journal article·2022-08

Influences of SiC infiltration and coating on compressive mechanical behaviours of 2D C/SiC composites up to 1600 °C at wide-ranging strain rates

Chao Zhang, Tianhao Guan, Tengfei Ren, Xinyue Zhang, Bo Wang, Xi Zhou, Tao Suo

Publisher page

Abstract

No abstract is available for this record. The assistant can identify its topic from the title, but cannot infer the study’s results.

Source: Not provided · Quality: missing

Research context

OpenAlex topics: Advanced ceramic materials synthesis · MXene and MAX Phase Materials · Advanced materials and composites

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (44)

Show source-provided references
1. Advanced structural ceramics in aerospace propulsion10.1038/nmat4687 ↗
2. Real-time quantitative imaging of failure events in materials under load at temperatures above 1,600°C10.1038/nmat3497 ↗
3. Advances in modifications and high-temperature applications of silicon carbide ceramic matrix composites in aerospace: a focused review10.1016/j.jeurceramsoc.2021.03.051 ↗
4. Machining of SiC ceramic matrix composites: a review10.1016/j.cja.2020.08.001 ↗
5. Dynamic fracture of C/SiC composites under high strain-rate loading: microstructures and mechanisms10.1016/j.carbon.2015.05.015 ↗
6. Compressive behavior of C/SiC composites over a wide range of strain rates and temperatures10.1016/j.carbon.2013.06.044 ↗
7. Dynamic compressive fracture of C/SiC composites at different temperatures: microstructure and mechanism10.1016/j.ijimpeng.2017.08.001 ↗
8. Fracture behavior of C/SiC composites at elevated temperature10.1007/s12206-017-0702-3 ↗
9. Experimental study of high-temperature tensile mechanical properties of 3D needled C/C–SiC composites10.1016/j.msea.2015.12.010 ↗
10. Mechanical properties of a carbon fiber reinforced self-healing multilayered matrix composite at elevated temperatures10.1016/j.msea.2011.01.009 ↗
11. Tensile behavior of 2D-C/SiC composites at elevated temperatures: experiment and modeling
12. Interlaminar shear damage mechanisms of a 2D-C/SiC composite at elevated temperature in vacuum10.1016/j.vacuum.2014.02.017 ↗
13. Improvement of the mechanical and thermophysical properties of C/SiC composites fabricated by liquid silicon infiltration10.1016/j.compscitech.2015.04.019 ↗
14. Tensile fatigue of a 2.5D-C/SiC composite at room temperature and 900 °C10.1016/j.matdes.2013.01.076 ↗
15. Kinetics and mechanisms of oxidation of 2D woven C/SiC composites: I, experimental approach10.1111/j.1151-2916.1994.tb07096.x ↗
16. Thermal residual stresses in ceramic matrix composites—I. Axisymmetrical model and finite element analysis10.1016/0956-7151(94)00429-3 ↗
17. Finite element simulation of stress distribution and development of Cf/SiC ceramic–matrix composite coated with single layer SiC coating during thermal shock10.1016/j.compositesb.2013.03.028 ↗
18. Influence of the strain rate on the mechanical behavior of the 3D needle-punched C/SiC composite10.1016/j.msea.2009.01.024 ↗
19. Dynamic compressive mechanical properties and a new constitutive model of 2D-C/SiC composites
20. Strain rate-dependent compressive properties of C/C composites10.1016/j.msea.2007.10.077 ↗
21. Layer-directional dynamic compressive mechanical properties of two kinds of densifications 2D-C/SiC
22. Oxidation behavior of C/SiC-Ti3SiC2 at 800–1300°C in air10.1016/j.jeurceramsoc.2016.03.029 ↗
23. The effect of hole defects on the oxidation behaviour of two-dimensional C/SiC composites10.1016/j.ceramint.2016.06.200 ↗
24. Tensile strength degradation of a 2.5D-C/SiC composite under thermal cycles in air10.1016/j.jeurceramsoc.2015.12.007 ↗
25. Creep behavior of C/SiC composite in hot oxidizing atmosphere and its mechanism10.1016/j.ceramint.2017.04.102 ↗
26. Compressive strength of 2D-C/SiC composite at high temperature in air, Hangkong Cailiao Xuebao/Journal of Aeronautical
27. An equivalent diffusion coefficient model of the oxidation of ceramic matrix composites10.1016/j.ceramint.2021.04.084 ↗
28. Effect of oxidation and residual stress on mechanical properties of SiC seal coated C/SiC composite10.1016/j.ceramint.2017.10.085 ↗
29. Increasing the strength and toughness of a carbon fiber/silicon carbide composite by heat treatment10.1016/j.carbon.2012.11.001 ↗
30. A damage-induced short-circuit diffusion model applied to the oxidation calculation of ceramic matrix composites (CMCs)10.1016/j.compositesa.2019.105621 ↗
31. Study of dynamic compressive behaviors of 2D C/SiC composites at elevated temperatures based on in-situ observation10.1016/j.jeurceramsoc.2020.06.036 ↗
32. Measurements for displacement and deformation at high temperature by using edge detection of digital image10.1364/AO.54.008731 ↗
33. An experimental method for determination of dynamic mechanical behavior of materials at high temperatures10.1016/j.ijimpeng.2016.12.002 ↗
34. In-plane mechanical behavior and failure mode of a 2D-SiC/SiC composite under uniaxial dynamic compression10.1016/j.ceramint.2018.07.280 ↗
35. Mechanical behaviour in compression loading of 2D-composite materials made of carbon fabrics and a ceramic matrix10.1007/BF01161188 ↗
36. Dynamic fiber debonding and frictional push-out in model composite systems: numerical simulations10.1016/S0167-6636(02)00141-2 ↗
37. Dynamic effect on strength in SiCf/SiCm composite10.1016/S0734-743X(00)00036-1 ↗
38. Shear strength as a function of test rate for SiCf/BSAS ceramic matrix composite at elevated temperature10.1111/j.1151-2916.2004.tb06340.x ↗
39. Fiber-matrix adhesion and its effect on composite mechanical properties. III. Longitudinal (0) compressive properties of graphite/epoxy composites10.1177/002199839202600301 ↗
40. Oxidation and defect control of CVD SiC coating on three-dimensional C/SiC composites10.1016/S0008-6223(02)00103-3 ↗
41. Oxidation behavior of C–SiC composites with a Si–W coating from room temperature to 1500°C10.1016/S0008-6223(00)00066-X ↗
42. Oxidation effects on in-plane and interlaminar shear strengths of two-dimensional carbon fiber reinforced silicon carbide composites10.1016/j.carbon.2015.10.091 ↗
43. Oxidation and microstructure of SiCf /SiC composites in moist air up to 1600°C by X‐ray tomographic characterization10.1111/ijac.13450 ↗
44. The development of compression damage zones in fibrous composites10.1016/S0266-3538(01)00176-2 ↗