Interfacial behavior on Al2O3/HAYNES® 214™ joints fabricated by solid state bonding technique with Ni or Cu–Ni–Cu interlayers
Source abstract
Abstract
Abstract The residual stresses due to the difference in thermal expansion between ceramic and metal is a significant parameter to control during the fabrication of ceramics/metal joint. In this work, residual stress distribution, after solid state bonding of different joints, was measured using X-ray diffraction (XRD) and Vickers Indentation Fracture (VIF) methods. Tensile stress concentration in alumina caused by the thermal expansion mismatch in the Al 2 O 3 /Ni/Ni alloy (HAYNES ® 214™) joint severely deteriorated the assembly and caused cracks in alumina. To solve this problem, this paper shows that the use of a Cu/Ni/Cu multi-layer, associated with the direct copper bonding method (DCB), by pre-oxidation of copper, reduces significantly the tensile residual stresses in alumina material. Consequently, this process offers the possibility of producing an interlayer with a high melting temperature and hence joints which can withstand high-temperatures.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Advanced ceramic materials synthesis · Advanced materials and composites · 3D IC and TSV technologies
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (55)
Show source-provided references
1. Calculation and experimental determinations of the residual stress distribution in alumina/Ni/alumina and alumina/Ni/nickel alloy systems10.1007/s10853-010-4502-8 ↗
2. Study of SiC–nickel alloy bonding for high temperature applications10.1016/j.jeurceramsoc.2008.06.035 ↗
3. Microstructural development during diffusion bonding of α-silicon carbide to molybdenum10.1016/0921-5093(94)09633-8 ↗
4. Effect of thermal residual stresses on the strength for both alumina/Ni/alumina and alumina/Ni/nickel alloy bimaterials10.1007/s10853-009-3426-7 ↗
5. Larson · 1985
6. Ceramic joining. I. Partial transient liquid-phase bonding of alumina via Cu/Pt interlayers10.1007/BF00363367 ↗
7. New approaches to joining ceramics for high-temperature applications
8. Ceramic joining II partial transient liquid-phase bonding of alumina via Cu/Ni/Cu multilayer interlayers10.1007/BF00356663 ↗
9. Ceramic/metal joining for structures and materials10.1051/jp4:19937203 ↗
10. Reactions and microstructure at selected ceramic/metal interfaces10.1080/10426919408934924 ↗
11. Nicholas · 1990
12. Interfacial reactions between metals and oxides during sealing
13. Nicholas · 1989
14. Progress in joining of advanced materials
15. Theoretical fundamentals and technology of electron beam welding ceramics to metals10.1080/09507119509548788 ↗
16. Ultrasonic welding of ceramics/metals using inserts10.1016/S0924-0136(97)00372-5 ↗
17. A new method for explosive welding of AI/ZrOz joint using regulated underwater shock wave10.1016/S0924-0136(98)00286-6 ↗
18. Active metal brazing
19. Diffusion bonding stainless steel to alumina using aluminium interlayers10.1007/BF01203505 ↗
20. Effect of residual stress on the strength of an alumina–steel joint by partial transient liquid phase (PTLP) brazing10.1016/S0924-0136(02)00010-9 ↗
21. Preoxidation of the Cu layer in direct bonding technology10.1016/S0169-4332(03)00243-5 ↗
22. Progress in joining ceramics to metals10.1016/S1006-706X(06)60032-0 ↗
23. The strength and fracture of alumina bonded with aluminum alloys10.1016/0001-6160(89)90077-1 ↗
24. Effect of residual stress on the strength of an alumina–steel joint by partial transient liquid phase (PTLP) brazing10.1016/S0924-0136(02)00010-9 ↗
25. Nickel-alumina bonds: mechanical properties related to interfacial chemistry10.1016/0955-2219(95)00187-5 ↗
26. Experimental observations of substrate fracture caused by residually stressed films10.1111/j.1151-2916.1990.tb06564.x ↗
27. Finite elements analysis and X-ray measurement of the residual stress of ceramic/metal joints10.1016/S0924-0136(96)02838-5 ↗
28. Tréheux · 1989
29. The strength of ceramics bonded with metals10.1016/0001-6160(88)90304-5 ↗
30. Analysis and measurements of residual stress distribution of vanadium/ceramics joints for fusion reactor applications10.1016/S0022-3115(98)00330-4 ↗
31. Colin C. Les assemblages métal-céramique. Thesis Ecole des mines de Paris; 1991.
32. Direct bonding of metals to ceramics by the gas–metal eutectic method10.1149/1.2134293 ↗
33. A new hybrid power technique utilizing a direct copper to ceramic bond10.1109/T-ED.1976.18517 ↗
34. Jürgen · 2000 · 315
35. Thermal and electrical aging of DBC substrates
36. A new method for preparation of direct bonding copper substrate on Al2O3
37. Interfaces in bioceramics: surface energetics and interfacial interactions10.4028/www.scientific.net/KEM.224-226.417 ↗
38. Stages of reactive wetting10.4028/www.scientific.net/KEM.280-283.1801 ↗
39. A highly linear and efficient differential CMOS power amplifier with harmonic control10.1109/JSSC.2006.874276 ↗
40. A review of recent investigations on zirconia joining for biomedical applications
41. Study of copper–alumina bonding10.1007/BF00544543 ↗
42. Metal–ceramic solid state bonding: mechanisms and mechanics10.1016/0956-716X(94)90526-6 ↗
43. Adhesion and reactivity in the copper–alumina system10.1163/156856199X00280 ↗
44. A test specimen for determining the fracture resistance of bimaterial interfaces10.1115/1.3176069 ↗
45. Adhesion and residual stresses determination of thermally sprayed molybdenum on steel10.1016/S0257-8972(02)00818-6 ↗
46. Determination of Kscc by indentation in ceramics10.1007/BF00544209 ↗
47. Measurement of thin-layer surface stresses by indentation fracture10.1007/BF00980772 ↗
48. Solid state bonding of Al2O3 with Cu, Ni and Fe: characteristics and properties10.1023/A:1004397019927 ↗
49. Kubashewski · 1979
50. Influence of Cu2O and CuAlO2 interphases on crack propagation at Cu/α-Al2O3 interfaces10.1111/j.1151-2916.1997.tb02847.x ↗
51. Silver-alumina solid state bonding: influence of the work hardening of the metal10.1016/0956-7151(93)90067-3 ↗
52. Damages and cracks in ceramic/metal interfaces10.1051/jp4:19937164 ↗
53. Relationship between the nature of dopants and charging or mechanical properties of ceramics
54. Electric charge trapping, residual stresses and properties of ceramics after metal–ceramics bonding10.1016/j.jeurceramsoc.2011.10.025 ↗
55. Wettability of solids by liquid metals10.1016/B978-0-12-571814-1.50011-7 ↗