Comparison of residual strength behavior after indentation, scratching and grinding of zirconia-based ceramics for medical-technical applications

B. Denkena, A. Wippermann, S. Busemann, M. Kuntz, L. Gottwik

Publisher page

Abstract

Abstract In this study, three methods of characterizing the damage tolerance of different zirconia-based ceramics for medical-technical applications are presented. The damage is inflicted statically, with Vickers hardness impressions and dynamically by scratching with a Rockwell diamond, as well as by means of a reproducible grinding process. The damage intensity is, in each case, successively increased. The measured strength values as a function of the inflicted damage thus provide information on the grinding robustness of the material. This permits the determination of critical grinding parameters above which the component quality is impaired and, ultimately, the patient is endangered. The continuing pressure to reduce production costs by shortening processing times makes damage tolerant behavior of materials extremely important. Ultimately, this permits the reduction of production costs while maintaining component quality and the guarantee of future patient safety.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Advanced materials and composites · Advanced ceramic materials synthesis · Orthopaedic implants and arthroplasty

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (26)

Show source-provided references
1. Grinding mechanisms and strength degradation for ceramics
2. Strength prediction of machined ceramics by X-Ray diffraction techniques, machining of advanced ceramics
3. Indentation fracture: principles and applications10.1007/BF00823224 ↗
4. Equilibrium penny-like cracks in indentation fracture, (1975)10.1007/BF00557479 ↗
5. A critical evaluation of indentation techniques for measuring fracture toughness: I, direct crack measurements10.1111/j.1151-2916.1981.tb10320.x ↗
6. Multi-scale effects in the strength of ceramics10.1111/jace.13814 ↗
7. Lierse · 1998
8. Wobker · 1991
9. Roth · 1994
10. Scratch damage in zirconia ceramics
11. Residual strength of ground hot isostatically pressed silicon nitride10.1007/BF00585749 ↗
12. Review surface/subsurface damage and fracture strength of ground ceramics10.1016/0924-0136(95)02090-X ↗
13. Bearbeitung keramischer Funktionsflächen für Knieimplantate, Dr.-Ing. Dissertation
14. Marinescu · 2000
15. Efficient improved strength grinding of ceramics
16. Effect of grit depth of cut on strength of ground ceramics10.1016/S0007-8506(07)62220-3 ↗
17. Grinding of reaction bonded silicon nitride (RBSN) ceramic
18. Ceramic steel?10.1038/258703a0 ↗
19. Microstructural design of toughened ceramics10.1111/j.1151-2916.1991.tb06872.x ↗
20. Piezospectroscopic analysis of the residual stresses in the strontium hexaluminate/zirconia (SrAl12O19/ZrO2) System10.1111/j.1151-2916.1999.tb02215.x ↗
21. A comparison of microstructure and mechanical properties of 12Ce-TZP reinforced with alumina and in situ formed strontium- or lanthanum hexaaluminate precipitates10.1016/j.jeurceramsoc.2013.08.037 ↗
22. The influence of platelet-like LaMgAl11O19 on the toughness of 3mol% yttria partially stabilized zirconia ceramic10.1111/ijac.12177 ↗
23. Review structural ceramic nanocomposites: a review of properties and powders' synthesis methods10.3390/nano5020656 ↗
24. Internal stresses in ceramics10.1111/j.1151-2916.1961.tb15475.x ↗
25. Springer Verlag 3., bearb. u. erw
26. Temperature and energy partition for grinding of mixed oxide ceramics10.1007/s11740-017-0757-0 ↗