Effect of sintering temperature on electrical properties of SiC/ZrB2 ceramics
Source abstract
Abstract
Abstract SiC/20 wt% ZrB2 composite ceramics were fabricated via pressureless solid phase sintering in argon atmosphere at different temperature. The effect of sintering temperature on microstructure, electrical properties and mechanical properties of SiC/ZrB2 ceramics was investigated. Electrical resistivity exhibits twice significant decreases with increasing sintering temperature. The first decrease from 1900 °C to 2000 °C is attributed to the obvious decrease of continuous pore channels in as-sintered materials. The second decrease from 2100 °C to 2200 °C results from the improvement of carbon crystallization and the disappearance of amorphous layers enveloping ZrB2 grains. Additionally, the increase of sintered density with increasing temperature caused greatly advance of flexural strength, elastic modulus and Vickers hardness. But excessive temperature is detrimental to flexural strength because of SiC grain growth.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Advanced ceramic materials synthesis · Advanced materials and composites · MXene and MAX Phase Materials
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (32)
Show source-provided references
1. Processing and characterization of fine-grained monolithic SiC ceramic synthesized by spark plasma sintering10.1016/j.msea.2009.12.027 ↗
2. 2.04 - Processing of silicon carbide-based ceramics
3. High-temperature strength of silicon carbide ceramics sintered with rare-earth oxide and aluminum nitride10.1016/j.actamat.2006.08.059 ↗
4. Mechanical properties of hot-forged silicon carbide ceramics10.1016/j.scriptamat.2004.09.012 ↗
5. Clarke · J. Am. Ceram. Soc. · 1999 · 82 · 48510.1111/j.1151-2916.1999.tb01793.x ↗
6. Electrical properties of grain boundaries in polycrystalline compound semiconductors10.1088/0268-1242/5/2/001 ↗
7. Improvement in nonlinear properties and electrical stability of ZnO varistors with B2O3 additives by nano-coating method10.1111/j.1551-2916.2011.04900.x ↗
8. Modern technical aspects of field discharge equipment for excitation systems
9. Highly conductive SiC ceramics containing Ti2CN10.1016/j.jeurceramsoc.2013.11.001 ↗
10. Effect of AlN–Y2O3 addition on the properties and microstructure of in-situ strengthened SiC–TiB2 composites prepared by hot pressing10.1016/j.ceramint.2013.06.105 ↗
11. Electrical and thermal properties of SiC-Zr2CN composites sintered with Y2O3-Sc2O3 additives10.1016/j.jeurceramsoc.2016.09.001 ↗
12. Recent advances in Schottky barrier concepts10.1016/S0927-796X(01)00037-7 ↗
13. Zur Halbleitertheorie der Sperrschicht- und Spitzengleichrichter10.1007/BF01340116 ↗
14. The theory of crystal rectifiers10.1098/rspa.1939.0051 ↗
15. Structural and electrical characterisation of titanium and nickel silicide contacts on silicon carbide10.1016/S0167-9317(01)00604-9 ↗
16. CVD-based tungsten carbide schottky contacts to 6H-SiC for very high-temperature operation10.1007/s11664-000-0080-x ↗
17. Improved Schottky contacts on n-type 4H-SiC using ZrB2 deposited at high temperatures10.1007/s11664-007-0170-0 ↗
18. Transition metal carbides, nitrides, and borides for electronic applications10.1007/BF02914655 ↗
19. Refractory diborides of zirconium and hafnium10.1111/j.1551-2916.2007.01583.x ↗
20. Densification of ZrB2-based composites and their mechanical and physical properties: A review10.1016/j.jeurceramsoc.2008.11.008 ↗
21. Pressureless densification of zirconium diboride with boron carbide additions10.1111/j.1551-2916.2006.00949.x ↗
22. Properties of ZrB2–SiC ceramics by pressureless sintering10.1111/j.1551-2916.2009.03039.x ↗
23. Mechanical properties of sintered ZrB2–SiC ceramics10.1016/j.jeurceramsoc.2010.11.013 ↗
24. Potential-current characteristics in SiC/ZrB2 composite ceramics10.1016/j.jeurceramsoc.2018.01.020 ↗
25. Influence of the boundaries in the impedance of porous film electrodes10.1039/b001708f ↗
26. Application of A.C. impedance techniques in studies of porous cementitious materials: (I): influence of solid phase and pore solution on high frequency resistance10.1016/0008-8846(93)90003-R ↗
27. Electroceramics: characterization by impedance spectroscopy10.1002/adma.19900020304 ↗
28. Forming and sintering behavior of B‐and C‐doped α and β‐SiC10.1111/j.1151-2916.1984.tb18829.x ↗
29. Percolation properties of random ellipses10.1103/PhysRevA.38.2650 ↗
30. Formation of low-resistance ohmic contacts between carbon nanotube and metal electrodes by a rapid thermal annealing method10.1088/0022-3727/33/16/303 ↗
31. Ceramic tensile strength-grain size relations: grain sizes, slopes, and branch intersections
32. The effect of zirconia sintering temperature on flexural strength, grain size, and contrast ratio10.1007/s00784-012-0692-6 ↗