Effect of green body density on the properties of graphite-molybdenum-titanium composite sintered by spark plasma sintering
Source abstract
Abstract
This manuscript contains a study about the effect of the degree of compaction of green parts on the properties of a Graphite-5.5 vol. % Molybdenum- 0.6 vol. % Titanium composite obtained by SPS. The composite, sintered at 2000 °C, below the eutectic temperature of the C-Mo system (2584 °C), exhibits different properties depending on the direction of the applied pressure. On this matter, properties are significantly better in-plane than in the other directions. Samples uniaxially pressed at 60 MPa to obtain the green compact exhibit highly improved properties which are competitive with those obtained under extreme conditions, i.e. uniaxial pressure at 300 MPa and sintering temperature > 2000 °C in presence of a liquid phase. The composite production process could be easier scaled up to the industrial level. Thus, this graphite-molybdenum-titanium composite could be used as heat sink in a panoply of applications.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Advanced materials and composites · Advanced ceramic materials synthesis · Aluminum Alloys Composites Properties
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (38)
Show source-provided references
1. Graphite-base cermets: a new material for bearing, electrical and high-temperature applications
2. Hot-working of graphite for graphite-matrix nuclear fuels10.1016/0008-6223(65)90001-1 ↗
3. Graphite-carbide materials prepared by hot-working with the carbide phase in the liquid state10.1038/2091018a0 ↗
4. Graphite-carbide materials prepared by hot-working with a dispersed liquid-carbide phase10.1016/0008-6223(66)90043-1 ↗
5. HWLC graphites prepared by hot-working extruded stock10.1016/0008-6223(68)90043-2 ↗
6. Fabrication and characterization of metal carbide-graphite composites
7. Matthews · 1970
8. Metal/graphite-composites in fusion engineering
9. Hot-working and strengthening in metal carbide-graphite composites10.1007/BF00551515 ↗
10. Strength and fracture toughness of interpenetrating graphite/aluminium composites produced by the indirect squeeze casting process10.1016/S0921-5093(04)00915-3 ↗
11. Aluminium carbide formation in interpenetrating graphite/aluminium composites10.1016/j.msea.2006.11.088 ↗
12. Manufacturing processes and properties of copper—graphite composites produced by high frequency induction heating sintering10.1177/0021998307074145 ↗
13. Fabrication and properties of graphite flakes/metal composites for thermal management applications10.1016/j.scriptamat.2008.02.026 ↗
14. Hutsch · 2010
15. Thermal properties of aluminum–graphite composites by powder metallurgy10.1016/j.compositesb.2012.01.083 ↗
16. Copper–graphite composites: thermal expansion, thermal and electrical conductivities, and cross-property connections10.1007/s10853-016-0067-5 ↗
17. Copper-graphite composite: shear modulus, electrical resistivity, and cross-property connections10.1016/j.ijengsci.2020.103232 ↗
18. Composites of aluminum alloy and magnesium alloy with graphite showing low thermal expansion and high specific thermal conductivity10.1080/14686996.2017.1286222 ↗
19. Cu-expanded graphite composite material preparation and thermal properties10.18321/ectj671 ↗
20. Thermal and mechanical properties of copper-graphite and copper-reduced graphene oxide composites10.1016/j.compositesb.2018.11.004 ↗
21. Characterization of copper–Graphite composites fabricated via electrochemical deposition and spark plasma sintering10.3390/app9142853 ↗
22. Cross property connection between the electric and the thermal conductivities of copper graphite composites10.1016/j.ijengsci.2019.103130 ↗
23. Microstructure and properties of copper–Graphite composites fabricated by spark plasma sintering based on two-step mixing10.3390/met10111506 ↗
24. Microstructure, and physical and mechanical properties of copper–Graphite composites obtained by in situ reaction method10.1007/s11665-020-04646-8 ↗
25. Mariani · 2014
26. Inventors; CERN - european organization for nuclear research, brevetti bizz S.R.L., assignees. A molybdenum carbide / carbon composite and manufacturing method
27. Development and properties of high thermal conductivity molybdenum carbide - graphite composites10.1016/j.carbon.2018.04.010 ↗
28. Concentrated solar energy applications in materials science and metallurgy10.1016/j.solener.2018.05.065 ↗
29. Formation of hexagonal η-MoC1-x phase at a temperature lower than 1660 °C by solar radiation heating under presence of excess free carbon10.1016/j.ijrmhm.2006.05.004 ↗
30. Carbide synthesis from graphite/molybdenum powder mixtures at sub-stoichiometric ratios under solar radiation heating to 1900 °C10.2320/matertrans.MRA2008202 ↗
31. Carbide phases synthesised from C/Mo powder compacts at specified sub-stoichiometric ratios by solar radiation heating to temperatures between 1600 °C and 2500 °C10.2320/matertrans.M2009167 ↗
32. The structure of dimolybdenum carbide by neutron diffraction technique10.1107/S0365110X63000487 ↗
33. Nagai. X-ray Spectroscopic Analysis of Solid State Reaction during Mechanical Alloying of Molybdenum and Graphite Powder Mixture10.2320/matertrans.43.2292 ↗
34. The high temperature interaction between molybdenum and graphite10.1007/BF00754489 ↗
35. Low temperature catalytic graphitization of hard carbon10.1016/0008-6223(66)90060-1 ↗
36. A model to describe neutron-induced dimensional changes in pyrolytic carbon10.1016/0008-6223(67)90025-5 ↗
37. Interaction of evaporated carbon with heated metal substrates10.1016/0008-6223(67)90056-5 ↗
38. Compaction and Hot working of natural graphite-molybdenum carbide composite