Wettability and infiltration of Si melt on SiO2-Si3N4 composite ceramic
Source abstract
Abstract
Abstract Non-wettable material with Si melt is preferred to manufacture crucible in order to avoid adhesion between Si and traditional fused silica crucible. In this work, wetting and infiltration behaviors of Si drop on porous/dense SiO2-Si3N4 ceramic and SiO2 ceramic were systematically studied via the sessile drop technology and microstructural analysis method. The porous SiO2-Si3N4 ceramic exhibited non-wetting behavior with stable contact angle of about 130 °. Nevertheless, dense SiO2-Si3N4 ceramic and SiO2 ceramic displayed wetting features with Si drop. For both SiO2-Si3N4 ceramics, three kinds of infiltrations were observed, including infiltration under Si drop, infiltration under substrate surface (beyond drop) and infiltration on substrate surface. Notably, the infiltration under Si drop had the slowest speed with tiny infiltration depth. The above non-wetting behavior and tiny infiltration under drop of porous SiO2-Si3N4 ceramic were closely related to material pore characteristics and Si/substrate interfacial reaction.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Advanced ceramic materials synthesis · Aerogels and thermal insulation · Additive Manufacturing and 3D Printing Technologies
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (37)
Show source-provided references
1. Silicon solar cells: toward the efficiency limits
2. Improvement of multi-crystalline silicon ingot growth by using diffusion barriers10.1016/j.jcrysgro.2014.01.045 ↗
3. Chemical stability of silicon nitride coatings used in the crystallization of photovoltaic silicon ingots. Part II: Stability under argon flow10.1016/j.jeurceramsoc.2016.07.021 ↗
4. Wetting, infiltration and sticking phenomena in Si3N4 releasing coatings in the growth of photovoltaic silicon10.1016/j.solmat.2009.10.020 ↗
5. The crucible/silicon interface in directional solidification of photovoltaic silicon10.1016/j.actamat.2017.02.072 ↗
6. Effect of pre-oxidation of Si3N4 powders on the interaction between Si3N4 coating and molten Si10.1016/j.ceramint.2018.05.152 ↗
7. Influence of oxidation on the wetting behavior of liquid silicon on Si3N4-coated substrates10.1016/j.jcrysgro.2010.05.006 ↗
8. Wettability and infiltration of Si drop on silica substrate containing α-Si3N4 coating: influence of oxygen content in α-Si3N4 coating10.1016/j.ceramint.2020.02.036 ↗
9. Wetting properties of silicon incorporated DLC films on aluminum substrate10.1002/9781118511428.ch15 ↗
10. Wetting of ceramics by molten silicon and silicon alloys: a review10.1007/s10853-012-6663-0 ↗
11. Reactive wetting in the liquid-silicon/solid-carbon system10.1111/j.1151-2916.1996.tb08519.x ↗
12. Studying the wettability of Si and eutectic Si-Zr alloy on carbon and silicon carbide by sessile drop experiments10.1016/j.jeurceramsoc.2018.11.049 ↗
13. Wettability and infiltration of liquid silicon on graphite substrates10.3390/met9030300 ↗
14. Reactions between silicon and graphite substrates at high temperature: in situ observations10.1007/s11663-013-9947-0 ↗
15. Wetting properties of molten silicon with graphite materials10.1007/s11661-010-0362-8 ↗
16. Wetting and infiltration of nitride bonded silicon nitride by liquid silicon10.1016/j.jcrysgro.2016.02.002 ↗
17. Wetting and adhesion of Si on Si3N4 and BN substrates10.1016/j.jeurceramsoc.2009.01.024 ↗
18. Surface tension of liquid silicon: high or low value?10.1016/j.jcrysgro.2013.02.010 ↗
19. Wetting behavior and reactivity of molten silicon with h-BN substrate at ultrahigh temperatures up to 1750°C10.1007/s11665-017-3114-8 ↗
20. Inhibiting crystallization of fused silica ceramic at high temperature with addition of α-Si3N410.1016/j.ceramint.2020.12.266 ↗
21. Wettability and reactivity of molten silicon with various substrates10.1007/s00339-002-2001-8 ↗
22. Wetting and reaction between Si droplet and SiO2 substrate10.1007/s10853-007-2090-z ↗
23. Wetting behavior and reaction mechanism of molten Si in contact with silica substrate10.1016/j.ceramint.2019.07.123 ↗
24. Mould shaping silicon crystal growth with a mould coating material by the spinning method10.1016/0022-0248(86)90524-5 ↗
25. Wettability of porous surfaces10.1039/tf9444000546 ↗
26. Effect of gas evolution at solid-liquid interface on contact angle between liquid Si and SiO210.1023/A:1004673605025 ↗
27. Preparation and evaluation of porous Si3N4 ceramic substrates that repel Si melt10.2109/jcersj2.121.401 ↗
28. Image analysis characterization of periodic porous materials produced by additive manufacturing10.1016/j.matdes.2015.12.062 ↗
29. Using image analysis to measure the porosity distribution of a porous pavement10.1016/j.conbuildmat.2013.06.093 ↗
30. Determination of mechanical properties of porous silicon with image analysis and finite element10.1016/j.phpro.2014.07.056 ↗
31. Study on the gel casting of fused silica glass10.1016/j.jnoncrysol.2007.01.109 ↗
32. A novel approach to improve flexural strength of Al2O3-20 wt% ZrO2 composites by oscillatory pressure sintering10.1111/jace.15341 ↗
33. Reactive infiltration by Si: infiltration versus wetting10.1016/j.scriptamat.2010.02.030 ↗
34. Initial stages of silicon-crucible interactions in crystallisation of solar grade silicon: kinetics of coating infiltration10.1016/j.actamat.2014.04.072 ↗
35. Eustathopoulos · 1999
36. The effect of sharp solid edges on the droplet wettability10.1016/j.jcis.2019.05.081 ↗
37. Chemical stability of silicon nitride coatings used in the crystallization of photovoltaic silicon ingots. Part I: Stability in vacuum10.1016/j.jeurceramsoc.2016.07.019 ↗