Abstract

Abstract A new toughness test for ball-shaped specimens is presented. In analogy to the “Surface Crack in Flexure”-method the fracture toughness is determined by making a semi-elliptical surface crack with a Knoop indenter into the surface of the specimen. In our case the specimen is a notched ball with an indent opposite to the notch. The recently developed “Notched Ball Test” produces a well defined and almost uniaxial stress field. The stress intensity factor of the crack in the notched ball is determined with FE methods in a parametric study in the practical range of the notch geometries, crack shapes and other parameters. The results correlate well with established calculations based on the Newman–Raju model. The new test is regarded as a component test for bearing balls and offers new possibilities for material selection and characterisation. An experimental evaluation on several ceramic materials will be presented in a consecutive paper.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Advanced ceramic materials synthesis · High-Velocity Impact and Material Behavior · Advanced materials and composites

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (39)

Show source-provided references
1. Köttritsch · 2007
2. Rolling contact silicon nitride bearing technology: a review of recent research10.1016/S0043-1648(00)00504-4 ↗
3. Strength tests on silicon nitride balls10.4028/www.scientific.net/KEM.409.193 ↗
4. The Notched Ball Test – a new strength test for ceramic spheres
5. The strength of ceramic balls – the Notched Ball Test
6. A new test to determine the tensile strength of brittle balls – the Notched Ball Test10.1016/j.jeurceramsoc.2009.02.018 ↗
7. Strength measurement of ceramic spheres using a diametrally compressed “C-Sphere” specimen10.1111/j.1551-2916.2007.01639.x ↗
8. ASTM · 2008
9. Indentation crack profiles in silicon nitride10.1016/S0955-2219(00)00197-7 ↗
10. Relationship between fracture toughness determined by surface crack in flexure and fracture resistance measured by indentation fracture for silicon nitride ceramics with various microstructures10.1016/j.ceramint.2008.01.006 ↗
11. Further reply to “comments on elastic/plastic indentation damage in ceramics: the median/radial crack system”10.1111/j.1151-2916.1982.tb10482.x ↗
12. A critical evaluation of indentation techniques for measuring fracture toughness. I. Direct crack measurements10.1111/j.1151-2916.1981.tb10320.x ↗
13. CEN EN 14425-5 · 2005
14. Critical notch root radius in SENB-S fracture toughness testing10.1016/0955-2219(95)00197-2 ↗
15. Polished notch modification of SENB-S fracture toughness testing10.1016/S0955-2219(97)00024-1 ↗
16. ASTM C 1421-01b · 2001
17. ISO 18756 · 2003
18. Witschnig S. Zähigkeitsmessung an keramischen Kugeln. Institut für Struktur- und Funktionskeramik. Diploma Thesis. Leoben: Montanuniversitaet Leoben; 2010.
19. Munz · 2001
20. Lawn · 1993
21. Murakami · 1987
22. Fracture toughness by the surface crack in flexure (SCF) method: results of the VAMAS round robin10.1002/9780470314555.ch30 ↗
23. Quinn GD, Kübler J, Gettings RJ. Fracture toughness of advanced ceramics by the surface crack in flexure (SCF) method: a VAMAS round robin. VAMAS Report No. 17. Report 1994.
24. Newman JC, Raju IS. Analysis of surface cracks in finite plates under tension or bending loads NASA. Report TP-1578; 1979.
25. An empirical stress-intensity factor equation for the surface crack10.1016/0013-7944(81)90116-8 ↗
26. Raju IS, Newman JC. Improved stress-intensity factors for semi-elliptical surface cracks in finite-thickness plates NASA. Report TM-X-72825; 1977.
27. Fett · 1997
28. Anderson · 2005
29. Quantification of the influence of vertex singularities on fatigue crack behavior10.1016/j.commatsci.2008.08.009 ↗
30. The effect of a free surface on fatigue crack behaviour10.1016/j.ijfatigue.2010.01.009 ↗
31. Fracture mechanics of the three-dimensional crack front: vertex singularity versus out of plain constraint descriptions10.1016/j.proeng.2010.03.225 ↗
32. Application of the finite element method to linear elastic fracture mechanics10.1115/1.3119488 ↗
33. Advantages of the J-integral approach for calculating stress intensity factors when using the commercial finite element software ABAQUS10.1016/j.engfracmech.2005.02.003 ↗
34. Virtual crack closure technique: history, approach, and applications10.1115/1.1595677 ↗
35. Implementation of the virtual crack closure technique in engineering FE calculations10.1016/j.finel.2006.10.004 ↗
36. A virtual crack closure-integral method (VCCM) to compute the energy release rates and stress intensity factors based on quadratic tetrahedral finite elements10.1016/j.engfracmech.2008.04.014 ↗
37. Fett · 2009
38. The influence of the Poisson's ratio and corner point singularities in three-dimensional plasticity-induced fatigue crack closure: a numerical study10.1016/j.ijfatigue.2008.01.009 ↗
39. Fracture toughness of ceramic balls