealing solid oxide fuel cells10.1111/j.1551-2916.2005.00804.x ↗
17. The effect of enamel coating on the oxidation behavior of Ti3Al based intermetallics at 750°C in air10.1016/j.msea.2007.01.058 ↗
18. The oxidation behavior of TiAlNb intermetallics with coatings at 800°C10.1016/j.surfcoat.2004.11.019 ↗
19. The oxidation and oxygen permeation resistance of quartz particle-reinforced aluminosilicate glass coating on titanium alloy10.1111/j.1551-2916.2011.04587.x ↗
20. Effect of enamel coating on oxidation and hot corrosion behaviors of Ti-24Al-14Nb-3V alloy10.1361/105994906X136151 ↗
21. Synergistic corrosion behavior of coated Ti60 alloys with NaCl deposit in moist air at elevated temperature10.1016/j.corsci.2007.06.007 ↗
22. Oxidation and hot corrosion behavior of a novel enamel-Al2O3 composite coating on K38G superalloy10.1016/j.surfcoat.2005.09.004 ↗
23. Effect of sand blasting and glass matrix composite coating on oxidation resistance of a nickel-based superalloy at 1000°C10.1016/j.corsci.2013.04.022 ↗
24. Preparation and thermal shock behaviorat 1000°C of a glass-alumina-NiCrAlY tri-composite coating on K38G superalloy10.1016/j.surfcoat.2011.11.015 ↗
25. Cyclic oxidation behavior of glass-ceramic composite coatings on superalloy K38G at 1100°C10.1016/j.tsf.2011.01.047 ↗
26. Glass coating on stainless steels for high-temperature oxidation protection mechanisms10.1016/j.corsci.2014.01.033 ↗
27. Phase evolution of SiO2-Al2O3-ZnO-CaO-ZrO2-TiO2-based glass with added YSZ particles10.1111/jace.12307 ↗
28. The elastic and thermo-elastic properties of composite media10.1088/0370-1301/69/8/305 ↗
29. Glass-alumina composite coatings for high temperature corrosion protection. Part I: effect of crystallization and interfacial reaction on the thermo-physical properties10.1016/j.msea.2010.12.090 ↗
30. Ceramic materials for thermal barrier coatings10.1016/S0955-2219(03)00129-8 ↗
31. The tetragonal-monoclinic transformation in zirconia: lessons learned and future trends10.1111/j.1551-2916.2009.03278.x ↗
32. Glass-ceramic protective coating for titanium alloys10.1111/j.1151-2916.2002.tb00547.x ↗
33. Al2O3–ZrO2–SiO2 ternary glasses for molybdenum oxidation barriers10.1111/j.1551-2916.2005.00189.x ↗
34. Nitrogen doping in cuprous oxide films synthesized by radical oxidation at low temperature10.1016/j.matlet.2012.10.083 ↗
35. Microstructure and oxidation resistance of Si–Mo–B coating for C/SiC coated carbon/carbon composites10.1016/j.corsci.2013.03.015 ↗
36. Microstructure stabilization of a novel glass/YSZ composite coating material by adding alumina particles10.1016/j.ceramint.2015.04.047 ↗
37. Interfacial reactions between a SiO2-Al2O3-ZnO-CaO based glass and alpha alumina10.1016/j.surfcoat.2013.04.044 ↗
38. Oxidation behavior of glass-based composite thermal barrier coating on K417G superalloy with a NiCoCrAlY bond coat at 1000°C10.1016/j.surfcoat.2015.02.014 ↗
39. Effect of sand blasting on oxidation behavior of K38G superalloy at 1000°C10.1016/j.corsci.2014.12.015 ↗
40. Protective glass coating for carbon-carbon composites10.1016/S0008-6223(98)00100-6 ↗
41. Felix · 1972
42. High temperature oxidation of superalloys
43. Reaktionstypen bei der oxidation von legierungen
44. High-temperature oxidation resistance of sputtered micro-grain superalloy K38G
45. The effect of nanocrystallization on the selective oxidation and adhesion of A12O3 scales10.1007/BF01670500 ↗
46. The nature of the third-element effect in the oxidation of Fe-xCr-3at.% Al alloys in 1atm O2 at 1000°C10.1016/j.corsci.2007.06.019 ↗
47. The third-element effect in the oxidation of Ni-xCr-7Al (x=0 5, 10, 15 at.%) alloys in 1atm O2 at 900–1000°C10.1016/j.corsci.2006.03.008 ↗
48. Interfacial reaction between SiO2-Al2O3-ZnO-CaO based glass coatings and K38G superalloy substrates10.1016/j.surfcoat.2012.11.045 ↗
49. Thermal stability of zircon (ZrSiO4)10.1016/j.jeurceramsoc.2007.12.040 ↗
50. Mechanism of formation of zircon stains10.1111/j.1151-2916.1970.tb12677.x ↗
51. Thermal expansion data of some alkali alumino silicate glasses and their respective glass-ceramic10.1016/0040-6031(85)87104-5 ↗
52. Transformation toughening in zirconia-containing ceramics10.1111/j.1151-2916.2000.tb01221.x ↗
53. Preparation of zirconia-toughened bioactive glass-ceramic composite by sinter-hot isostatic pressing10.1111/j.1151-2916.1992.tb05545.x ↗
54. Garvie · 1970
55. Bose · 2007
56. The measurement of strains within the bulk of aged and as-sprayed thermal barrier coatings using synchrotron radiation