Hot corrosion of cordierite/mullite composites by Na-salts

Junichi Takahashi, Yoshie Kawai, Shiro Shimada

Publisher page

Abstract

Abstract Cordierite/mullite (C/M) ceramic composites were corroded by NaCl and Na 2 SO 4 at 1000 °C for 24 h. The predominant corrosion products in attack by the Na-salts were found to be nepheline and carnegieite for the cordierite and mullite component, respectively. NaCl attacked both components with different corrosion rates, producing corrosion layers consisting of two distinct regions where both cordierite and mullite were chemically attacked near the surface region and only the cordierite phase was damaged in the succeeding inner part. In the hot corrosion by Na 2 SO 4 , on the other hand, only the cordierite component was severely attacked in the composites, resulting in occurrence of selective corrosion. Thus, the corrosion of the C/M composites by the Na-salts proceeded through the path of the less resistive cordierite component at 1000 °C in air.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Advanced ceramic materials synthesis · MXene and MAX Phase Materials · Aluminum Alloys Composites Properties

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (22)

Show source-provided references
1. Corrosion of cordierite ceramics by sodium sulphate at 1000 °C10.1007/BF02385645 ↗
2. The latest status of the development of the advanced ceramic tube filter
3. Assessment of porous ceramic materials for hot gas filtration applications
4. Preparation and properties of mullite-cordierite composites
5. Thermal expansion and microstructure of cordierite and mullite composite
6. Considering some thermal applications for cordierite and cordierite-mullite materials
7. The mechanical properties of cordierite–mullite composites as a function of temperature
8. Thermal, mechanical, and dielectric properties of mullite-cordierite composites
9. Microstructure development in mullite-cordierite ceramics10.1111/j.1151-2916.1989.tb09733.x ↗
10. Hot corrosion of cordierite ceramics by Na- and K-salts10.1016/S0955-2219(98)00007-7 ↗
11. Aluminous refractoriesalkali reactions
12. Alkali attack on a mullite refractory in the grand forks energy technology center slagging gasifier10.1007/BF02833526 ↗
13. Action of alkali and alkali-vanadium oxide slags on alumina-silica refractories10.1111/j.1151-2916.1962.tb11082.x ↗
14. Corrosion of mullite by molten salts10.1111/j.1151-2916.1996.tb08951.x ↗
15. The system Na2O–Al2O3–SiO210.2475/ajs.254.3.129 ↗
16. Corrosion of mullite refractory by alkaline vapor10.2109/jcersj1950.77.886_208 ↗
17. Babushkin · 1985
18. Chase, M. W. Jr. (ed.), NIST-JANAF Thermochemical Tables. J. Phys. Chem. Ref. Data Monograph No. 9 (Part I and II). Am. Chem. Soc. and Am. Inst. Phys., Washington DC, 1998.
19. 1964
20. Sata, T. et al., Advances in Ceramics, vol. 10, ed. W. D. Kingery. Am. Ceram. Soc., Columbus, 1985, pp. 541.
21. 1967
22. 1964