journal article·2022-10

Compressive strength degradation of SiC fibers exposed to high temperatures due to impurity-induced internal oxidation

Xinwei Yuan, Sosuke Kondo, Kazuya Shimoda, Hao Yu, Yasuki Okuno, Ryuta Kasada

Publisher page

Abstract

No abstract is available for this record. The assistant can identify its topic from the title, but cannot infer the study’s results.

Source: Not provided · Quality: missing

Research context

OpenAlex topics: Advanced ceramic materials synthesis · Advanced materials and composites · Aluminum Alloys Composites Properties

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (41)

Show source-provided references
1. Study on silicon carbide
2. SiC matrix/SiC fiber composite: a high-heat flux, low activation, structural material10.1016/S0022-3115(86)80025-3 ↗
3. Properties of silicon carbide for nuclear fuel particle coatings10.13182/NT77-A31892 ↗
4. Handbook of SiC properties for fuel performance modeling10.1016/j.jnucmat.2007.05.016 ↗
5. The effect of porous carbon preform and the infiltration process on the properties of reaction-formed SiC10.1016/j.carbon.2004.03.018 ↗
6. Development of a silicon carbide fibre with high tensile strength10.1038/261683a0 ↗
7. Critical issues and current status of SiC/SiC composites for fusion10.1016/S0022-3115(00)00374-3 ↗
8. Current status and recent research achievements in SiC/SiC composites10.1016/j.jnucmat.2014.06.003 ↗
9. Growth of SiO2 on SiC by dry thermal oxidation: mechanisms10.1088/0022-3727/40/20/S10 ↗
10. Silicon carbide oxidation in steam up to 2 MPa10.1111/jace.13094 ↗
11. A review of third generation SiC fibers and SiCf/SiC composites10.1016/j.jmst.2019.07.020 ↗
12. Mechanical properties of high purity SiC fiber-reinforced CVI-SiC matrix composites10.13182/FST03-A336 ↗
13. Continuous SiC fiber, CVI SiC matrix composites for nuclear applications: properties and irradiation effects10.1016/j.jnucmat.2013.06.040 ↗
14. Mechanical behavior of SiCf/SiC composites with alternating PyC/SiC multilayer interphases10.1016/j.matdes.2012.07.073 ↗
15. Thermophysical and mechanical properties of near-stoichiometric fiber CVI SiC/SiC composites after neutron irradiation at elevated temperatures10.1016/j.jnucmat.2010.06.002 ↗
16. Model for SiC fiber strength after oxidation in dry and wet air10.1111/jace.15907 ↗
17. Evaluation of neutron irradiated silicon carbide and silicon carbide composites10.1016/j.jnucmat.2007.05.007 ↗
18. Irradiation-induced shrinkage of highly crystalline SiC fibers10.1016/j.actamat.2014.07.057 ↗
19. Microstructure and oxidative degradation behavior of silicon carbide fiber Hi-Nicalon type S10.1016/S0022-3115(98)00223-2 ↗
20. High-strength alkali-resistant sintered SiC fibre stable to 2,200 °C10.1038/35820 ↗
21. High-temperature tensile strength of near-stoichiometric SiC/SiC composites10.1016/S0022-3115(02)01049-8 ↗
22. Effects of specimen geometry and base material on the mechanical behavior of focused-ion-beam-fabricated metallic-glass micropillars10.1016/j.actamat.2008.11.043 ↗
23. A statistical distribution function of wide applicability10.1115/1.4010337 ↗
24. A practical and systematic review of Weibull statistics for reporting strengths of dental materials
25. Guidelines for two-parameter weibull analysis for flaw-containing materials10.1007/s11663-011-9556-8 ↗
26. Characterization of nearly stoichiometric SiC ceramic fibres10.1023/A:1017988827616 ↗
27. Comparison of stress concentration versus minimum solid area based mechanical property-porosity relations10.1007/BF00367582 ↗
28. Bubble formation in oxide scales on SiC10.1111/j.1151-2916.1984.tb19160.x ↗
29. Oxidation behaviour of silicon carbide-a review
30. SiC-based ceramic fibers prepared via organic-to-inorganic conversion process-review10.2109/jcersj.114.445 ↗
31. An interacting micro-crack damage model for failure of brittle materials under compression10.1016/j.jmps.2007.06.012 ↗
32. A detailed study of the microstructure and thermal stability of typical SiC fibers10.1016/j.matchar.2018.09.041 ↗
33. Hi-nicalonTM-S SiC fiber oxidation and scale crystallization kinetics10.1111/j.1551-2916.2011.04647.x ↗
34. Sliding wear resistance of sintered SiC-fiber bonded ceramics10.1016/j.ijrmhm.2014.06.020 ↗
35. Multiscale characterization of irradiation behaviour of ion-irradiated SiC/SiC composites10.1016/j.actamat.2018.09.012 ↗
36. Mechanical properties of SiC composites neutron irradiated under light water reactor relevant temperature and dose conditions10.1016/j.jnucmat.2017.07.007 ↗
37. Influence of the carbon interface on the mechanical behavior of SiC/SiC composites10.1016/j.compositesa.2020.105867 ↗
38. X-ray diffraction study of the effect of high-temperature heat treatment on the microstructural stability of third-generation SiC fibers10.1111/jace.12174 ↗
39. Cavity formation in Tyranno-SA SiCf/SiC composite irradiated with multiple-ion beam at elevated temperatures10.1016/j.jnucmat.2007.03.087 ↗
40. Longitudinal dilation behavior of ion-irradiated TyrannoTM-SA SiC fibers at elevated-temperatures10.1016/j.jnucmat.2012.06.009 ↗
41. G.L. Abernethy, R.B., Breneman, J.E., Medlin, C.H., Reinman, Weibull analysis handbook, Pratt and Whitney West Palm Beach Fl Government Products DIV. (1983).10.21236/ADA143100 ↗