journal article·2014-11

The influence of Ti addition on fracture toughness and failure of directionally solidified LaB6–ZrB2 eutectic composite with monocrystalline matrix

Halyna Volkova, Vladimir Filipov, Yurij Podrezov

Publisher page

Abstract

Abstract Fracture toughness and failure mechanism of directionally solidified eutectic composites LaB 6 –ZrB 2 and LaB 6 –(Zr 0,9 Ti 0,1 )B 2 were investigated. The addition of Ti increases the cohesion strength of the matrix–fiber interface, causes redistribution of stresses in the whole composite, and thus influences the mechanism of crack propagation. Fracture toughness of composites was determined by Brazilian test. The central crack was introduced in the plane, parallel to the axis of the eutectic rod, in direction, perpendicular to the axis. Such experimental setup enables to investigate the interaction of crack with fiber–matrix interface and eliminates the effect of other factors on K 1 C . The present investigation shows that Ti additions to LaB 6 –ZrB 2 result in up to 25% increase of fracture toughness of the composites.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Advanced ceramic materials synthesis · Rare-earth and actinide compounds · Boron and Carbon Nanomaterials Research

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (26)

Show source-provided references
1. Directionally solidified ceramicfiber-reinforced boride composites10.1023/A:1011334230820 ↗
2. Some crystal chemistry relationships in eutectic cocrystallization of d- and f-transition metal borides10.1016/0925-8388(94)05047-3 ↗
3. Some peculiarities of structure formation in d- and f-transition metals boride alloys10.1063/1.40787 ↗
4. Anisotropy of microhardness of directionally crystallized materials based on lanthanum hexaboride10.1007/BF02365754 ↗
5. Volodymyr · 2011
6. Crystal chemistry of eutectic growth of d- and f-transition metals borides
7. Interface crystallography and structure in LaB6–ZrB2 directionally solidified eutectics10.1111/j.1551-2916.2007.01812.x ↗
8. Matrix fracture in fiber-reinforced ceramics10.1016/0022-5096(86)90035-9 ↗
9. Crack deflection at an interface between dissimilar elastic materials – role of residual stresses10.1016/0020-7683(94)90025-6 ↗
10. Crack bifurcation features in laminar specimens with fixed total thickness10.1016/S0266-3538(02)00040-4 ↗
11. Prediction of fracturess toughness of ceramic composites as function of microstructure: II. Analytical model10.1016/j.jmps.2012.09.011 ↗
12. Crystallographic characterization and indentation mechanical properties of LaB6–ZrB2 directionally solidified eutectics10.1023/B:JMSC.0000041695.40772.56 ↗
13. Microstructure, mechanical performance and oxidation mechanism of boride in situ composites10.1016/S0266-3538(00)00187-1 ↗
14. Effect of Zr substitution by Ti on growth direction and interface structure of LaB6–TixZr1−xB2 directionally solidified eutectics10.1016/j.jeurceramsoc.2014.01.026 ↗
15. Some peculiarities of eutectic crystallization of LaB6–(Ti,Zr)B210.1006/jssc.2000.8830 ↗
16. Chaoshui · 1993
17. Determination of fracture toughness of anisotropic rocks by boundary element method10.1007/s00603-005-0089-9 ↗
18. 1987
19. Properties of LaB6 elucidated by density functional theory10.1103/PhysRevB.70.193403 ↗
20. The stress distribution mound a crack perpendicular to an interface between materials10.1007/BF00182624 ↗
21. Temperature dependence of thermal expansion and elastic constants of single crystals of ZrB2 and the suitability of ZrB2 as a substrate for GaN film10.1063/1.1525404 ↗
22. Elastic constants of LaB6 at room temperature10.1016/0038-1098(77)90272-1 ↗
23. Bornstein L.The Landolt-Bornstein Database on line, 2005, Available from http://www.springermaterials.com/docs/index.html
24. Elastic-stiffness coefficients of titanium diboride10.6028/jres.114.024 ↗
25. 1970
26. Anisotropic elastic constants and thermal expansivities in monocrystal CrB2, TiB2, and ZrB210.1016/j.actamat.2009.08.058 ↗