Fracture toughness and slow crack growth behaviour of metal-proton conducting ceramic composites
Source abstract
Abstract
The fracture toughness and slow crack growth behaviour of two load-bearing metal ceramic components adopted in negatrode-supported electrochemical devices, namely Ni-BCZY27 and Ni-BCZY442, are investigated via double torsion technique. The investigation showed that the two metal-ceramic composites are considerably less sensitive to slow crack growth when compared to oxide ceramics such as stabilized zirconia and alumina, with KI0/KIC equal to approximately 0.8. On the other hand, they also showed lower fracture toughness than Ni-3YSZ, with Ni-BCZY442 and Ni-BCZY27 having a fracture toughness of respectively 1.74 and 3.04 MPa*m1/2 for porosities equal to 25.8% and 19.1% respectively, compared to Ni-3YSZ reported in previous work with similar Ni content and porosity of approximately 30% having a fracture toughness equal to 3.4 MPa*m1/2. Furthermore, the analysis of samples presenting extensive barium depletion indicated fast fracture propagation upon application of loads significantly lower than the critical fracture load.
Source: openalex_inverted_index · Quality: baseline
Research context
OpenAlex topics: Advancements in Solid Oxide Fuel Cells · Thermal Expansion and Ionic Conductivity · Electronic and Structural Properties of Oxides
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (65)
Show source-provided references
1. Chemically stable yttrium and tin co-doped barium zirconate electrolyte for next generation high performance proton-conducting solid oxide fuel cells10.1002/aenm.201201062 ↗
2. Structural study and proton conductivity in BaCe0.7Zr0.25−xYxZn0.05O3 (x = 0.05, 0.1, 0.15, 0.2 & 0.25)10.1016/j.ijhydene.2016.02.135 ↗
3. Proton conductivity: compounds and their structural and chemical peculiarities10.1002/bbpc.19920961143 ↗
4. Proton-conducting oxides for energy conversion and storage10.1063/1.5135319 ↗
5. Trends in research and development of protonic ceramic electrolysis cells10.1016/j.ijhydene.2019.08.130 ↗
6. Improved mechanical strength, proton conductivity and power density in an ‘all-protonic’ ceramic fuel cell at intermediate temperature
7. Review—Electrochemical CO2 reduction for CO production: comparison of low- and high-temperature electrolysis technologies10.1149/1945-7111/ab7099 ↗
8. Progress report on proton conducting solid oxide electrolysis cells10.1002/adfm.201903805 ↗
9. High temperature electrolysis in alkaline cells, solid proton conducting cells, and solid oxide cells10.1021/cr5000865 ↗
10. Solid-oxide fuel cells: recent progress on advanced materials for solid-oxide fuel cells operating below 500°C (Adv. Mater. 48/2017)10.1002/adma.201770345 ↗
11. A short review of cathode poisoning and corrosion in solid oxide fuel cell10.1016/j.ijhydene.2017.08.057 ↗
12. Tailoring the chemical stability of Ba(Ce0.8−xZrx)Y0.2O3−δ protonic conductors for Intermediate Temperature Solid Oxide Fuel Cells (IT-SOFCs)10.1016/j.ssi.2008.04.002 ↗
13. A high performance BaZr0.1Ce0.7Y0.2O3-δ-based solid oxide fuel cell with a cobalt-free Ba0.5Sr0.5FeO3-δ–Ce0.8Sm0.2O2-δ composite cathode10.1016/j.ijhydene.2010.05.084 ↗
14. Ni-Ce0.9Gd0.1O1.95 anode for GDC electrolyte-based low-temperature SOFCs10.1016/j.ssi.2003.11.012 ↗
15. Proton conductivity: materials and applications10.1021/cm950192a ↗
16. Chemical solution deposition of thin films for protonic ceramic fuel cells10.1016/j.ssi.2013.10.027 ↗
17. Proton trapping in yttrium-doped barium zirconate10.1038/nmat3638 ↗
18. High total proton conductivity in large-grained yttrium-doped barium zirconate10.1021/cm900208w ↗
19. Fuel cell materials and components10.1016/j.actamat.2003.08.004 ↗
20. Progress in material selection for solid oxide fuel cell technology: a review10.1016/j.pmatsci.2015.01.001 ↗
21. Nanomaterials and technologies for low temperature solid oxide fuel cells: recent advances, challenges and opportunities10.1016/j.nanoen.2017.12.044 ↗
22. Mathematical modelling of proton-conducting solid oxide fuel cells and comparison with oxygen-ion-conducting counterpart10.1002/fuce.200600049 ↗
23. Exceptional power density and stability at intermediate temperatures in protonic ceramic fuel cells10.1038/s41560-017-0085-9 ↗
24. Proton-conducting solid oxide fuel cell (SOFC) with Y-doped BaZrO3 electrolyte10.1016/j.elecom.2017.05.006 ↗
25. High oxide ion and proton conductivity in a disordered hexagonal perovskite10.1038/s41563-020-0629-4 ↗
26. Highly efficient reversible protonic ceramic electrochemical cells for power generation and fuel production10.1038/s41560-019-0333-2 ↗
27. Highly dense and novel proton conducting materials for SOFC electrolyte10.1016/j.ijhydene.2017.09.067 ↗
28. Proton-conducting oxides10.1146/annurev.matsci.33.022802.091825 ↗
29. Chemo-thermo-mechanical coupling in protonic ceramic fuel cells from fabrication to operation10.1149/2.1071912jes ↗
30. Nanostructured ceramic oxides with a slow crack growth resistance close to covalent materials10.1021/nl050492j ↗
31. Global description of crack propagation in ceramics10.1016/j.jeurceramsoc.2005.11.004 ↗
32. Crack growth resistance of alumina, zirconia and zirconia toughened alumina ceramics for joint prostheses10.1016/S0142-9612(01)00206-X ↗
33. Slow crack growth and hydrothermal aging stability of an alumina-toughened zirconia composite made from La2O3-doped 2Y-TZP10.1016/j.jeurceramsoc.2016.11.003 ↗
34. Fracture toughness, strength and slow crack growth in a ceria stabilized zirconia–alumina nanocomposite for medical applications10.1016/j.biomaterials.2008.05.021 ↗
35. Subcritical crack propagation in 3Y-TZP ceramics: static and cyclic fatigue10.1111/j.1151-2916.1999.tb02213.x ↗
36. Improving the durability of a biomedical-grade zirconia ceramic by the addition of silica10.1111/j.1151-2916.2002.tb00103.x ↗
37. Influence of porosity on mechanical properties of tetragonal stabilized zirconia10.1016/j.jeurceramsoc.2017.09.029 ↗
38. Fracture toughness and slow crack growth behavior of Ni-YSZ and YSZ as a function of porosity and temperature, in: adv. solid oxide fuel cells II10.1002/9780470291337.ch36 ↗
39. Double Torsion testing of thin porous zirconia supports for energy applications: Toughness and slow crack growth assessment10.1016/j.jeurceramsoc.2020.02.019 ↗
40. Aspects of the formation and mobility of protonic charge carriers and the stability of perovskite-type oxides10.1016/S0167-2738(99)00188-5 ↗
41. Yttrium and hydrogen superstructure and correlation of lattice expansion and proton conductivity in the BaZr0.9Y0.1O2.95 proton conductor10.1063/1.3268454 ↗
42. Chemical expansion and change in lattice constant of Y-Doped BaZrO 3 by hydration/dehydration reaction and final heat-treating temperature10.1111/jace.12172 ↗
43. Chemical expansion due to hydration of proton-conducting perovskite oxide ceramics10.1111/jace.12990 ↗
44. Toughening of Y-doped BaZrO3 proton conducting electrolytes by hydration10.1039/C6TA11022C ↗
45. Planar proton-conducting ceramic cells for hydrogen extraction: Mechanical properties, electrochemical performance and up-scaling10.1016/j.ijhydene.2021.12.041 ↗
46. Fracture of brittle solids10.1017/CBO9780511623127 ↗
47. Effects of chemical environments on slow crack growth in glasses and ceramics10.1029/JB089iB06p04072 ↗
48. Double-torsion testing a 3Y-TZP ceramic10.1016/0272-8842(95)00076-3 ↗
49. An evaluation of the double torsion technique10.1007/s11340-011-9468-1 ↗
50. The double torsion loading configuration for fracture propagation: an improved methodology for the load-relaxation at constant displacement10.1016/S1365-1609(00)00045-9 ↗
51. Realistic finite-element model for the double-torsion loading configuration10.1111/j.1151-2916.2000.tb01625.x ↗
52. Simple method for studying slow crack growth10.1520/JTE10015J ↗
53. E. Fuller, An Evaluation of Double-Torsion Testing—Analysis, in: Fract. Mech. Appl. to Brittle Mater., ASTM International, 100 Barr Harbor Drive, PO Box C700, West Conshohocken, PA 19428-2959, 1979: pp. 3-3–16. https://doi.org/10.1520/STP36621S.10.1520/STP36621S ↗
54. A method for evaluating the time-dependent failure characteristics of brittle materials and its application to polycrystalline alumina10.1007/BF00550196 ↗
55. Experimental evaluation of the double torsion analysis on soda-lime glass10.1007/s10853-007-1660-4 ↗
56. NIH Image to ImageJ: 25 years of image analysis10.1038/nmeth.2089 ↗
57. On the vickers indentation fracture toughness test10.1111/j.1551-2916.2006.01482.x ↗
58. Slow crack propagation in Y-TZP/metal composites10.1016/j.jeurceramsoc.2005.06.005 ↗
59. Slow crack growth resistance and bridging stress determination in alumina-rich magnesium aluminate spinel/tungsten composites10.1016/j.actamat.2009.01.004 ↗
60. Mechanical properties of tape cast nickel-based anode materials for solid oxide fuel cells before and after reduction in hydrogen10.1016/j.actamat.2004.08.023 ↗
61. Improving the fracture toughness of stabilized zirconia-based solid oxide cells fuel electrode supports: effects of type and concentration of stabilizer(s)10.1016/j.jeurceramsoc.2020.05.042 ↗
62. The phenomena of rupture and flow in solids
63. Non-stoichiometry, grain boundary transport and chemical stability of proton conducting perovskites10.1023/A:1004877708871 ↗
64. The influence of cation non-stoichiometry on the properties of undoped and gadolinia-doped barium cerate10.1016/S0167-2738(97)00029-5 ↗
65. Ionic conduction and nonstoichiometry in BaxCe0.90Y0.10O3−α10.1016/S0167-2738(98)00130-1 ↗